Part 9 · Health and Medicine
Pharmacy: Tablets, Capsules, Ointments and Inhalers
How to turn a weighed drug into a dose a patient can take safely — folded powder papers, rolled pills, tablets pressed in a steel punch and die, gelatin capsules dipped on pins, ointments and creams, suppositories, sterile eye drops, steam inhalers and spacers — and how to label, store and keep track of a medicine stock.
- Difficulty
- ●●●●●
- Time
- An hour for a batch of powders or ointment; a day for a batch of tablets; two days for capsules (dipping and drying); a week to build a hand tablet press
- Steps from zero
- 14 prerequisites →
This unlocks
—The full path from nothing — 14 steps before this one
- Fire
- Finding and Preparing Clay
- Foraging Wild Food
- Pottery
- The Kiln
- Medicinal Plants
- Lime
- Fermentation
- Lye and Potash
- Glass
- Distillation
- Acids, Bases and Testing
- Laboratory Glassware
- Making Medicines
- Pharmacy: Tablets, Capsules, Ointments and Inhalers
Do them roughly in this order. See it on the tech tree →
Why it matters
Making Medicines ends with a heap of white crystals and a balance. But nobody can swallow 0.6 g of bitter powder off a spoon three times a day for a week without spilling, gagging or forgetting. A baby cannot swallow at all. A cream that goes mouldy in a week does harm. Eye drops made with dirty water have blinded people.
The dose form — the shape a medicine takes when it reaches the patient — decides whether the right amount gets into the right place. Pharmacy is the craft of making those forms, and the discipline of labels, records and stock that stops the wrong medicine reaching the wrong person.
How it works
- Every dose must contain the same amount: accurate weighing and even mixing. A strong drug stirred carelessly into flour can put three times the drug in one dose as in the next.
- The form must release the drug. A tablet pressed too hard, or a pill dried to a pebble, can pass through the gut whole. Every batch is tested to show it breaks up in water at body heat.
- The form must keep. Dry forms keep a year or more; fat-only ointments for months; anything containing water spoils in days unless sterile or preserved.
- Anything for the eye must be sterile (Sterilising Instruments and Dressings).
Geometric dilution. To mix 1 g of a strong drug evenly into 99 g of filler, never tip the drug into the full heap. Grind the drug in a mortar with an equal volume of filler for a minute; add as much filler as is now in the mortar and grind again; keep doubling until all the filler is in. Six or seven doublings mix 1 part in 100 evenly. This one technique prevents most dosing errors in a small pharmacy.
What you need
| Item | Use | Source |
|---|---|---|
| Balance reading 0.1 g (better 0.01 g) | Everything | Making Medicines, Balances, Steelyards and Weighing Machines |
| Mortars and pestles, glass or glazed porcelain | Grinding, mixing | Stoneware and Porcelain |
| Glass or glazed tile slab 30 × 30 cm; flexible steel spatulas | Ointments, pills | Glass, Tiles and Clay Pipes |
| Sieves about 2 mm, 1 mm and 0.25 mm | Powders, granules | Brass wire or silk gauze (Iron and Brass Wire, Silk) |
| Water bath and The Thermometer | Melting bases gently | |
| Filler: dry starch, milk sugar, cane sugar | Bulk | The Great Staple Crops, Sugar, Dairy and Cheese |
| Binder: starch paste, gum arabic, honey, syrup | Pills, tablets | Gum arabic from acacia trees |
| Gelatin | Capsules, suppositories | Clean hide or bone (Glues and Adhesives) |
| Fats: lard, beeswax, wool fat; later petroleum jelly | Ointment bases | Oils and Pressing, Beekeeping, Petroleum and Refining |
| Cocoa butter | Suppositories | Tea, Coffee and Cocoa |
| Distilled or boiled water | Creams, eye drops | Distillation |
| Containers: amber glass, glazed pots, tins, paper | Packing | Bottles, Drinking Glasses and Glassware, Tins, Cans, Drums and Tanks, Paper |
Where to find it
- Starch: grate potatoes into water, let the starch settle, wash twice, dry. Pure starch squeaks between the fingers and turns blue-black with iodine (Iodine).
- Gum arabic: amber "tears" oozing from cut bark of acacia trees in dry savanna; dissolves slowly in cold water to a sticky mucilage.
