◆ Rebuild

Part 5 · Cloth and Clothing

Bags, Backpacks, Wallets and Luggage

How to cut, stitch, mould and rivet leather and canvas into the things people carry — belt pouches, purses and wallets, knife sheaths and quivers, satchels and handbags, saddlebags, rucksacks and framed backpacks, suitcases and travel trunks — and how to make them strong where they take the strain.

Difficulty
●●●●●
Time
A belt pouch in an evening; a wallet or sheath in a day; a satchel in 2–3 days; a framed backpack in about a week
Steps from zero
6 prerequisites →

You need first

Hides and LeatherSewing, Needles and Thread

This unlocks

—
The full path from nothing — 6 steps before this one
  1. Cordage and Rope
  2. Stone Tools
  3. Hunting and Trapping
  4. Spinning and Weaving Cloth
  5. Hides and Leather
  6. Sewing, Needles and Thread
  7. Bags, Backpacks, Wallets and Luggage

Do them roughly in this order. See it on the tech tree →

Why it matters

Tools, food, coins, knives and papers all have to be carried. A good pack lets a fit adult carry a quarter of their body weight all day without injury. A bad one cuts into the shoulders, tears at the strap, or spills its load in a river.

All bags use the same few skills: cutting leather or canvas cleanly, stitching a seam that will not unravel, finishing the edges, and fixing straps so the pull spreads over a wide area instead of tearing one hole. This chapter teaches those skills once, then goes through each object. Tanning is in Hides and Leather, stitches in Sewing, Needles and Thread, canvas in Ropewalks and Sailcloth, buckles in Buttons, Buckles, Hooks and Zips, and sacks and crates for goods in Sacks, Boxes, Crates and Packaging.

How it works

  • Strain gathers at corners and anchors. A loaded bag pulls hardest where the strap joins the body and at the bottom corners. Each of these needs a reinforcing patch, extra stitching or a rivet, with the load spread over 5–10 cm of seam.
  • Seams in shear, not in peel. A seam is strong when the load slides the layers past each other, and weak when it pulls them apart like opening a book. Sew strap anchors flat onto the bag face so the strap pulls along the stitches.
  • Leather has a direction. A hide is firmest along the backbone and stretchy at the belly and legs. Cut straps and anything that must not stretch parallel to the backbone, from the back of the hide (the "bend"). Use belly leather for linings and gussets.
  • Weight belongs close to the spine and on the hips. A load hanging away from the back levers you backwards. Packed close and high, it sits over your feet. On a long carry the hips should take most of it: a broad hip belt lets the legs carry the load directly.

What you need

Item For Notes
Bark-tanned leather Everything firm Only vegetable-tanned leather can be wet-moulded and burnished (Hides and Leather)
Soft leather Linings, purses, gussets Brain-tanned, or thin oiled bark-tanned
Canvas Rucksacks, saddlebags, cases 350–500 g/m² hemp or flax (Ropewalks and Sailcloth)
Thread All seams 4–6-ply linen or hemp, well waxed (Sewing, Needles and Thread)
Knife, awl, two blunt needles Cutting and stitching Keep the knife stropped (Axes, Chisels, Knives and Planes)
Burnisher Edges A smooth bone or hardwood stick
Mallet, punches, rivets Holes and hardware Iron tube punches 3–10 mm; copper rivets and burrs (Copper Smelting)
Buckles and rings Closures Forged iron or cast brass (Blacksmithing, Zinc and Brass)
Wood Frames, trunks Ash or hazel for bent frames; pine boards for trunks

Leather thickness decides the job. Measure a cut edge with a ruler:

Thickness Uses
0.8–1.2 mm Wallet pockets, linings, purses
1.5–2.5 mm Bag bodies, gussets, pouches, quivers
3–4 mm Straps, belts, sheaths, satchel flaps
4–5 mm Saddlebags, strap anchors, sheath welts

One cattle hide gives about 4 m² of leather, enough for several satchels; a goat or deer hide gives a few wallets and pouches. For frames, cut straight, knot-free ash or hazel green and split it, so the grain runs the full length (Basic Woodworking). Copper and brass hardware does not rust and stain the leather; iron is fine if greased. Padding is Felt or folded wool cloth.

