Part 8 · Chemistry
Matches
From splints tipped with sulfur, lit from a spark, to the safety match that lights only on its own box. How each kind works, how to make the simple ones yourself, why the old phosphorus match was banned, and the other ways to make fire quickly.
- Difficulty
- ●●●●●
- Time
- An hour to make a hundred sulfur matches; an afternoon to carve a fire piston
- Steps from zero
- 11 prerequisites →
This unlocks
—The full path from nothing — 11 steps before this one
- Fire
- Cordage and Rope
- Stone Tools
- Finding and Preparing Clay
- Sulfur
- Hunting and Trapping
- Charcoal
- Pottery
- Hides and Leather
- Tar, Pitch and Glue
- Glues and Adhesives
- Matches
Do them roughly in this order. See it on the tech tree →
Why it matters
Making fire from nothing is the first skill in this book (Fire) — but it is slow. A bow drill takes minutes of hard work and good dry wood; flint and steel need practice and a spark-catching tinder. For almost all of history, households avoided the problem by never letting the fire go out.
A match makes fire in a second, in the hand, in any weather, by anyone. That saves hours of labour every week, makes lamps and stoves practical (Lamps and Candles), and in a crisis — a cold night, a wet camp, a sick person — can save a life.
There are three steps on the road to the modern match, and the first two are well within your reach:
- The sulfur match — a splint tipped with Sulfur. It cannot make fire by itself, but it turns a glowing spark or ember into a flame instantly. Make these today.
- The tinderbox and the fire piston — reliable ways to get the glowing spark.
- The friction match and the safety match — chemistry that carries its own fire. These need an industrial chemical base; this chapter explains how they work and why some were banned, but keeps to principles.
How it works
Fire needs fuel, heat and oxygen (Fire). Every kind of match is a way to deliver enough heat to a small amount of fuel that lights easily, then pass the flame to something that burns longer.
- Sulfur melts at about 115 °C and catches fire at roughly 230–250 °C — far lower than wood (about 300 °C and up). A glowing spark on char cloth is hot enough to light it, but too small to light a wooden stick directly. Sulfur burns with a small blue flame, hot and lasting enough to light the wood under it. So a sulfur-tipped splint is a flame amplifier.
- A chemical match head carries its own oxygen. It contains an oxidiser — a substance that gives up oxygen when heated — mixed with fuels and held together by glue. Rubbed on a rough surface, friction heats a tiny spot to the point where the oxidiser and fuel start to react; the reaction makes more heat than it needs, and the whole head flares.
- "Strike-anywhere" matches contain an especially easily-lit ingredient in the head, so any rough surface will do — and so will a jolt, a rub in a pocket, or a rat gnawing the box.
- The safety match splits the job in two. The head holds the oxidiser and fuel; the easy-to-light ingredient (red phosphorus) is on the striking strip of the box. Neither part lights easily alone. Only when head meets strip does a trace of the strip's material rub off, catch fire from the friction and set off the head. Hence safety: the match lights only on its own box.
- The stick matters too. A good splint is dipped in wax (or, earlier, sulfur) just below the head so the flame passes from the brief, hot head flare to a steady burning stick. Modern splints are also soaked in a salt that stops them glowing after they are blown out.
What you need
For the sulfur matches and tinderbox you can make yourself:
| Item | Amount | Notes |
|---|---|---|
| Sulfur | 100–200 g for about 200 matches | Pure lumps or melted cakes. See Sulfur. |
| Splints | As many as you want | Straight-grained, dry aspen, poplar, willow, pine or cedar; 10–15 cm long, 2–3 mm square |
| Beeswax or tallow (optional) | A spoonful | To dip below the sulfur so the flame passes to the wood |
| Small clay pot or tin | 1 | To melt the sulfur in; with a lid |
| Flint or quartz and a steel striker | 1 each | See Fire, Steel |
| Char cloth or prepared tinder fungus | A handful | See Fire |
| A tight box of tin, horn or wood | 1 | To keep the whole kit dry |
Where to find it
- Sulfur: yellow crusts around volcanic vents and hot springs, or melted out of pyrite — see Sulfur.
- Splint wood: aspen and poplar (pale, light, straight-grained, splits cleanly — the classic match wood), willow, basswood (linden), and resinous pine or cedar, which catch even faster. Use dead, seasoned wood. Thin slivers can also be split from dry reeds or straw stalks, or rolled from strips of paper (Paper).
- Tinder fungus, flint, steel: see Fire.
