◆ Rebuild

Part 15 · Knowledge and Science

Platinum, Salt and Iron-Salt Prints

Printing photographs in sunlight with iron salts that need little or no silver. Light turns ferric iron into ferrous iron, and ferrous iron throws down silver, platinum or palladium as the picture. Salt prints improved and gold-toned, Van Dyke brown and kallitype prints from a few grams of silver, and platinum and palladium prints that last as long as the paper. How to make large negatives for contact printing, and how to judge and keep the prints.

Difficulty
●●●●●
Time
A week to make the iron and developer salts; an afternoon to coat and print; ten minutes in the sun per print
Steps from zero
28 prerequisites →

You need first

PhotographyOxalic Acid

This unlocks

—
The full path from nothing — 28 steps before this one
  1. Fire
  2. Cordage and Rope
  3. Stone Tools
  4. Finding and Preparing Clay
  5. Finding and Identifying Ores
  6. Sulfur
  7. Hunting and Trapping
  8. Basic Woodworking
  9. The Kiln
  10. Pottery
  11. Charcoal
  12. Farming from Seed
  13. Hides and Leather
  14. Lime
  15. Sugar
  16. Lye and Potash
  17. Glass
  18. Bellows
  19. Saltpeter
  20. Copper Smelting
  21. Lead
  22. Laboratory Glassware
  23. Sulfuric Acid
  24. Lenses
  25. Gold and Silver
  26. Nitric Acid
  27. Oxalic Acid
  28. Photography
  29. Platinum, Salt and Iron-Salt Prints

Do them roughly in this order. See it on the tech tree →

Why it matters

The gelatin dry plates of Photography make negatives; you then need prints to give to people, file in records and hang on walls. Silver paper uses a great deal of silver. The iron processes in this chapter use sunlight and iron salts, which are cheap, as the light-sensitive part. The image metal is added in tiny amounts: a 20 × 25 cm Van Dyke print uses about a tenth of a gram of silver nitrate, and a platinum print about a twentieth of a gram of platinum.

  • Very little precious metal. One gram of platinum makes some 15–20 large prints.
  • The most permanent photographs known. Platinum and palladium never tarnish or fade; prints from the 1890s look as they did then. For portraits, town plans, specimens and deeds meant to outlast everyone alive, they are the best paper print there is.
  • No darkroom. Coat in dim lamplight, print in the sun, develop in a dish by a window.
  • Beautiful, long, smooth tones, warm or cool as you choose.

The cyanotype, the simplest iron process of all, is described in Blueprints and Cyanotypes. This chapter covers the others.

How it works

Iron forms two kinds of salt: ferric (iron that has given up three electrons; yellow-brown) and ferrous (iron that has given up two; pale green). See Blueprints and Cyanotypes.

  1. Light converts ferric to ferrous. Certain ferric salts, chiefly ferric oxalate (iron with the acid of sorrel, Oxalic Acid) and ferric ammonium citrate, are changed to the ferrous salt by violet and ultraviolet light. Strong light makes much ferrous salt; weak light, little. The amount of ferrous iron in each spot records the picture.
  2. Ferrous iron gives up its extra electron to a metal. Ferrous salts are eager to become ferric again. Given a salt of silver, platinum or palladium, they hand an electron over, and the metal falls out as tiny black grains, right where the ferrous iron was.
  3. Clear away the iron. The unused ferric salt is washed out with a weak acid, leaving only metal in the paper fibres.
Process Light-sensitive salt Image metal Colour Negative needs Keeps
Salt print Silver chloride Silver Red-brown; purple-brown if gold-toned Very contrasty Fades if untoned; good if gold-toned
Cyanotype Ferric ammonium citrate Prussian blue Blue Contrasty Good, but alkali bleaches it (Blueprints and Cyanotypes)
Van Dyke Ferric ammonium citrate Silver Rich brown Very contrasty Like a salt print
Kallitype Ferric oxalate Silver Brown to black Contrasty Like a salt print; excellent if toned
Platinum Ferric oxalate Platinum Neutral to cool black Contrasty As long as the paper
Palladium Ferric oxalate Palladium Warm brown-black Contrasty As long as the paper
1. Exposure 2. Development 3. Cleared print clear part of negative: ferric → ferrous (green) dense part: ferric stays (yellow) silver, platinum or palladium salt ferrous hands an electron to the metal salt: metal grains form only where light fell weak acid washes out unused ferric salt black metal = shadows bare paper = highlights ferric salt ferrous salt dissolved metal salt metal grain The cyanotype works the same way, but the ferrous iron makes Prussian blue instead of metal.
Fig. 1 The shared chemistry of the iron processes. Light turns yellow ferric iron into ferrous iron. In the developer, each ferrous iron gives up an electron to a silver, platinum or palladium salt, and the metal is left as black grains in the paper. Unexposed ferric salt is washed out.