Basic leatherwork

A · SADDLE STITCH groove holes 3–5 mm apart, 3–5 mm from the edge two threads cross in every hole one broken stitch cannot unravel the seam B · SKIVING not skived: a double-thick lump skived: both ends shaved to a taper flat joint, same thickness C · COPPER RIVET AND BURR rivet head burr (copper washer) end cut 1.5–2 mm long, hammered into a dome over the burr D · BUCKLE AND KEEPER buckle frame tongue keeper holds the loose end holes 2–2.5 cm apart
Fig. 1 Four basic leatherworking skills. A stitch line is grooved and pierced, then saddle stitched with two needles so that one broken stitch does not unravel. Edges are thinned by skiving where layers overlap. A copper rivet is peened over a burr. A strap passes through a buckle and is held by a keeper.

Cutting

  1. Make patterns first from bark, stiff paper or thin board, and test them by folding cloth into the shape.
  2. Cut on a hard, smooth surface (an end-grain block) with the blade upright, pulling the knife towards you in one long stroke. On curves, turn the leather, not the knife.
  3. Straps: cut one straight edge, score a parallel line with dividers set to the width, and cut along it. For many straps make a strap cutter: a wooden block with a fence and a blade fixed across it at the chosen width; pull the leather through.

Stitching

  1. Mark the stitch line 3–5 mm from the edge with dividers, one point running along the edge. On firm leather cut a shallow groove along it with a gouge, so the thread sits below the surface and does not wear.
  2. Make the holes with a stitching fork (4–6 flat, sharpened teeth 3–5 mm apart in a handle, struck with a mallet) or one by one with the awl.
  3. Hold the work in a stitching clam: two wooden staves 80–90 cm long, joined at the bottom and gripped between the knees. Both hands are then free.
  4. Saddle stitch with a needle on each end of the thread (Sewing, Needles and Thread), every stitch pulled equally tight. Spacing: 2.5–3 mm on wallets and purses, 4–5 mm on bags and straps. Finish by going back through the last 2–3 holes.

Thinning and edges

  • Skiving is shaving leather thinner from the flesh side with a very sharp, flat-held knife. Skive every edge that is folded or overlapped, so three layers together are no thicker than two, and taper strap ends before folding them round a buckle.
  • Finishing an edge: round the corner of the cut with a gouge, rub it smooth with sandstone (Abrasives and Grinding Stones), wet it, rub in a little beeswax or tallow, and burnish — rub hard and fast with the bone stick until it is dark and glassy. A burnished edge does not fray and sheds water.

Wet moulding

  1. Soak bark-tanned leather in cool water until bubbles stop (1–5 minutes).
  2. Wrap it in a damp cloth for an hour or two until the surface returns almost to its dry colour. This cased leather holds any crease or press of the fingers.
  3. Press it round the object or a wooden form with fingers and a smooth bone.
  4. Dry slowly at room temperature for a day or two. Above about 50 °C wet leather shrinks and cracks.

Dipped for a minute in water at 60–80 °C, shaped and dried, wet leather shrinks and sets hard as horn. This is cuir bouilli ("boiled leather"), for bottle cases, sheaths and helmets. It is brittle in hard frost; test a scrap first.

Hardware

  • Rivets: push a flat-headed copper rivet through a punched hole from the face, slip a copper washer (burr) over the shank on the back, press it down with a hollow punch, cut the shank 1.5–2 mm above the burr, and hammer the end into a dome. Two rivets plus stitching anchor a strap.
  • Buckles for straps 2–4 cm wide: a rectangular or D-shaped frame of 4–5 mm iron or brass rod with a tongue. Fold the strap round the bar, punch a slot for the tongue, and stitch or rivet. A keeper — a loop of thin leather behind the buckle — holds the loose end. Punch strap holes 3–5 mm across, 2–2.5 cm apart.

Small things

Belt pouch and drawstring purse

Drawstring purse: a circle of soft leather 25–30 cm across, with holes punched in pairs every 2.5 cm, 2 cm in from the edge, and a thong threaded through and pulled tight. It holds coins, seeds or fire kit.

Belt pouch with flap:

  1. Cut a back 12 × 26 cm (the top 10 cm is the flap), a front 12 × 14 cm, and a gusset strip 4 cm wide as long as the front's sides and bottom plus 2 cm.
  2. Cut two vertical slits in the back, 3 cm apart and 1 cm shorter than the belt is wide, for the belt to pass through.
  3. Saddle stitch the gusset to the front, then to the back, flesh sides in, so the seams sit on the outer edge and can be burnished.
  4. Fold the flap over a rod while the leather is cased so it keeps the bend, and close it with a toggle and loop or a strap and buckle.