Method 1: Sulfur matches
These were the ordinary matches of Europe and China for centuries — called spunks or brimstone matches in English. They do not light by striking; you touch them to a glowing ember or a spark on char cloth.
- Split the splints. Saw or split seasoned wood into blocks 10–15 cm long, then split those into slivers about 2–3 mm square with a knife and a mallet. Dry them a day by the fire.
- Optional wax step. Melt a little beeswax or tallow and dip the last 2 cm of each splint for a moment. Wax helps the flame pass from the sulfur to the wood.
- Melt the sulfur. Put broken sulfur in a small pot at the edge of a low fire, outdoors. Heat until it is a thin, clear, amber-yellow liquid (about 120–150 °C). If it turns dark red-brown and thick like syrup, it is too hot — pull it back from the fire. If you see a blue flame on the surface, it is burning: put the lid on at once to smother it, and stand back from the fumes.
- Dip. Dip the tips about 1 cm into the sulfur, lift, and let the excess drip off. Dip again once or twice for a thicker coat. Bundling 20–30 splints with a band of cord lets you dip them all at once.
- Dry. Stand them tips up in a pot of sand, or spread them on a board. The sulfur sets hard and pale yellow in a minute.
- Double-ended spunks. Dip both ends and break the stick in the middle later; you get two matches from each splint.
- Store in a closed box in a dry place. They keep for years.
To use: strike a spark onto char cloth or blow a coal to a bright glow, then touch the sulfur tip to the glowing spot and blow gently. The sulfur melts, catches with a small blue flame, and in two or three seconds the wood takes a yellow flame. Light your candle, lamp or tinder from it.
Method 2: The tinderbox
Before 1830, every house kept a tinderbox: a tin box holding a steel striker, a flint, a supply of char cloth, and a bundle of sulfur matches. Often the lid had a candle socket.
- Hold the flint with a piece of char cloth on top of it, near the sharp edge.
- Strike glancing blows with the steel until a spark lands and makes a spreading red spot (Fire, Method 2).
- Touch a sulfur match to the glowing spot. It flames.
- Light the candle or lamp. Then close the lid on the remaining char cloth to snuff it out — the burnt cloth left in the box becomes next time's tinder.
With practice the whole sequence takes 30 seconds to a minute.
Tip Better tinder. Tinder fungus or cotton rag soaked in a weak solution of Saltpeter (a level teaspoon in a cup of water) and dried catches sparks far more readily and glows hotter. Use it only as a thin dry sheet, kept away from sulfur and the match bundle.
Method 3: The fire piston
A fire piston makes fire from compressed air. When you squeeze air very fast into a small space, it heats up — the same thing that warms a bicycle pump. Pushed hard and fast to a twentieth of its volume, air gets hotter than 400 °C, enough to make char cloth glow. People in South-East Asia and Madagascar used fire pistons of wood, horn and bamboo for centuries.
- The cylinder. A block of hard, close-grained wood (boxwood, ebony, hard maple), horn or bone, about 10–12 cm long and 2.5–3 cm thick. Bore a perfectly straight, smooth hole 10–13 mm across and 8–10 cm deep, closed at the bottom (Drills and Boring). The smoother and straighter the bore, the better. Polish it with a rod and fine sand (Abrasives and Grinding Stones).
- The piston. A rod of hard wood that slides easily in the bore, with a handle knob. Cut a groove 2–3 mm wide near the tip and wind thread into it until it makes a snug seal; grease it with fat or wax. Hollow the very end of the piston slightly into a small cup.
- Load. Put a pea-sized bit of char cloth or tinder fungus in the cup at the end of the piston.
- Fire. Push the piston into the cylinder a little, stand the cylinder on something firm, and strike the knob down sharply with your palm, all in one movement. Pull the piston out at once. The tinder should be glowing. Transfer it to a sulfur match or a tinder nest.
Note Troubleshooting. Sulfur flakes off the splint → the sulfur was too cool and thick, or the wood was damp. Dip hotter (but still amber, not dark) into dry wood. The sulfur flames but the wood will not catch → splints too thick, or wet. Split them thinner, dry them, add the wax dip. Sulfur matches smoulder but don't flame → blow very gently on the tip once it touches the coal. Fire piston will not light → the seal leaks (rewind and grease the thread), the stroke is too slow (one sharp blow, not a push), or the tinder is damp. Practise until you can hear a sharp "pop".
How it works in the factory: friction and safety matches
A true friction match needs two chemicals you cannot simply gather:
- An oxidiser for the head. Most matches since the 1830s use potassium chlorate, made industrially by passing electricity through hot salt solutions (Electrolysis, Chlorine and Bleach).