All these papers are slow. They are printed by contact, the negative pressed against the paper in a printing frame, so the print is exactly the size of the negative. To make a big print you need a big negative (below).

What you need

Item Amount Notes
Rag paper Smooth, strong, well-sized Cotton or linen (Paper); no chalk filler
Green vitriol 30 g makes about 70 ml of sensitiser For ferric oxalate; Sulfuric Acid
Oxalic acid 150 g Oxalic Acid
Potash 150 g, purified For the developer; Lye and Potash
Silver nitrate 5–10 g Photography
Platinum or palladium 1–5 g Platinum and the Platinum Metals, Palladium, Rhodium and Iridium; outline below
Hydrochloric or citric acid A little Clearing baths; Hydrochloric Acid, Citric and Tartaric Acid
Hypo 100 g Fixer, for the silver processes
Coating rod Glass rod 1 cm thick, 25 cm long Laboratory Glassware
Dropper bottles, brown glass 4–6 Drops are the unit of measure
Printing frame with split back Larger than your biggest negative Blueprints and Cyanotypes
Dishes Glass or glazed, larger than the print Never bare metal

Use rain or distilled water for every solution (Distillation). Iron and silver solutions spoil when they touch bare iron, copper or brass, so brushes must have no metal ferrule (tie the hairs with thread) and dishes must be glass, glazed ware or wood lined with wax.

Where to find it

Making the solutions

Ferric oxalate sensitiser

This is the heart of kallitype, platinum and palladium printing. Work in dim light from step 5 on.

  1. Make ferric iron. Dissolve 28 g green vitriol in 150 ml warm water with 3–4 drops of Sulfuric Acid. Add Hydrogen Peroxide and Oxygen Bleach a little at a time, stirring, until the pale green turns clear yellow-brown. (Nitric acid also works, outdoors, as in Blueprints and Cyanotypes.) Test: a drop of the liquid on a white tile with a drop of red prussiate solution must not turn blue. Blue means ferrous iron is still there; add more.
  2. Throw down the hydroxide. Pour in Ammonia water or a solution of Soda Ash and Baking Soda, stirring, until no more red-brown jelly forms. This is ferric hydroxide.
  3. Wash it well. Let it settle, pour off the liquid, and fill with fresh water. Repeat 8–10 times until a drop of the wash water dried on clean glass leaves no ring. Left-over sulfate spoils the prints.
  4. Drain it on a cloth until it is a thick paste. Do not let it dry; dried hydroxide will not dissolve.
  5. Dissolve. Stir the wet paste into 19 g of oxalic acid dissolved in 50 ml of water at about 40 °C. Cover, keep warm and dark, and stir now and then for one to two days. It slowly dissolves to a clear yellow-green liquid. A little brown hydroxide left over is good: it means there is no free acid to spare.
  6. Filter, make the volume up to 70 ml with water, and add 1.5 g of oxalic acid, which keeps it from clouding.
  7. Test again with red prussiate: no blue. Store in a brown, stoppered bottle in the dark. It keeps for some months, longer cold.

This is about a 27% solution, the standard strength. Call it Solution A.

Solution B (contrast). Take a third of Solution A and dissolve in it 0.3 g of potassium chlorate for every 55 ml. Mixing more B with A gives a more contrasty print. Chlorate is a strong oxidiser made by electrolysis of hot salt solutions (Chlorine and Bleach); some printers instead add 1–2 drops of 3% Hydrogen Peroxide and Oxygen Bleach to each coating.

Potassium oxalate developer

Dissolve 126 g oxalic acid in 400 ml hot water. Stir in purified potash (potassium carbonate) a spoonful at a time. It fizzes. Stop when one more spoonful no longer fizzes, about 138 g. Make up to 600 ml. This is a roughly 28% solution. It keeps forever, and gets better with use. Pour it back into its bottle after each session and let the sediment settle out.

The metal solutions

Silver nitrate: as in Photography.

Platinum (outline). The platinum salt for printing is potassium chloroplatinite, a red crystalline salt.

