◆ Rebuild

Part 11 · Power and Energy

Solar Cells

A solar cell turns light straight into electricity, with no moving parts and no fuel. How the photovoltaic effect works, the simple copper-oxide and selenium cells you can make early on (good for light meters, not for power), what it takes to make silicon cells, and how to use panels, batteries and charge control safely.

Difficulty
●●●●●
Time
A day for a copper-oxide test cell; weeks for a selenium cell; silicon cells need a whole semiconductor industry
Steps from zero
43 prerequisites →

You need first

Semiconductors and the Transistor

This unlocks

—
The full path from nothing — 43 steps before this one
  1. Fire
  2. Cordage and Rope
  3. Stone Tools
  4. Finding and Preparing Clay
  5. Finding and Identifying Ores
  6. Sulfur
  7. Hunting and Trapping
  8. Basic Woodworking
  9. The Kiln
  10. Pottery
  11. Charcoal
  12. Hides and Leather
  13. Lime
  14. Bricks
  15. Salt
  16. Mercury
  17. Lye and Potash
  18. Fermentation
  19. The Wheel and Axle
  20. Glass
  21. Firebrick and Refractories
  22. Bellows
  23. Saltpeter
  24. The Lathe
  25. Gears
  26. Copper Smelting
  27. Iron (the Bloomery)
  28. Laboratory Glassware
  29. Sulfuric Acid
  30. Pumps
  31. The Waterwheel
  32. Blacksmithing
  33. Hydrochloric Acid
  34. The Battery
  35. The Vacuum Pump
  36. Magnets
  37. The Light Bulb
  38. Copper Wire
  39. The Generator
  40. The Vacuum Tube
  41. The Electric Arc Furnace
  42. Pure Silicon
  43. Semiconductors and the Transistor
  44. Solar Cells

Do them roughly in this order. See it on the tech tree →

Why it matters

Every other way of making electricity in this book spins a magnet past a coil: a Water Turbines and Hydroelectric Power, a Wind Turbines, a The Steam Turbine. A solar cell does it with no motion at all. Light falls on a thin slice of the right material, and a current flows. A solar panel has no bearings to grease, no belts to slip, no fuel to haul; a good one keeps working for 25–40 years. It works on any rooftop, in any village, as long as the sun shines.

That is why solar cells power satellites, lighthouses, remote radio stations (Radio) and now a large share of the world's homes.

Be honest about what is realistic. The cells that give useful power — silicon cells — are made from silicon purer than almost anything else people produce, in furnaces and clean rooms (Clean Rooms) that need the whole chain of Pure Silicon, Semiconductors and the Transistor and precise chemistry behind them. A rebuilding community will get there late. What you can make early are copper-oxide and selenium cells: real solar cells that show the principle, and make excellent light meters and light-operated switches — but they give thousandths of the power of silicon. If you have salvaged panels, they are among the most valuable things you own: look after them as this chapter describes.

How it works

Light comes in packets

Light carries energy in tiny packets called photons. Blue light's packets carry more energy than red light's. When a photon is absorbed by certain materials — semiconductors such as silicon, selenium and copper oxide — it can knock an electron loose from its place, leaving behind a gap (a hole) that acts like a positive charge. This is the photoelectric effect.

On its own that does nothing useful: the loose electron soon falls back into a hole and the energy becomes a little heat.

The junction gives a one-way push

A solar cell is built so that freed electrons are swept away before they can fall back. It joins two slightly different versions of the same material:

  • n-type — with a trace of an impurity that gives it spare electrons (for silicon, phosphorus).
  • p-type — with a trace of an impurity that leaves it short of electrons (for silicon, boron).

Where they meet — the junction — a built-in electrical field forms, like a slope that electrons can only roll down one way. When light frees an electron near the junction, the field pushes it into the n-side and its hole into the p-side. Metal contacts on the front and back collect them. Join the contacts through a lamp or a battery and a current flows round, driven by light. The same kind of junction makes a diode, which lets current pass one way only (Semiconductors and the Transistor).

−+−+ Sunlight Front contactthin silver lines n-type layerthin; phosphorus Junctionpushes − up, + down p-type base0.2 mm; boron Back contactaluminium Lampor battery electrons flow out and back in about 0.5 Vper cell
Fig. 1 A silicon solar cell in cross-section. Light passes the thin front contacts and frees electrons near the junction; the junction drives them out through the front contact, round the outside circuit and back into the base.