- Phosphorus for easy lighting. Phosphorus is an element found in bones and phosphate rock; it is released by heating phosphate with carbon and sand at white heat in an The Electric Arc Furnace — a hazardous industrial process. It comes out as poisonous, self-igniting white phosphorus, which is changed into much safer red phosphorus by heating it for a long time without air.
Glue binds everything (Glues and Adhesives); fine ground glass gives grip; the box strip is red phosphorus and ground glass in glue painted on card (Paper). Splints are cut from aspen, dipped in paraffin wax, and soaked in a phosphate salt against afterglow.
This book does not give formulas for match heads. Chlorate mixtures are dangerously sensitive: a mixture of potassium chlorate with sulfur or phosphorus can explode from a grinding stroke, a knock or a little warmth, and has maimed many experimenters and match workers. Industrial match making grew up only with careful wet mixing, small batches and machines that kept people away from the dangerous steps. Until you have that, use Methods 1–3.
How to tell it worked
- Sulfur matches: a smooth, hard, evenly yellow tip; touched to a glowing coal, a blue flame within two seconds and a yellow flame on the wood within five.
- Tinderbox: a flame from flint and steel in under a minute, every time.
- Fire piston: a glowing ember on the tinder from one stroke in at least half of your tries.
- Storage test: after a month in the box, matches and tinder still work — if not, the box lets in damp.
Dangers
Danger White phosphorus — the "strike-anywhere" ingredient of the 1830s–1900s — catches fire by itself in air, causes deep burns that keep burning, and is a deadly poison (a fraction of a gram can kill). Match workers who breathed its fumes for years developed "phossy jaw": the jawbone rotted away, often fatally. Never try to make or use it.
Danger Never grind or mix chlorates with sulfur, phosphorus, charcoal or sugar. These mixtures can explode without warning from friction or a light blow. This is the reason this chapter gives only principles for friction matches.
- Burning sulfur gives off sulfur dioxide, the choking smell of a struck match. Melt sulfur only outdoors, with the wind at your back, and keep a lid handy. Molten sulfur sticks to skin and causes deep burns — cool any burn in water for 20 minutes (Wound Care and Antiseptics).
- House fires. Matches made fire easy — and made house fires and burned children common. Keep matches in a closed box, out of reach of children, away from the stove.
- Fire piston: the tinder can glow before you expect; pull the piston out and lay it on a stone, not on your clothes.
What this unlocks
Instant, portable fire for every household, workshop and traveller: lamps and candles lit in seconds (Lamps and Candles), stoves and forges started without keeping a fire overnight, fuses and burners lit at arm's length. The industrial safety match is a good marker of a working chemical industry: it needs Electrolysis, phosphorus from an The Electric Arc Furnace, Paper and glue factories, and machines (Machine Tools).
How it was first done
The first sulfur matches were probably Chinese. A tenth-century book by Tao Gu, the Qing Yi Lu (around 950), describes small pinewood sticks tipped with sulfur, called "light-bringing slaves" and later "fire inch-sticks", invented by poor court ladies of the Northern Qi in 577 who needed to light fires quickly; by the late 1200s they were sold in the markets of Hangzhou. Sulfur matches lit from a tinderbox were in general use in Europe by the 1500s.
The German alchemist Hennig Brand discovered phosphorus in 1669 by boiling down urine. Chemists soon found it lit sulfur matches by friction, but it was far too costly. Around 1805 Jean Chancel in Paris made matches that flared when dipped into sulfuric acid. In 1826 the English chemist John Walker, of Stockton-on-Tees, made the first true friction matches, which he sold from 1827; they lit when drawn through folded sandpaper. White-phosphorus matches, which lit on any surface, followed around 1830 (Charles Sauria in France and others) and spread worldwide — along with phossy jaw.
In 1844 Gustaf Erik Pasch in Sweden patented the idea of putting the phosphorus on the box rather than the head. Red phosphorus, found by Anton Schrötter in Vienna in the 1840s, made it practical, and the brothers Johan and Carl Lundström of Jönköping made safety matches in quantity from the 1850s. The London match girls' strike of 1888 drew public attention to phossy jaw; the Berne Convention of 1906 banned white phosphorus in matches, and a safe strike-anywhere head based on phosphorus sesquisulfide (French chemists Henri Sévène and Émile David Cahen, 1898) replaced it.
Source: content/entries/chemistry/matches.md