  1. Dissolve clean platinum in fresh aqua regia (Nitric Acid) on a warm sand bath, outdoors. It is slow: a gram takes hours.
  2. Evaporate nearly to dryness with a little Hydrochloric Acid two or three times to drive off the nitric acid. An orange-red syrup of chloroplatinic acid is left.
  3. Add a strong solution of potassium chloride: a yellow crystalline powder, potassium chloroplatinate, falls out. Wash it with a little cold water.
  4. This yellow salt must be reduced (given back some electrons) to the red chloroplatinite, by a mild reducing agent such as sulfur dioxide, under careful control. Too little does nothing; too much throws down black platinum powder and wastes it. This step is best learned beside an experienced chemist.

A 20% solution of chloroplatinite (10 g in 50 ml water) is Solution P. Every 10 g holds about 4.7 g of platinum.

Palladium is simpler. It dissolves in hot strong nitric acid, and the dried residue is turned into palladium chloride with hydrochloric acid. Dissolve 4.5 g palladium chloride and 3 g salt in 50 ml warm water: Solution Pd, sodium chloropalladite, a clear red-brown liquid.

The negative and the step tablet

Iron and salt papers need a negative with more contrast than silver bromide papers: thin, clear shadows and very dense highlights. Develop plates for these processes one and a half to two times as long as normal (Photography).

Make a step tablet to measure what your paper can do. Cut a strip of clear glass 4 × 25 cm. Glue onto it overlapping strips of thin tracing paper so that it has 12 steps: none, 1 layer, 2 layers … 11 layers. Print it on each new batch of paper beside a test negative.

  • The steps that print full black show where your exposure is longer than needed.
  • The first step that prints paper white shows the most density your paper can hold.
  • A good negative for this paper is one whose densest highlight looks, held against a window beside the tablet, about as dark as that first "white" step, and whose shadows look like the clear steps.

If your negatives are too thin, develop longer; if too dense, shorter. Write down the numbers.

Making a large negative

Small negatives make small contact prints. Three ways to get a big one:

  1. Use a big camera. A plate camera taking 18 × 24 cm or 20 × 25 cm dry plates (Photography) gives negatives ready to print. This is how most 19th-century platinum prints were made.
  2. Enlarge through a positive. Contact print the small negative onto a slow plate: a small positive. Put it in an enlarger, a camera run backwards (The Darkroom and the Enlarger): a bright lamp, a condenser lens to spread the light evenly, the positive, then the lens, projecting onto a large slow plate on the wall (Lenses). Develop it: a large negative. Adjust its contrast with development time.
  3. Paper negatives. Enlarge onto slow silver bromide paper to make a large positive, contact print that onto more paper to make a paper negative, and wax it to make it translucent, as for the calotype (Photography). Softer, but cheap.
Small negative contact Small positive on a slow plate Lamp Condenser lens Positive Projecting lens Large negative, 20 × 25 cm contact, sun Final print, same size
Fig. 2 Getting a large negative from a small one. The small negative is contact printed into a small positive. The enlarger projects it onto a large plate, making a large negative. That is contact printed onto iron-sensitised paper in the sun to give the final print, exactly its size.

Coating the paper

All of the iron papers are coated the same way, in dim tungsten or candle light (not daylight).

  1. Prepare the paper. If it contains chalk (a drop of vinegar on it fizzes), soak it 15 minutes in 1% oxalic or citric acid, rinse, and dry. Chalk spoils ferric salts. Pin the sheet flat on a board with a clean blotter under it, and pencil the edges of the image area.
  2. Measure drops into a small glass cup: see each process for amounts. For a 20 × 25 cm image, you need about 24 drops (about 1.2 ml) in total.
  3. Coat. Pour the pool along one edge and draw it across and back with a glass coating rod, held lightly at both ends, 6–8 passes, until the surface is evenly damp with no puddles. Or brush it on with a soft, wide brush, first lengthwise then crosswise.
  4. Dry in the dark for 10 minutes until the shine has gone, then over gentle warm air for a few minutes until bone dry. Damp paper gives muddy, weak prints and stains the negative.
  5. Print the same day. Most of these papers spoil in a day or two.
1. Coat with a glass rod 2. Expose in the sun 3. Develop 4. Clear and wash 24 drops for 20 × 25 cm; 6–8 passes; dry bone-dry glass, negative, paper, felt split back: lift half to check 3–15 minutes in sun potassium oxalate, one smooth pour; image appears at once weak acid baths, 5 minutes each, until the last stays colourless; then wash 20–30 minutes wash yellow paler clear
Fig. 3 Coating and printing. Sensitiser is drawn across the paper with a glass rod and dried. The negative and paper are pressed together in a printing frame and put in the sun. Half the back is lifted to check progress. The print is developed in a dish, cleared and washed.