What a cell gives

  • Voltage is set by the material, not the size: a silicon cell gives about 0.6 V with no load and about 0.5 V when working. Bigger cells do not give more voltage.
  • Current rises with the area of the cell and the brightness of the light: a modern silicon cell gives about 35–40 mA per square centimetre in full sun. A cell 15 × 15 cm gives about 8–9 A at 0.5 V — some 4–5 W.
  • Efficiency — the share of the sunlight turned into electricity: modern silicon 15–23%; the first silicon cells of 1954 about 6%; selenium cells about 0.5–1%; copper-oxide cells far less.
  • Heat lowers the voltage: a panel loses about 0.4–0.5% of its power for every degree above 25 °C. Panels work best on cold, bright days.

To get a useful voltage, cells are joined in series (the front of one to the back of the next) into a panel: 36 silicon cells give about 18 V working and 21–22 V with no load — right for charging a 12 V battery.

What you need

For Item Notes
Copper-oxide cell Clean copper sheet, two pieces about 10 × 5 cm; salt; a glass jar; a sensitive galvanometer Copper Smelting, Measuring Electricity
Selenium cell Grey selenium; an iron or brass plate; gold leaf; a hotplate you can hold near 200 °C See below
Using panels Panel(s), a lead-acid battery, a blocking diode, a charge controller or relay, fuses, thick copper wire The Rechargeable Battery, Wiring and Electrical Safety

Where to find it

  • Copper — see Copper Smelting; native copper or copper smelted from ores such as chalcopyrite.
  • Selenium is never found pure. It hides in small amounts in sulfide ores — pyrite and chalcopyrite especially. When those ores are roasted to make Sulfuric Acid, a red-brown sludge collects in the acid chambers and flues; when copper is purified by Electrolysis, it collects in the dark slime under the anodes. Both are rich in selenium, and pure selenium is recovered from them by further chemistry (Selenium and Tellurium). That is how it was discovered — in the sludge of a sulfuric acid works.
  • Silicon is the second most common element in the Earth's crust: every grain of quartz and white sand is silicon dioxide. The difficulty is not finding it but purifying it — see Pure Silicon.

Method 1: A copper-oxide cell (a demonstration)

This simple cell proves that light can make electricity. Its output is tiny, but you can make it as soon as you have copper sheet.

Oxidised platered cuprous oxidefacing the light Clean copperplate Salt water Galvanometerneedle moves in sunlight Sunlight plates must not touch
Fig. 2 The copper-oxide test cell. One plate carries a skin of red cuprous oxide made by heating; the other is clean copper. In salt water, light on the oxide plate sends a small current through the galvanometer.
  1. Clean two pieces of copper sheet, each about 10 × 5 cm, with sand and water until bright. Do not touch the faces with greasy fingers.
  2. Heat one piece in a clean charcoal fire, or on an iron plate over a strong fire, until it glows a dull red and stays there for about 30 minutes. It will turn black.
  3. Let it cool slowly in the dying fire. As it cools, the black skin (cupric oxide) cracks and flakes off, showing a red-orange to purplish layer beneath: cuprous oxide, the semiconductor. Brush off loose black flakes gently; do not scrub the red layer.
  4. Set up the cell. Bend both plates so they hang over the rim of a glass jar without touching each other, with the oxidised face towards the light. Fill the jar two-thirds with water in which you have dissolved 2–3 spoonfuls of salt.
  5. Connect the two plates to a sensitive galvanometer (Measuring Electricity).
  6. Test. Cover the jar with a cloth and note the needle. Uncover it in bright sunlight: the needle moves. Cover it again: it returns.

What to expect: tens of microamps (millionths of an amp) at a fraction of a volt. Not enough to light anything — but enough to show the principle, test which colours of light work best (filter sunlight through coloured glass), and act as a crude light detector.

Method 2: A selenium cell

Selenium cells were the first solid solar cells (1883), and for fifty years the photographer's light meter. They are a real, dry, long-lasting cell — still too weak for power, but excellent for measuring light, opening a door when a beam is broken, or reading exposure.

  1. Base plate. A clean, flat iron or brass plate, a few centimetres square, roughened slightly with fine sand.
  2. Melt on the selenium. Heat the plate to just above 221 °C (selenium's melting point — a scrap of tin, which melts at 232 °C, held on the plate just begins to melt). Rub a stick of selenium over it so a thin film melts on, and press it flat with a warm glass or mica plate to an even layer about a tenth of a millimetre thick.
  3. Anneal. Keep the plate at about 200 °C — just below melting — for several hours. The glassy, dark red-black selenium slowly turns to dull grey crystalline selenium, the form that responds to light. This step makes or breaks the cell.
  4. Top contact. The light must reach the selenium through the top electrode, so it must be thin enough to see through. Gold leaf (Gold and Silver) — beaten so thin it glows green when you hold it up to the light — is ideal. Lay it over the selenium, press it down lightly, and make contact with it at one edge through a thin copper strip. Never let the strip touch the base plate.
  5. Protect the cell under a glass cover sealed with wax or varnish.
  6. Test with a galvanometer between the base plate and the gold strip. In full sun a good cell gives up to a few tenths of a volt and a current you can read on an ordinary galvanometer.