- Gelatin: made like hide glue (Glues and Adhesives) but from fresh, clean pig or calf skin or bones, washed in many changes of water, extracted at 60–70 °C (never boiling), strained and set into a pale, nearly clear jelly.
- Wool fat (lanolin): skimmed from fleece scoured in hot soapy water (Toothpaste, Shampoo, Perfume and Cosmetics).
- Cocoa butter: press warm ground cacao nibs in a cloth bag (Tea, Coffee and Cocoa). Hard at room temperature; melts on the tongue.
Powders and powder papers
One weighed dose folded in a paper: accurate, keeps well, suits doses of 0.1–2 g.
- Grind the drug fine and sift it through the 0.25 mm sieve. If a dose is under about 0.2 g, bulk it with milk sugar or starch by geometric dilution so each paper holds at least 0.2 g.
- Weigh each dose onto its paper. For many papers, make a scoop that holds exactly one dose levelled off, and check it on the balance every fifth paper.
- Fold: papers about 10 × 12 cm. Fold one long edge over 1 cm; put the powder in the middle; bring the other edge up under the first fold; fold the pair over twice to a strip about 3 cm wide; turn the ends under to fit a box.
- For powders that take up damp, use paper rubbed with beeswax inside a plain one.
Good: every paper within 5 % of the dose; powder loose after a month. Bad: caked lumps, or weights varying by a tenth.
Pills
A pill is a small rolled ball of drug held by a sticky binder. Pills hide taste, but harden with age and may pass whole.
- Mass: grind the drug with a filler (liquorice root powder, flour or starch), then knead in binder (honey, syrup or gum mucilage) a few drops at a time until it is like stiff putty — not sticky, not cracking when bent.
- Roll it into an even rod under a flat board on a starch-dusted tile.
- Cut on a pill machine: two brass plates with matching rows of half-round grooves, usually 12 or 24, about 4–5 mm across. Lay the rod across the lower plate and roll the upper over it; the ridges cut equal pieces. Without one, cut at equal marks against a ruler.
- Round each piece under a flat wooden disc moved in small circles; dust with starch.
Pills of 0.1–0.3 g; larger are hard to swallow. Test: a pill dropped into water at blood heat (neither warm nor cool on the inside of the wrist, about 37 °C) breaks up within an hour; 20 pills each within 10 % of their average weight. Make fresh batches every few months.
Tablets and the hand tablet press
A tablet is powder squeezed hard in a steel die. Tablets keep for years, can be made by the thousand, and are all the same size: the backbone of a working pharmacy.
The punch and die
- Die: hardened tool steel (Steel), about 40 mm across and 20–25 mm thick, with a straight polished hole: 10 mm for 300–500 mg tablets, 8 mm for 150–300 mg, 6 mm for small ones.
- Punches: two rods turned on a The Lathe to slide in the hole by hand with only a few hundredths of a millimetre clearance, so powder cannot squeeze past. Flat or slightly cupped faces; a raised line across one face presses a score line for halving.
- Harden fully, temper only to pale straw (about 220 °C), and polish the hole and faces mirror-bright (Abrasives and Grinding Stones). Scratches make tablets stick.
The press
- Simplest: the lower punch stands on a stop under the die; fill, strike the upper punch once with a heavy mallet, lift the die off the stop and push the tablet out. The first compressed tablets were made this way.
- Lever press: a frame holds the die in a table; a lever of about 10:1 (Simple Machines) drives the upper punch, so a 50 kg pull gives about half a tonne. The lower punch rests on an adjusting screw that sets the fill depth and so the weight; a short second lever lifts it to eject the tablet. A screw press (Screws, Nuts and Bolts) works the same way.
- A 10 mm tablet needs about 0.5–1 tonne; a 6 mm one about a third of that.
Granules
Fine powder flows unevenly and traps air, so tablets split. Make granules first.
- Mix drug and filler by geometric dilution. For 1,000 tablets each weighing about 300 mg and holding 200 mg of drug: drug 200 g, starch or milk sugar 80 g (binder, disintegrant and lubricant make up the rest).
- Starch paste: 10 g starch stirred into 100 ml cold water, heated until it clears to a jelly, cooled.
- Wet the mix with paste until a squeezed handful holds its shape but crumbles when poked.