Method 1: Salt prints, improved

The basic salt print is in Photography. Three improvements make it a finer and more lasting print.

  • Size with starch. Instead of plain salt water, salt the paper in 2% arrowroot or other clean starch cooked clear, with 2% salt. The image sits on the surface and is crisper.
  • Acidify the silver. Add 6 g citric acid to each 100 ml of the 12% silver nitrate. The coated paper keeps several days instead of hours, and the highlights stay cleaner.
  • Tone with gold before fixing. After the first wash, put the print in a borax gold toner: 1 litre water, 5 g borax, 10 ml of 1% gold chloride (gold dissolved in aqua regia, Nitric Acid). In 5–10 minutes the brick-red image turns purple-brown. Rinse, fix in 10% hypo for 5 minutes, wash an hour. Gold coats the silver grains and greatly slows fading.

Method 2: Van Dyke brown prints

A one-solution paper that is easy to mix and gives a rich brown image of silver.

  1. Solutions. A: 9 g ferric ammonium citrate (Blueprints and Cyanotypes) in 33 ml water. B: 1.5 g tartaric acid (from the tartar of wine casks, Citric and Tartaric Acid) in 33 ml water. C: 3.8 g silver nitrate in 33 ml water.
  2. Mix A and B, then stir C in slowly. Store in a brown bottle for 3 days before use. It keeps for months.
  3. Coat with about 2 ml per 20 × 25 cm (Van Dyke likes a generous coat), dry.
  4. Expose in sun for 5–15 minutes. The image prints out visibly in brown. Print until the shadows have a hint of metallic sheen.
  5. Develop in running water with a pinch of citric acid for 2–3 minutes: the yellow washes out.
  6. Fix in weak hypo: 3 g in 100 ml, for 3–5 minutes. Stronger fixer bleaches the image.
  7. Wash 30 minutes. The print darkens as it dries.

Gold toning before fixing improves colour and life.

Method 3: Kallitype

Ferric oxalate and silver: the cheap cousin of platinum.

  1. Sensitiser. Dissolve 10 g silver nitrate in 100 ml of ferric oxalate solution diluted to about 20% (3 parts Solution A to 1 part water). Store dark. Some cloudiness may settle out; use the clear liquid.
  2. Coat 24 drops per 20 × 25 cm, dry thoroughly.
  3. Expose in sun for 2–8 minutes. Only a faint image appears.
  4. Develop. Slide the print into the developer. The choice sets the colour:
    • 20% sodium acetate (vinegar neutralised with soda, boiled down): warm brown.
    • 10% borax with 5% Rochelle salt (wine tartar boiled with washing soda): cool brown-black.
    • Potassium oxalate, as for platinum: neutral black. Develop 3–5 minutes.
  5. Clear for 5 minutes in 2% citric acid, rinse.
  6. Tone (strongly advised): gold toner as above, or a palladium toner of a few drops of Solution Pd in 500 ml of 1% citric acid, 5–10 minutes.
  7. Fix 5 minutes in 5% hypo with a spoonful of ammonia water per litre. Fixer must not be acid; acid fixer eats kallitype images.
  8. Wash 30 minutes.

Method 4: Platinum and palladium prints

The finest and most permanent print.

  1. Count the drops for a 20 × 25 cm print:
Contrast wanted Solution A Solution B Solution P or Pd
Soft (for a contrasty negative) 12 0 12
Normal 9 3 12
Hard (for a flat negative) 4 8 12

Platinum alone gives cool black; palladium alone, warm brown-black; mix them for anything between. Palladium is cheaper and easier to make and gives smoother tones; most modern printers use mostly palladium.

  1. Mix just before coating, coat with the rod, dry.
  2. Expose in sun for 3–10 minutes, or 10–30 minutes under an arc or mercury lamp (Arc Lamps, Neon and Fluorescent Lights). A faint grey-orange image prints out; stop when the deepest shadows show clearly.
  3. Develop. Pour warm potassium oxalate (20–40 °C) over the print in one smooth sweep. The image appears instantly and completely. Rock 1–2 minutes.
  4. Clear the iron: three baths of 1 part strong hydrochloric acid to 60–100 parts water, 5 minutes each, or three of 2% citric acid. The last bath must stay perfectly colourless; yellow means iron is still coming out.
  5. Wash 20–30 minutes. No fixer is needed: there is no silver.

