Part 3 · Metals
Sheet Metal and Rolling
Turn bars of iron and ingots of copper into thin, even sheet — first by hand hammering, then with a water-powered trip hammer and a rolling mill — and cut, fold, seam and rivet it into buckets, pipes, tanks and boilers.
- Difficulty
- ●●●●●
- Time
- Days to hammer a sheet by hand; a season to build a water-powered hammer or rolling mill; an afternoon to make a bucket once you have sheet
- Steps from zero
- 15 prerequisites →
This unlocks
Boilers and Pressure VesselsHorns, Pianos, Organs and AccordionsMops, Dustpans and Cleaning ToolsKitchen Utensils and GadgetsPots, Pans and KettlesCorrosion and Its PreventionMetal Spinning and RaisingMetal Pipes and TubesPresses, Punches and DiesTins, Cans, Drums and TanksEnamel on MetalThe full path from nothing — 15 steps before this one
- Fire
- Cordage and Rope
- Stone Tools
- Finding and Preparing Clay
- Finding and Identifying Ores
- Hunting and Trapping
- Basic Woodworking
- Charcoal
- Hides and Leather
- The Wheel and Axle
- Bellows
- Gears
- Iron (the Bloomery)
- The Waterwheel
- Blacksmithing
- Sheet Metal and Rolling
Do them roughly in this order. See it on the tech tree →
Why it matters
A bar of iron makes tools; a sheet of iron or copper makes containers. Buckets, cooking pots, kettles, lanterns, funnels, stovepipes, gutters, roofs, water tanks, cans for Canning and Bottling and the cylinders and boilers of the The Steam Engine are all sheet or plate, bent and joined. Sheet also feeds other trades: strips slit from it become nail rod (Nails, Rivets and Wire Fasteners) and wire (Copper Wire); discs cut from it become coins (Money, Trade and Record-keeping); thin copper and zinc sheet make the plates of the The Battery.
Making sheet by hand is slow and uneven. The great leap is to let a The Waterwheel do the hammering — and then to replace the hammer with a pair of rolls that squeeze the metal into even sheet many times faster. The rolling mill is one of the foundations of industry: the same machine with grooved rolls makes bars, rods, rails and beams.
How it works
Squeezing makes metal thinner, longer and wider. Every hammer blow or pass between rolls pushes the metal sideways. A cross-peen hammer (a hammer with a narrow, rounded wedge on one face) pushes the metal mainly at right angles to its edge, so you can steer which way it spreads. Rolls push it mainly lengthways.
Working hardens metal. Copper, brass and cold iron get stiffer and springier the more you hammer or roll them cold — this is work hardening. Keep going, and they crack. Annealing — heating to a dull red and cooling — makes them soft again.
- Copper and brass: hammer or roll cold; anneal (dull red, about 600 °C, then quench in water or let cool) whenever the metal feels springy, roughly every time its thickness has dropped by a third.
- Iron: work it hot (orange to yellow), so it never hardens. Thin iron loses heat in seconds, so it is worked in stacks, called packs.
- Lead and tin: soft enough to roll cold without annealing.
Rolls do the same thing as a hammer, continuously. Two heavy cylinders turn toward each other. The metal is gripped by friction and dragged through the gap, which is a little narrower than the metal. Each pass can reduce hot iron by roughly 10–25% of its thickness, copper cold by 10–20%. The rolls must not bend, so they are thick and short, and the frame holding them must be massive.
What you need
| Item | Notes |
|---|---|
| Forge, anvil, tongs | See Blacksmithing. A large, smooth, flat anvil face matters most |
| Hammers | Cross-peen hammer (1–1.5 kg) for spreading; flat planishing hammer with a polished, very slightly domed face for smoothing; wooden and rawhide mallets for bending |
| Stakes | Small anvils of various shapes on a spike that fits a hole in a stump: a straight sharp edge (hatchet stake), a round horn, a flat square head |
| Snips and shears | Below |
| Folding bars | Two straight hardwood boards or iron bars 60–100 cm long, clamped together with the sheet between |
| Mandrels | Round wooden logs or iron bars for rolling cylinders and pipes |
| Scriber, dividers, straight edge | For marking out; a long cord and nail for big arcs |
| Metal | Iron bar from Iron (the Bloomery); copper ingot from Copper Smelting; brass from Zinc and Brass |
| For powered work | A The Waterwheel of several kW, oak beams, iron for hammer heads, rolls and gears; for iron rolls, The Blast Furnace and Cast Iron |
Common thicknesses:
| Article | Sheet thickness |
|---|---|
| Tinplate cans | 0.25–0.4 mm |
| Buckets, stovepipe, lanterns | 0.5–0.8 mm |
| Copper kettles and pans | 0.8–1.2 mm |
| Roofing, gutters | 0.5–1 mm |
| Small low-pressure tanks | 2–4 mm |
| Boiler plate | 6–12 mm |
Where to find it
All the metal comes from earlier chapters. The things you must find for powered work are a site with water power (see The Waterwheel), big straight oak for the hammer helve and frames (an oak trunk 30–40 cm thick and 3–4 m long), and enough iron for the hammer head and rolls — tens to hundreds of kilograms. The rolls for iron are best cast from hard white The Blast Furnace and Cast Iron; until you have it, start with a hammer.