- Push it through the 2 mm sieve; dry in a thin layer at 50–60 °C until dry right through; sieve again through 1 mm.
- Toss in (don't grind) dry starch 5–10 %, which swells in the stomach and bursts the tablet apart, and a lubricant so tablets don't stick: talc (ground soapstone, Rocks and Minerals) 1–2 % or calcium stearate 0.5–1 %. Calcium stearate is the white scum soap makes with hard water (Detergents and Wetting Agents): stir soap solution into calcium chloride solution, filter, wash and dry the curd.
Pressing and testing
Set the screw so 10 tablets weigh exactly 10 doses, then check 10 tablets every 50.
| Test | How | Pass |
|---|---|---|
| Weight | Weigh 20 separately | Each within 5 % of average (over 250 mg) or 7.5 % (smaller) |
| Hardness | Snap between the thumbs | Clean snap, no crumbling |
| Wear | Shake 20 for 4 minutes in a closed tin | Lose under 1 %; edges whole |
| Break-up | Water at 37 °C, swirled now and then | Apart within 15 minutes |
Note Troubleshooting tablets. Top splits off as a cap → too much dust or air, granules too dry: re-granulate and sieve out fines. Sticks to the punch → more lubricant, drier granules, polish the punch. Too soft → more pressure or binder. Won't break up → less pressure, more starch. Weights vary → uneven granules: re-sieve.
Gelatin capsules
A capsule is a two-piece gelatin shell — a longer body and a shorter cap sliding over it. It hides taste, swallows easily, and needs no binder or pressing.
- Pins: rods of brass or steel turned with rounded ends and a very slight taper, polished mirror-smooth. For the common "size 0" (about 0.68 ml, 400–700 mg of powder): body pins about 7.3 mm, cap pins about 7.6 mm across. Set 10–20 upright in a wooden bar.
- Solution: soak 1 part gelatin in 2 parts cold water for an hour; melt in a water bath at 50 °C; skim bubbles. It should look like warm honey.
- Dip the pins, wiped with a barely oily cloth, to shell depth (about 20 mm for bodies, 11 mm for caps) for 5–10 seconds; withdraw slowly.
- Turn the bar pins-up and rotate it slowly for a minute while the film sets evenly.
- Dry in cool, still air, out of the sun, half a day to overnight, until no longer tacky.
- Strip with a twist; trim square on a mandrel to length (size 0: body 18–19 mm, cap 10–11 mm).
A good shell is clear, about 0.1 mm thick, and springs back when squeezed. Store in a jar with a bag of dry silica gel or quicklime (Water Glass (Sodium Silicate), Lime).
Filling board: a 12 mm hardwood board with rows of holes holding bodies upright, flush with the surface. Heap powder on, spread it into the bodies with a card, tap, spread again, scrape off, put on caps. Weigh 10: each within 10 %. Adjust the filler so one full capsule holds exactly one dose.
Ointments
An ointment is a drug in a greasy base that stays on the skin. With no water in it, it keeps for months.
- Simple ointment: 1 part beeswax melted with 4 parts lard in a water bath, stirred until cool. Heating the lard first for 2 hours with 1 % benzoin resin or a few cloves slows rancidity.
- Wool fat (up to a quarter of the base) helps it rub in. Petroleum jelly (Petroleum and Refining) never goes rancid: the best base of all.
Mixing in a drug (levigation): rub the fine, sifted powder with a little base on the slab under a flexible spatula with firm flat strokes until no grains can be felt, then work in the rest by geometric dilution. Gritty ointment irritates.
| Ointment | Recipe | For |
|---|---|---|
| Zinc ointment | Zinc oxide 15–20 % in simple ointment (Zinc and Brass) | Nappy rash, sore weeping skin |
| Sulfur ointment | Very fine sulfur 10 % adults, 5 % babies (Sulfur) | Scabies: spread from the neck down at night on three nights running; wash off 24 hours after the last. Wash all clothes and bedding the same day (Personal Hygiene). Safe in babies and pregnancy |
| Salicylic ointment | Salicylic acid 2 % (Making Medicines) | Thick scaly skin, dandruff |
| Plain base | Cracked hands and feet, chapped lips |
Fill clean glazed pots or tins from the bottom so no air is trapped. Keeps 6–12 months cool.