A good pouch stays shut when you run and when you hang it upside down.

Wallet

  1. Size it from the largest note or paper it must hold, folded once: the closed wallet is 1 cm wider and taller than that, usually about 11–12 × 9–10 cm (21–24 cm wide when open).
  2. Cut an outer piece of 1.2–1.5 mm leather and two pocket pieces of 0.8–1 mm, each half the width. For card pockets, cut strips that overlap like steps 1.5 cm apart.
  3. Skive every edge where layers stack. Glue the layers at the edges with hide glue (Glues and Adhesives) to hold them, and stitch round the outside at 2.5–3 mm, leaving the pocket tops open.
  4. Fold it while cased over a rod 1 cm thick so the spine does not crack. Burnish the edges.

A coin purse is two pieces 9 × 8 cm sewn round three sides, with a button flap.

Knife sheath

The secret of a safe sheath is the welt: a strip of 3–4 mm leather sewn between the two layers along the cutting edge, so the blade rests against leather, not against the stitches.

  1. Fold 3–4 mm leather along the back of the blade. Mark round it, 1.5 cm outside the edge and 1 cm beyond the tip, plus a belt loop 8–10 cm above the mouth.
  2. Cut a welt 1–1.5 cm wide to the shape of the edge side (two stacked for a long blade). Glue it between the layers and saddle stitch through all three, 5–7 mm from the edge.
  3. Case the sheath, push in the knife wrapped in thin cloth, and press the leather round the handle and guard. When dry, the knife clicks in and is held by the moulding.
  4. Punch a 3 mm drain hole at the tip. Fold the belt loop over and rivet it.

Test: shake the sheath upside down — the knife must stay in. Draw it twenty times — no stitch may be cut. For an axe, a folded leather mask over the bit held by a strap and stud does the same job.

Quiver

For 12–20 arrows (Bow and Arrow), make a tube 8–10 cm across. A back quiver is 10–15 cm shorter than the arrows so the fletchings can be grasped; a hip quiver hangs from the belt at an angle. Roll 1.5–2.5 mm leather round a pole and stitch the overlap, or use a birch-bark tube (Baskets and Containers) covered with hide. Fit a bottom disc of 4–5 mm leather or a wooden plug, with a pad of grass or wool inside so the points do not cut through. Sew a strap 4–5 cm wide near the top and bottom, to be worn across the chest; a hide flap keeps rain off the feathers.

Satchel and handbag

PATTERN (35 × 27 × 9 cm SATCHEL) 35 cm back 27 cm bottom 9 cm flap 22 cm one piece; dashed lines are folds front 35 × 27 cm 2gussets 9 × 27 cm shoulder strap 3–4 cm wide, 110–140 cm long, from the bend ASSEMBLED strap flap anchor box-X stitch + 2 rivets gusset buckle straps front Round every corner to 2–3 cm:sharp corners wear through first.
Fig. 2 A satchel pattern and the finished bag. The flap, back and bottom are one long piece; the front and two gussets close the box. The shoulder strap is anchored to the gussets with box-X stitching and rivets, and the flap fastens with straps and buckles.

A satchel is a box-shaped bag with a flap on one strap: the school bag, the postman's bag. A handbag is a smaller version with short handles, usually lined.

  1. Size. A school satchel is about 35 cm wide, 27 cm tall and 9 cm deep; a shoulder bag 25 × 20 × 7 cm; a handbag 22–28 cm wide.
  2. Main piece, from 2–3 mm leather, in one length: flap + back + bottom. For the satchel: 35 × (27 + 9 + 22) ≈ 35 × 58 cm. Cut a front 35 × 27 cm and two gussets 9 × 27 cm.
  3. Round the corners of flap and front to a 2–3 cm radius; sharp corners wear through first.
  4. Strap anchors. Stitch a 6 × 8 cm reinforcing patch inside the top of each gusset. Sew a 4 cm strap tab through it in a box with an X across, plus two rivets.
  5. Assemble. Stitch the gussets to the front, then to the back, with 4–5 mm saddle stitch. Soft leather: sew inside out and turn the bag. Firm leather: sew with edges outside and burnish them.
  6. Closures: two short straps with buckles on the front, meeting two straps on the flap.
  7. Strap: 3–4 cm wide, 110–140 cm long, adjustable through a buckle, with a pad of felt 6–8 cm wide where it crosses the shoulder.
  8. Lining (handbags): sew the same pieces in linen into a bag and hem it into the mouth.