How to tell it worked

  • Highlights are clean paper white. A yellow or brown tint in the margins means the iron was not cleared, or the paper was fogged by light during coating.
  • Shadows are deep and rich, not grey or muddy. Weak shadows mean too short an exposure, damp paper, or a thin coat.
  • Even tone across flat areas such as sky: streaks mean uneven coating; spots mean dust, or metal touched the sensitiser.
  • The step tablet prints at least 8–10 distinct steps from black to white.
  • Clearing test: a drop of yellow prussiate solution on the margin of a cleared platinum print must not turn blue (blue means iron is left: clear longer).
  • For silver prints, a washing test: a drop of 1% silver nitrate on the margin stays colourless. A yellow-brown spot means hypo is left in the paper: wash longer (Photography).

Note Troubleshooting. Fog: grey all over → sensitiser contains ferrous iron (test with red prussiate), the paper saw daylight, or the coating dried too slowly. Add more Solution B. Image washes away in the developer → paper was damp, or the paper holds chalk. Acid-wash it. Grainy, speckled image → coating too dry when spread; use a little more liquid or a softer paper. Bronzed, metallic shadows in Van Dyke → overexposed; shorten. Kallitype fades in the fixer → fixer too acid or too strong. Add ammonia; use 5%. Print too flat → negative too thin for the process; use more Solution B, or develop negatives longer. Blotchy, brown-stained platinum print → clearing too short, or clearing bath exhausted.

Permanence

  • Platinum and palladium are noble metals: light, air, damp and pollution do not harm them. The print lasts as long as the paper. On good rag paper, washed free of iron and acid, that is many centuries.
  • Gold-toned salt prints and toned kallitypes last well in clean, dry, dark storage. Untoned silver prints slowly yellow and fade in polluted air, near rubber, sulfur, fresh paint and wood.
  • Cyanotypes fade a little in strong light (they recover partly in the dark) and are destroyed by alkali, including soap and lime (Blueprints and Cyanotypes).
  • Store prints flat, in folders of acid-free rag paper, cool and dry, away from light (Microfilm and Document Storage has more on archives). Never mount them on wood or cheap card.

Dangers

Danger Oxalic acid and all oxalates are poisons. A few grams can kill by stopping the heart and damaging the kidneys; they look like Epsom salts and sugar. Label every bottle clearly, keep it away from food and children, and wash hands after work. See Oxalic Acid.

  • Platinum salts cause a serious allergy. Repeated contact with chloroplatinates can bring on asthma, sneezing and skin rash that come back with every later exposure. Wear gloves, never breathe dust, and mix solutions with care. Palladium is milder but not harmless.
  • Silver nitrate stains and burns skin and can blind (Photography).
  • Aqua regia and the fumes of dissolving metals are deadly (Nitric Acid): outdoors, upwind, small amounts.
  • Potassium chlorate mixed with sugar, sulfur, charcoal or other organic matter can explode when struck or heated. Keep it as a dilute solution only, never dry.
  • Ferricyanide used for testing must never be heated or mixed with strong acid (Blueprints and Cyanotypes).

What this unlocks

Permanent prints for archives, maps and medical records (Libraries and Preserving Knowledge). Enlarging skills that lead to Microfilm and Document Storage and copying. A cheap Van Dyke or cyanotype print for every working copy, and a platinum print of what must last. The same light-driven iron chemistry is used to measure ultraviolet light with potassium ferrioxalate, still a standard in chemistry laboratories.

How it was first done

William Henry Fox Talbot made salted-paper prints in England from 1834 and announced them in 1839. Sir John Herschel, in 1842, published the cyanotype and the argentotype (silver with ferric ammonium citrate, the ancestor of Van Dyke and kallitype printing), having already studied light-sensitive platinum salts in the 1830s. William Willis patented the platinum process in 1873, improved it in 1878 and 1880, and founded the Platinotype Company in London in 1879 to sell ready-coated paper. Giuseppe Pizzighelli described a printing-out platinum paper in the 1880s. W. W. J. Nicol patented the kallitype in 1889. Brown printing papers of the Van Dyke type were sold from the 1890s.

Platinum paper was the choice of the finest photographers of the 1890s–1920s, but during the First World War platinum went into munitions and its price soared; palladium paper replaced it for a while, and by the late 1930s commercial platinum paper had gone. Photographers revived the process by hand from the 1960s onward.

Source: content/entries/knowledge/iron-printing.md