Creams
A cream is an emulsion — oil droplets held in water — so it rubs in and washes off. Make the borax–beeswax cold cream in Toothpaste, Shampoo, Perfume and Cosmetics and levigate the drug into it. Its water feeds mould, so without a preservative: use freshly boiled water and utensils, make only two weeks' supply in small pots, take it out with a clean spatula, and throw it away if it smells sour, separates or shows spots. 10–15 % glycerine (Soap) slows spoilage a little. When in doubt, use an ointment instead.
Suppositories
A dose in a solid that melts at body heat, put into the rectum: for patients who are vomiting or unconscious, small children who refuse medicine, constipation and piles.
- Cocoa butter melts at 31–34 °C. Melt it gently in a water bath until creamy with a few lumps left. Above about 36 °C it sets into a soft form that melts at room temperature.
- Glycerine–gelatin base (for hot climates): gelatin 14 g, glycerine 70 g, water to 100 g, heated in a water bath until clear. Plain, it relieves constipation within 15–30 minutes.
Suppository mould: two blocks of brass or aluminium (Metal Casting) screwed together, with torpedo-shaped cavities split down the middle, holding 1 g (children) or 2 g (adults) of cocoa butter. Leave it dry for cocoa butter, which shrinks and drops out; oil it lightly for gelatin. Stir the fine drug into the melted base, pour slightly overfilled, let set 30 minutes, scrape level, open. Without a mould, knead grated cocoa butter with the drug, roll a rod on a starch-dusted tile, cut equal lengths and point one end. Wrap each; keep below 25 °C.
Eye drops
Eye drops must be sterile, perfectly clear, and about as salty as tears (isotonic, 0.9 % salt) so they don't sting. The dropper is in Medical Instruments.
- Use freshly distilled water (Distillation), or water boiled 10 minutes and filtered.
- Dissolve the drug and enough salt for the right saltiness. Plain 0.9 % salt water (9 g pure salt per litre) is the standard wash for grit and chemicals in the eye.
- Filter until perfectly clear.
- Fill clean dark 10 ml bottles, cap them, and sterilise the filled bottles: steam at 121 °C for 15 minutes, or, for drugs that stand it, 30 minutes in boiling water.
- Label with the date made and the date opened.
Without a preservative, an opened bottle is for one patient and is thrown away after 24 hours; with a proper preservative, after 4 weeks.
Danger Eye drops made wrong blind people. Germs in the water can destroy an eye in two days; a too-strong caustic burns the cornea. Silver nitrate for newborn eyes must never be stronger than 1 % (Silver Nitrate and Silver Salts). Work from a written recipe, have a second person check every weighing, and never use a cloudy bottle.
Inhalers
The steam inhaler
Warm moist air loosens thick mucus and soothes a sore throat. An inhaler jug is safer than a bowl under a towel: a lidded glazed stoneware or pewter jug of about 1 litre (Pottery, Tin and Pewter), with a curved mouthpiece tube about 1.5 cm across and 12 cm long through the lid, and a small air hole. Half fill it with water at 60–70 °C, stand it in a bowl on a table, and breathe in through the mouthpiece and out through the nose for 5–10 minutes. For adults, a few drops of eucalyptus or pine oil, or a teaspoon of tincture of benzoin, may be added. Honestly, steam eases the feeling of a blocked nose, but it has not been shown to shorten colds or chest infections.
Danger Steam inhalation is a common cause of serious scalds in children. Never use a bowl and towel for a child, or leave a child with hot water. No menthol, eucalyptus or camphor under 2 years: they can stop a baby's breathing. A child with croup needs calm, upright sitting and watching (Emergencies).
The spacer
A pressurised metered-dose inhaler (a canister that sprays a measured puff of asthma medicine) needs propellant gas and precision valves; a rebuilding community will not make these until it has an advanced chemical industry (Pressure Vessels and Valves). But salvaged or traded inhalers work far better with a spacer, because most of a puff sprayed straight into the mouth hits the throat. A spacer holds the puff as a cloud to be breathed slowly.
- Make: a tube 5–7 cm across and 15–20 cm long (about 500 ml), of tinplate soldered at the seams (Sheet Metal and Rolling) or thick glass for adults. One end grips the inhaler's mouthpiece in a leather or rubber collar (Rubber); the other has a smooth rounded mouthpiece, or a soft mask for children under about 4. Metal holds no static charge, which makes medicine stick to plastic spacers.