A frame bag (doctor's bag, clasp purse) has its mouth sewn onto two hinged jaws of strip iron or brass with a snap catch.

A good satchel stands on its own bottom when empty, its flap lies flat, and its anchors do not move when 15 kg hangs from the strap for a day.

Saddlebags

Saddlebags are two matched bags joined by a broad yoke that lies across a riding saddle (Leatherwork and Harness-Making) behind the rider. (Panniers for pack animals are in Pack Animals.)

  1. Make each bag like a satchel, about 30 × 28 × 11 cm, of 4–5 mm leather or doubled canvas, with a full-width flap and two buckled straps. Each carries 3–7 kg; more bounces and galls the horse, and it all counts against the horse's weight limit (Riding and Training Horses).
  2. Join them with a yoke of thick leather 25 cm wide and 40–50 cm long, stitched and riveted to the back of each bag, with slots for the saddle's tie thongs.
  3. Add a thong at the bottom of each bag to tie to the girth, so the bags do not swing at a trot.
  4. Balance the two sides within 0.5 kg, and let nothing hard lie against the horse.

The same pattern, smaller, hangs either side of a The Bicycle rack.

Rucksacks and backpacks

SIDE VIEW, LOADED bag on frame shoulder strap 5–7 cm, padded hip belt 8–10 cm wide, carries two-thirds of the load bent ash frame follows the spine torso 40–52 cm Measure from the bony knob at the base of the neck down to the tops of the hip bones. FRAME FROM BEHIND crossbar sidebar back band strap hip belt buckles in front
Fig. 3 A framed backpack in use. The frame holds the load close against the spine. Shoulder straps leave the frame at shoulder height; the broad hip belt rests on the bones of the hips and carries most of the weight. Torso length is measured from the bony knob at the base of the neck to the top of the hip bones.

A rucksack (German for "back sack"; also knapsack) is a soft sack with two shoulder straps. A backpack in the strict sense has a frame that holds its shape and puts the weight on the hips.

Rucksack

  1. Body: a tube of 400–500 g/m² canvas. A tube 90 cm round (28.6 cm across) and 60 cm tall holds about 38 litres: 640 cm² × 60 cm ≈ 38,000 cm³. A day bag is 20–30 L; a long journey 50–70 L.
  2. Bottom: an oval of doubled canvas or 3 mm leather, sewn in with a flat-felled seam (Sewing, Needles and Thread). Add 1 cm to every edge for seams.
  3. Mouth: 8–12 eyelets 5 cm below the top with a drawstring.
  4. Lid: a flap sewn to the back, reaching 15 cm down the front, with two straps and buckles and a pocket for small things.
  5. Shoulder straps: 5–7 cm wide over the shoulders, padded with 1–1.5 cm of felt in a leather or canvas tube, narrowing to 2.5 cm below. Sew the tops onto the back 5–8 cm apart, just below the top, through a reinforcing patch; the lower ends to the bottom corners through buckles.
  6. Waterproof it by rubbing in beeswax melted with an equal weight of linseed oil and warming it in the sun (Oils and Pressing, Raincoats, Oilskins, Umbrellas and Rubber Boots).

Framed backpack

This improves on the pole-and-crossbar pack frame in Baskets and Containers with a curve that fits the back and a hip belt.

  1. Measure the torso from the knob at the base of the neck (the vertebra that sticks out when you bow your head) down the spine to the level of the tops of the hip bones. Most adults measure 40–52 cm. The shoulder bar sits at the top of this length, the hip belt at the bottom.
  2. Side bars: two strips of ash or hazel 3 × 2 cm and 60–70 cm long. Steam or boil them for an hour, bend them over a form into a gentle S that follows the spine, and leave them tied to dry for a week.
  3. Crossbars: three or four, 30–35 cm long, set into mortises or lashed with wet rawhide (Doors, Windows and Joinery, Hides and Leather).
  4. Back band: canvas or leather 15 cm wide laced tight across the frame on your side, so the bars never touch you and air can pass.
  5. Hip belt: 8–10 cm wide over the hip bones, padded with felt, narrowing to a 4 cm strap and buckle in front. It should carry two-thirds or more of the load.
  6. Shoulder straps from the top crossbar to the bottom of the frame; on heavy packs a chest strap across the breastbone stops them sliding off.
  7. The bag: a canvas sack with a lid, laced to the frame. A tent, firewood or a carcass can be lashed to the bare frame.