Method 1: Hammering sheet by hand
Copper or brass:
- Cast a flat ingot 4–6 mm thick in an open stone or sand mould (see Metal Casting), or forge a lump flat.
- Hammer it cold with the cross-peen, in rows of overlapping blows, turning the sheet 90° between courses so it spreads evenly.
- When it rings and springs instead of moving, anneal it: heat it evenly to a dull red in the forge or a wood fire, and quench it in water. Scrub off the black scale with wet sand, or dip it in a pickle of vinegar or very dilute Sulfuric Acid.
- Repeat until it is about the thickness you want, then planish: lay it on a smooth anvil or stake and go over the whole surface with light, overlapping blows of the polished hammer. This smooths and stiffens it.
Iron:
- Start with a bar 10–15 mm thick and 40–60 mm wide. Forge it hot to 3–4 mm with the cross-peen, then flatten with the flat face.
- Below about 2 mm, a single sheet cools too fast. Make a pack: cut it into pieces, brush them with a thin wash of clay and water (so they do not weld together), stack four to eight, heat the pack to yellow, and hammer the whole stack together. As it spreads, fold the pack double and carry on. In this way the old ironmasters made sheet as thin as 0.5 mm.
- Peel the sheets apart, trim the edges, and flatten each one cold with a mallet on a flat block.
Hand hammering is slow — expect a day or more to make a square metre of thin, even sheet. That is why water power came next.
Method 2: The water-powered hammer
A helve hammer is a heavy hammer head on the end of a long wooden beam (the helve) that pivots near its other end. Cams — strong wooden or iron lugs fixed on the waterwheel shaft — lift the helve as the shaft turns, then let it drop. The head falls under its own weight.
- The shaft. Extend the waterwheel's axle (or drive a second shaft through Gears) past the hammer: round oak 40–50 cm thick, banded with iron.
- The cams. Mortise 3–6 iron-shod hardwood cams through the shaft, evenly spaced, each sticking out 15–25 cm.
- The helve. An oak beam 3–4 m long and about 30 × 35 cm, pivoting in iron or hardwood bearings on a heavy frame (see Bearings and Lubrication). For a belly helve, the cams lift the beam near the middle; for a tail helve (or tilt hammer), the cams press down the short tail behind the pivot, tilting the head up. Tilt hammers are lighter and faster.
- The head. Forge or cast an iron head of 50–250 kg for a belly helve, or 30–100 kg for a tilt hammer, wedged onto the end of the helve.
- The anvil. An iron block of at least ten times the weight of the head, set on a huge oak stump or a timber crib bedded deep in the ground, so the blows go into the earth, not into the frame.
- The blow rate is the number of cams times the turns per minute of the shaft. Four cams at 15 turns a minute give 60 blows a minute — about right for a heavy belly helve. A tilt hammer geared up can strike 100–300 times a minute, for drawing out bars and finishing sheet.
- Control. Start and stop the hammer with the sluice gate that feeds the wheel, or prop the helve up out of reach of the cams.
Steam and drop hammers, which take this further, are in Anvils, Trip Hammers and Power Hammers.
Method 3: The rolling mill
A hand mill for soft metals
Start small: a mill for lead, tin, copper, brass, silver and gold strip, turned by hand or by an animal.
- Forge two rolls of the best, most even Steel you have, 5–8 cm across and 10–15 cm long, with a journal (shaft end) 2–3 cm thick at each end. Turn them truly round on the The Lathe and harden and temper the faces.
- Make two heavy iron side frames (housings), each with slots for the roll journals. The bottom roll sits in fixed bearings; the top roll's bearings slide up and down in the slots.
- Fit a screw (or a pair of wedges) above each top bearing to set the gap (see Screws, Nuts and Bolts).
- Fit two equal gears (pinions) on the roll ends on one side so both rolls turn at the same speed in opposite directions, and a crank on the bottom roll.