Many cells fail at the anneal (the selenium stays glassy) or the top contact (gold too thick, or a short circuit to the base). Make several at once and keep the best.

Method 3: Silicon cells, in outline

This is how working panels are made. It cannot be done in a workshop; it is listed so you understand the path and what each step needs.

  1. Silicon from quartz. Pure quartz is heated with carbon (Charcoal or coke) in an The Electric Arc Furnace at about 1,900 °C. The carbon takes the oxygen and leaves liquid silicon about 98–99% pure.
  2. Purification to at least 99.9999% ("six nines"). The silicon is turned into a liquid chlorine compound, distilled many times (Distillation), and decomposed back to silicon on heated rods. These chemicals are poisonous, corrosive and catch fire in air. See Pure Silicon.
  3. Crystals. The pure silicon is melted with a trace of boron and a single crystal is pulled slowly up from the melt on a seed, forming a cylinder; or the melt is cast in blocks.
  4. Wafers. The crystal is sawn into slices about 0.2 mm thick and etched clean.
  5. The junction. The wafers are heated to about 850–900 °C in a furnace with a phosphorus compound, which soaks a fraction of a micrometre into the surface and makes a thin n-type layer over the p-type base.
  6. Contacts and coating. Fine silver lines are printed on the front, aluminium on the back, and fired on. A thin coating (which gives cells their blue colour) cuts reflection.
  7. Panels. Cells are soldered in series and sealed between toughened glass and a backing, in an aluminium frame.

Every step needs precision heating, pure chemicals, testing instruments and great care — which is why solar cells arrive near the end of the road (Integrated Circuits uses the same skills).

Using solar panels

Panel, 36 cells~95 W for 260 Wh a day;18 V working; tilt ≈ latitude Blockingdiodeno leakat night Charge controllerstops charging at 14.4 V;cuts loads at 11.8 V fuse 12 V battery~130 Ah fuse Lamps, radiofrom the battery
Fig. 3 A small solar power system. The panel charges the battery through a blocking diode and a charge controller; loads draw from the battery through fuses. Size the panel and battery from your daily use.

Placing the panel

  • Face it towards the noon sun (south in the northern hemisphere, north in the southern), tilted up from flat by about your latitude — steeper to favour winter. See Solar Heat for finding the sun.
  • No shade. Shading a single cell can cut the output of the whole panel, because all the cells are in series: one blocked cell blocks them all. Good panels have bypass diodes that let current go round shaded groups of cells, but still: keep branches, chimneys and snow off them.
  • Keep it cool and clean. Mount it with air behind it. Wash dust and bird droppings off with water and a soft cloth.

Sizing a system

  1. Daily use. Add up watt-hours: 4 lamps of 10 W for 5 hours = 200 Wh; a 20 W radio for 3 hours = 60 Wh; total 260 Wh a day.
  2. Sun hours. A sunny place gets the equivalent of 4–6 hours of full sun a day in summer; a cloudy winter may give 1–2.
  3. Panel: daily use ÷ (sun hours × 0.7). With 4 sun hours: 260 ÷ 2.8 ≈ 95 W of panels. The 0.7 covers heat, dust, wiring and battery losses.
  4. Battery: to ride through 3 dull days without emptying the battery below half: 260 Wh × 3 ÷ 0.5 = 1,560 Wh, which at 12 V is 130 amp-hours (The Rechargeable Battery).

Charge control

A panel connected straight to a lead-acid battery will overcharge it on sunny days, boiling the acid and ruining the plates, and the battery can leak back through the panel at night.

  • Blocking diode. A diode in series with the panel lets current flow into the battery but not back out at night. If you have no diode, disconnect the panel at dusk by hand.
  • Stop charging when full. For a 12 V lead-acid battery, stop or reduce charging at about 14.4 V (2.4 V per cell); hold it at 13.5–13.8 V to keep it topped up. Without a voltmeter, watch the cells: steady gassing (fine bubbles) means full.
  • Stop discharging when low. Disconnect the loads at about 11.8–12.0 V, or when the hydrometer shows the battery half empty. Batteries drained flat repeatedly die in months.
  • A controller without electronics: an The Electromagnet relay whose coil is connected across the battery, with an adjustable spring. Set the spring so the armature pulls in at 14.4 V and opens the panel circuit (or switches it to a dump load); it drops out again as the voltage falls. A second relay, set lower, can cut off the loads. This is how dynamo chargers were regulated for decades.