Fit it: with the hip belt tight on the hip bones, the shoulder straps should just touch the shoulders. If the weight is on the shoulders, the frame is too short; if the straps lift off, it is too long.

Suitcases and travel trunks

Travel trunk — a strong box for journeys by ship, cart or rail (boxes in general are in Sacks, Boxes, Crates and Packaging):

  1. Box: pine boards 10–15 mm thick, dovetailed or nailed at the corners (Doors, Windows and Joinery). A typical trunk is 90 × 50 × 50 cm; a cabin trunk to slide under a ship's bunk is 90 × 50 × 35 cm.
  2. Lid: a shallow box 10–15 cm deep on two strap hinges. A flat lid lets trunks stack.
  3. Cover the outside with canvas or thin leather glued with hide glue or flour paste, then oil or paint the canvas.
  4. Reinforce with hardwood slats nailed round the box and sheet-iron or brass caps on every corner (Sheet Metal and Rolling).
  5. Fit leather end handles riveted through metal plates, a hasp and padlock or box lock (Locks and Keys), and a lift-out tray inside.

Suitcase — the same idea built light: a frame of thin wood strips with sides of thin board (Plywood, Veneer and Boards), or stiff leather alone, about 65 × 42 × 18 cm, hinged along one long side, with a central handle and two catches or straps. A good suitcase weighs 3–5 kg empty.

How to tell it worked

  • Stitch line: straight, evenly spaced, the same slope and tension on both faces; no stitch pulling through the edge.
  • Edges: smooth, rounded and glassy, with no fuzz or splitting layers.
  • Load test: fill the bag with twice its working load and hang it by the strap for a day. Nothing may stretch, creak or shift at the anchors.
  • Rain test: pour a cup of water over the closed bag; the inside stays dry.
  • Walk test: carry the loaded pack 5 km. No red marks, rubbing or numbness at shoulders or hips.

Note Troubleshooting

  • Stitches wear through → groove the stitch line deeper and use heavier thread.
  • Strap stretches thin → cut across the hide or from the belly. Recut it along the backbone.
  • Moulded leather cracked → dried too fast or too hot. Dry at room temperature; feed with tallow.
  • Pack pulls you backwards → heavy things are too far from your back or too low. Repack; tighten the straps.

Dangers

Danger Knives and awls. Most leatherworking injuries are a slipping knife or an awl driven through the hand. Cut on a firm board with your free hand behind the blade, never in front of it. Hold work in a clamp, not in your palm, when piercing. Keep blades sharp: a dull blade needs force and slips.

  • Overloading. More than about a quarter of body weight for adults, or a fifth for children, on long carries strains the back, knees and feet. Tight shoulder straps with no hip belt can press on the nerves below the collarbone and numb the arms ("rucksack palsy"). Loosen the straps at once if your fingers tingle.
  • Hot water for cuir bouilli scalds; handle the leather with tongs.

What this unlocks

Bags carry the kit of the surveyor (Surveying and Levelling), the medic (The First Aid Kit) and the The Post. Packs and frames lead to Tents, Sleeping Bags and Camping Gear for long journeys. A The Sewing Machine strong enough for leather turns bag-making into a trade, and zips from Buttons, Buckles, Hooks and Zips and rubberised cloth from Rubber lead to the modern bag.

How it was first done

The oldest known backpack belongs to Ötzi, the man who died in the Alps about 5,300 years ago: a U-shaped hazel rod with two larch boards, very like a pack frame, which probably held a bag of hide or fur. He also carried a hide belt pouch holding a flint scraper, a drill, a bone awl and tinder fungus, a hide quiver with arrows, and a knife sheath plaited from lime bast. Leather bags and purses appear in Egyptian tombs and Roman forts, and Roman soldiers slung their kit on a carrying pole. The word wallet first meant a traveller's food bag; folding cases for paper money spread with banknotes from the 1600s. In 1858 the Paris trunk-maker Louis Vuitton introduced flat-topped, canvas-covered trunks that stacked in ships' holds and luggage vans, and the light, hand-carried "suit case" became common with rail travel in the late 1800s. Around 1908 the Norwegian Ole F. Bergan patented a backpack with a curved metal frame.

Source: content/entries/textiles/bags-and-luggage.md