- Roll the metal through, tightening the screws a quarter turn each pass. Anneal copper and brass between every few passes.
A water-powered mill for iron
The same machine, much bigger: rolls 25–45 cm across and 30–60 cm long, ideally cast in hard, chilled white The Blast Furnace and Cast Iron, set in housings of cast iron or heavy timber bound with iron, driven from a waterwheel through a heavy flywheel so the rolls do not stall when a bar enters.
- Couple the wheel to the rolls through a deliberately weak breaking piece of cast iron, which snaps if something jams.
- Rolling plate: feed slabs at bright yellow heat with tongs; a catcher passes each back over the top roll. Close the screws a little each pass; reheat when it fades to red.
- Thin sheet: roll pairs or packs of sheets together and fold them double between heats, as in hand hammering.
- Grooved rolls (rolls with matching grooves cut round them) shape hot iron into square or round bar and rod.
- Slitting mill: a pair of rolls made of interleaved steel discs, like the teeth of two combs. Flat bar fed through comes out slit into square rods — nail rod for Nails, Rivets and Wire Fasteners in one pass.
A large iron rolling mill needs a big waterwheel — tens of kilowatts. Be honest about what your site can drive; a small stream can still turn a hand-sized mill for copper and brass strip.
Cutting, folding and joining
Cutting
- Snips: two steel-edged blades 8–10 cm long with 15–20 cm handles, hardened and tempered brown, riveted together (see Axes, Chisels, Knives and Planes and Scissors, Shears and Folding Knives). The edges are ground nearly square, at 80–85°: they shear, not slice.
- Bench shears: one blade fixed to a block, the other on a lever 60–100 cm long, for iron up to 2–3 mm.
- Chisel thicker sheet on end-grain hardwood or lead; punch holes with a hollow punch.
File off the sharp burr on every cut edge.
Folding
- Scribe the fold line.
- Clamp the sheet between the two folding bars with the line exactly at their edge.
- Push the free part over by hand, then dress the bend down flat with a mallet. For a tight 180° fold, finish over the hatchet stake.
Seams and edges
- Lock (grooved) seam: fold a 6 mm hook on the edge of each piece, one up and one down; hook them together and hammer the joint flat, then set it down with a grooved punch (a groover). It holds by itself; solder it for watertightness (see Soldering and Brazing).
- Wired edge: fold the edge round an iron wire 3–5 mm thick, using an allowance of about 2½ times the wire thickness. It stiffens a rim and removes the sharp edge.
- Riveted lap: overlap 3–4 rivet diameters, rivet (see Nails, Rivets and Wire Fasteners), and solder or caulk.
- Forge-welded lap: for iron pipes and thick plate, overlap, flux, and weld in sections over a mandrel (Blacksmithing).
Project: a bucket
For a bucket 30 cm across the top, 24 cm across the bottom and 30 cm along the sloping side, from sheet 0.5–0.8 mm thick:
- Lay out the side. A tapered side unrolls into a curved band — part of a ring. Its outer radius is R = slant height × top diameter ÷ (top diameter − bottom diameter) = 30 × 30 ÷ 6 = 150 cm. The inner radius is R minus the slant height = 120 cm. The band's angle is 180 × top diameter ÷ R = 180 × 30 ÷ 150 = 36°. Swing the two arcs with a cord and nail on a big flat surface (or on the sheet itself), and mark the angle by making the outer arc's length equal to the top circumference: π × 30 = 94.2 cm.
- Add allowances: 6 mm at each end for the lock seam, 10 mm at the top for a wired edge with 4 mm wire, and 6 mm at the bottom.
- Cut out, fold the seam hooks, roll the band round a log, hook the seam and close it. Wire the top edge.
- Bottom: cut a disc 24 cm across plus 6 mm all round. Turn up the extra 6 mm as a flange with light mallet blows over a stake. Fit it on, fold the body's bottom allowance over the flange, and hammer it down tight.
- Solder the side seam and bottom seam on the inside.
- Ears and handle: rivet two small iron ears below the rim and hook on a handle of 5 mm rod.
A straight-sided bucket is easier still: the side is a simple rectangle, π × diameter long.
Pipes and boilers
- Pipes: cut a strip π × the diameter wide plus the seam allowance, roll it round a mandrel, and close it with a lock seam (stovepipe), a soldered or brazed lap (copper water pipe), or a forge-welded lap (iron pipe for water or steam). See Pipes, Plumbing and Aqueducts and Metal Pipes and Tubes.