Wiring

Panels in series add their voltages; panels in parallel add their currents. Use thick copper wire for short, low-voltage runs (see Power Lines and Distribution for the voltage-drop rule) and fuse the battery output and each panel string close to the battery.

How to tell it worked

  • Open-circuit voltage. With nothing connected, a 36-cell panel in sun reads 20–22 V; a single silicon cell about 0.6 V. Even weak light gives most of the voltage.
  • Short-circuit current. Briefly connect the panel through an ammeter alone: the current should be close to the figure on its label in full noon sun, and fall in step as you shade it. (Do this only with a panel, never with a battery.)
  • Shade test. Cover one cell with your hand: the panel's current should drop sharply. If it does not change, a cell or connection is already dead.
  • The battery gains charge by afternoon and the lamps burn all evening.

Note Troubleshooting. Copper-oxide cell gives nothing → oxide layer too thin, or rubbed off; plates touching; galvanometer not sensitive enough. Re-heat longer; use a more sensitive needle. Selenium cell shorted (needle jumps with no light) → the gold or contact strip touches the base plate through a pinhole. Make the selenium layer thicker and even. Selenium cell barely responds → selenium not fully converted to grey; anneal longer at just under 221 °C. Panel output much lower than its label → dirty glass, heat, partial shade, or a corroded connector. Clean, cool and check the junction box. Battery empty every morning → loads bigger than the panel can supply, or current leaking back through the panel at night (fit a blocking diode). Battery boils and needs water often → overcharging; set the controller lower.

Dangers

Danger High-voltage DC. One panel gives a safe voltage, but many in series can give 300–600 V of direct current — enough to kill. A DC arc does not stop by itself the way an AC arc does: pull a connector apart under load and it can draw a fierce arc that burns and starts fires. Disconnect strings only when covered or at night, and never with loads on.

Danger Batteries. A battery bank short-circuited by a spanner delivers hundreds of amps: the tool glows red and can explode molten metal into your face. Charging batteries also make hydrogen, which explodes with a spark. Fuse every battery, cover the terminals, ventilate the room, and keep flames away. See The Rechargeable Battery.

  • Selenium and its compounds are poisonous, especially as fumes or dust. Melt and anneal it outdoors or under a good draught, never above about 250 °C, and wash hands carefully. Selenium compounds smell strongly of horseradish or rotting radish — a warning sign.
  • Silicon refining chemicals (silicon chlorides, silane, hydrofluoric acid used for etching) are among the most dangerous substances in industry: they burn, corrode lungs and eat through flesh to the bone. Do not attempt them without full training and equipment.
  • Roofs. More people are hurt falling off roofs while fitting panels than by the electricity. Use ladders properly and ropes on steep roofs.
  • Broken panels still make electricity in the light. Cover them before handling.

What this unlocks

Even a small panel brings light, Radio and The Telephone and The Telegraph repeaters to places no power line will reach, and keeps The Computers and Networks and the Internet running off-grid. Combined with Wind Turbiness and Water Turbines and Hydroelectric Powers on a shared Power Lines and Distribution, solar cells make a community independent of fuel. The light-sensitive cells of Methods 1 and 2 are useful in their own right as light meters for Photography and as sensors (Photocells and Sensors).

How it was first done

In 1839 the 19-year-old French physicist Edmond Becquerel found that light falling on one of two coated metal plates in an acid solution increased the current between them — the first photovoltaic effect, in a cell much like Method 1. In 1873 the English engineer Willoughby Smith noticed that selenium conducts electricity better in light than in the dark, and in 1876 William Grylls Adams and Richard Day in London found that light alone could drive a current through selenium. In 1883 the American inventor Charles Fritts made the first true solar cells, of selenium covered with gold leaf, and installed a panel on a New York rooftop; his cells turned about 1% of the light into electricity.

Nobody understood why until Albert Einstein explained the photoelectric effect in 1905 by treating light as packets of energy, the work for which he received the Nobel Prize. Copper-oxide and selenium cells became the light meters of 1930s cameras. At Bell Laboratories in 1940, Russell Ohl stumbled on the p–n junction in a cracked silicon rod that produced a voltage in light, and in 1954 his colleagues Daryl Chapin, Calvin Fuller and Gerald Pearson demonstrated the first practical silicon solar cell, about 6% efficient. In 1958 solar cells powered the radio of the satellite Vanguard 1, and space was where they were first used in earnest. Steady improvement since then has made them one of the cheapest sources of electricity on Earth.