- Use: shake the inhaler, fit it, seal the lips (or mask), press once, and breathe slowly in and out 5 times (or one deep breath held 10 seconds). Wait 30 seconds before the next puff.
- Clean monthly in warm soapy water and let it drip dry.
Labels, records and stock
Most deaths from medicines in small pharmacies come from mix-ups, not bad chemistry. Label every container when you fill it. A dispensing label carries:
- Medicine and strength ("Quinine sulfate tablets, 300 mg").
- Dose in words: "Take ONE tablet THREE times a day with food for SEVEN days."
- Patient's name and the date.
- Batch number and "use before" date.
- Warnings: KEEP OUT OF REACH OF CHILDREN, FOR EXTERNAL USE ONLY, SHAKE THE BOTTLE, POISON.
For people who cannot read, draw a rising sun, high sun and moon with the number of tablets under each (Writing and Numbers); explain aloud and have the patient repeat it back.
- Batch record: date, recipe, weight of every ingredient, who weighed, who checked, number of units made, test results. Put the batch number on every label.
- Stock book: a page per medicine — date, amount in or out, to whom, balance. Count the shelf against the book monthly.
- First to expire, first out. Store below 25 °C, dry, dark, off the floor, away from food.
- Lock up poisons and strong drugs with their own register, signed at every use (Making Medicines). Put external medicines and poisons in ribbed bottles you can tell by touch in the dark.
- Shelf life of home-made forms kept well: powders, tablets, capsules 1–2 years; ointments 6–12 months; liquid mixtures 1–2 weeks; unpreserved creams 2 weeks. Destroy out-of-date stock.
How to tell it worked
- Dose weights agree within the limits above; tablets, pills and capsules break up at 37 °C in the times given.
- Ointments feel smooth, with no grit, on the back of the hand; eye drops stay perfectly clear.
- Patients take the right amount: ask them to show you how they will take it.
Note Troubleshooting. Powder papers cake → dry the powder over quicklime first; use waxed papers. Pills pass whole → too much gum or too old; use honey, make smaller batches. Capsules crack → too dry: leave them a few hours in a jar with a damp (not wet) cloth. Ointment sweats oil → too little wax for the climate; use 1 part wax to 3. Suppositories soft and greasy → the cocoa butter was overheated. Cream goes mouldy → water or tools not boiled, or batch too big.
Dangers
Danger Concentrated drugs are poisons. A heap of pure drug may hold a hundred lethal doses. Weigh strong drugs with a second person watching, and clean the balance, mortar and slab between drugs.
- Children die from swallowing tablets that look like sweets. Use stiff lids; never call medicine sweets.
- Drug dust is breathed in while grinding: grind under a damp cloth or wear a cloth mask.
- Burns: melt bases over warm water, never straight over the fire.
- Look-alike labels: never shelve two similar-looking medicines side by side.
What this unlocks
Reliable dose forms let every drug in Making Medicines, Sulfa Drugs, Penicillin and Antibiotics Beyond Penicillin be given at the right strength to adults and children. The tablet press is a small cousin of the coin press (Presses, Punches and Dies) and also makes salt tablets for Oral Rehydration. Sterile eye drops lead to sterile injections (Syringes and Hypodermic Needles, Intravenous Fluids). A well-kept stock book is the start of the Running a Hospital pharmacy.
How it was first done
The Egyptian Ebers Papyrus (about 1550 BC) lists pills, ointments, suppositories and medicines breathed in as vapour. Greek and Roman physicians rolled pills, and the apothecary's pill tile and pill machine were standard by the 1700s. In Paris, François Mothes and Joseph Dublanc patented the soft gelatin capsule in 1834, and Jules Lehuby the two-piece hard capsule in 1846. In 1843 the English inventor William Brockedon patented a punch and die, struck with a mallet, for "shaping pills, lozenges and black lead by pressure"; by 1900 the machine-pressed tablet had largely replaced the pill. Earthenware inhaler jugs such as the Nelson inhaler were sold from the 1860s. Riker Laboratories in the United States introduced the pressurised metered-dose inhaler in 1956; spacers came into wide use in the 1970s and 1980s.
Source: content/entries/health/pharmacy.md