- Boilers and pressure vessels are plate shells riveted along lapped seams, with the plate edges then caulked — the edge driven against the next plate with a blunt chisel — to make them tight. The plate must be thick enough: the force trying to burst a cylinder is carried by the two walls, so required thickness = pressure × diameter ÷ (2 × allowable stress × joint efficiency). For wrought iron use an allowable stress of no more than 50 MPa (one-sixth or so of its breaking strength) and a joint efficiency of 0.6 for a riveted lap. For a boiler 1 m across at a working pressure of 3 bar (0.3 MPa) that gives 0.3 × 1,000 ÷ (2 × 50 × 0.6) = 5 mm — then add 3–5 mm for corrosion. Early steam engines ran at little more than atmospheric pressure for good reason. Design and testing are covered fully in Pressure Vessels and Valves and Boilers and Pressure Vessels.
How to tell it worked
- Even thickness: feel along the sheet between finger and thumb, or check with calipers at a dozen points. Hold it up to the light at a low angle: lumps and hollows show as shadows.
- Flat: laid on a flat stone, it does not rock.
- Not cracked: bend a trimmed strip double and back. Good sheet bends without cracking; cracks at the bend mean it needed annealing, or the iron is cold-short (see Nails, Rivets and Wire Fasteners).
- Watertight: fill a bucket or tank with water and stand it on dry paper overnight.
- Pressure vessels: test full of water, never air or steam, at 1½ to 2 times the working pressure, using a hand pump (see Pumps). Watch for weeping seams; caulk and test again. Water stores little energy, so a split under water test does not explode.
Note Troubleshooting. Copper cracks at the edges → too long without annealing. Anneal more often, and trim cracks off before they run. Sheet comes out wavy at the edges → the edges were thinned more than the middle. Hammer or roll more in the middle; on rolls, crown the rolls very slightly (fatter in the middle). Pack of iron sheets welded together → clay wash too thin, or the pack overheated. Use a thicker wash and keep to yellow heat. Rolls won't grip the metal → too large a reduction for one pass, or rolls too smooth. Take smaller bites, round the leading edge of the slab, and roughen the rolls slightly. Seam leaks → solder did not run through. Clean, flux and re-solder from the inside.
Dangers
Danger Powered hammers and rolls do not stop for flesh. A helve hammer falls with enough force to crush a hand flat. Rolls grab a glove, a sleeve or a finger and pull the whole arm in. Feed work only with long tongs; wear close-fitting sleeves; and always have a way to stop the wheel instantly — a sluice gate within reach, and someone standing by it. Never reach between rolls that are turning, for any reason.
Danger Boiler explosions. A pressure vessel that bursts releases its stored steam all at once, destroying buildings and killing everyone near. Make plate thick enough, test every vessel with water at 1½–2 times working pressure before use, fit a weighted safety valve that you test daily, and never let water run low over a hot fire. See The Steam Engine.
- Cuts. Sheet edges and burrs cut like knives. File every edge, handle large sheets with leather gloves or pads, and carry them vertically.
- Noise. A hammer mill is deafeningly loud. Plug your ears with wax and wool.
What this unlocks
Sheet makes cans for Canning and Bottling and the other containers of Tins, Cans, Drums and Tanks, cooking pots and Kitchen and Cooking, raised and spun vessels (Metal Spinning and Raising), pressed parts (Presses, Punches and Dies), lanterns (Lamps and Candles), Roofs, gutters, stovepipes and water Pipes, Plumbing and Aqueducts. Plate makes boilers for the The Steam Engine, Steamships and Railways. Strip makes nail rod and wire. Grooved rolls lead to rolled bars, rails and beams for Steel Frames and Tall Buildings, especially once steel is made in quantity (Steel in Quantity).
How it was first done
Bronze Age smiths beat copper and bronze into sheet for cauldrons, helmets and armour, annealing it in the fire. Chinese engineers were driving trip hammers with waterwheels by the 1st century AD, mainly to pound grain; in Europe, water-powered hammers for iron spread from the 12th and 13th centuries, often at monastery forges. Leonardo da Vinci sketched rolling mills around 1480–1500, and small mills rolled soft metals — lead, tin and the gold and silver strip for coins — in the 1500s. The slitting mill, which slit iron bar into nail rod, was brought to England from the area of Liège around 1590. Around 1700 John Hanbury at Pontypool in Wales was rolling iron sheet for tinplate, and in 1783 Henry Cort patented grooved rolls for making bar iron, which, with his puddling furnace (see The Blast Furnace and Cast Iron), made British iron cheap and plentiful.