Part 7 · Home and Daily Life
Toys
How to make the toys children have always played with, from rag dolls, spinning tops, yo-yos and marbles to rocking horses, building blocks, kites, swings, seesaws and slides, and how to make every one of them safe for small children.
- Difficulty
- ●●●●●
- Time
- An hour for a pinwheel or rag doll; a day for a top, yo-yo or set of blocks; a week for a rocking horse or a swing frame
- Steps from zero
- 5 prerequisites →
This unlocks
Playgrounds and Outdoor PlayThe full path from nothing — 5 steps before this one
- Stone Tools
- Cordage and Rope
- Basic Woodworking
- Spinning and Weaving Cloth
- Sewing, Needles and Thread
- Toys
Do them roughly in this order. See it on the tech tree →
Why it matters
Children learn by playing. A child stacking blocks is learning balance, counting and fractions; one working a puppet is practising speech; one spinning a top or flying a kite is feeling the physics that later becomes Simple Machines and Gliders and Aeroplanes. Swings and skipping ropes build strength. In a hard time, toys also keep children busy, safe and happy while the adults work.
Almost every toy here uses skills you already have from Basic Woodworking, Sewing, Needles and Thread and the The Lathe (Wood Turning and Treen), and most can be made from offcuts. What takes care is safety: small children put everything in their mouths, pull everything apart and climb everything. So that comes first.
How it works
- A spinning top stays upright the way a rolling hoop does. The more of its weight sits far from the axis (in the rim), and the faster it spins, the longer it stays up.
- A yo-yo trades height for spin. Falling, it unwinds and spins up; at the bottom, the spin winds it back up the string. A flick of the hand replaces what friction steals.
- A rocking toy must keep its weight low. It is stable while the centre of gravity (the balance point) of toy and rider stays below the centre of the curve of the rockers. Short, tightly curved rockers tip over.
Making toys safe for small children
These rules matter more than any design. Children under three are most at risk.
- Choking. Any piece that fits into a tube 3.2 cm wide and 6 cm deep can choke a child under three: marbles, beads, button eyes, small blocks, balls under 4.5 cm across, and any part that can break off. Pull hard on every part; if it comes off, it must be too big to swallow.
- Cords and loops. On toys for babies under 18 months, a cord over about 30 cm, or any loop a head fits through, can strangle. Never hang a toy across a cot; take pull-toys away at bedtime.
- Splinters and edges. Round every edge to at least 2 mm and sand until a cotton cloth dragged over the toy does not snag. Use close-grained woods (beech, maple, birch, sycamore, fruit woods), not splintery oak.
- Traps. Gaps between 5 and 12 mm in moving parts trap fingers. Openings between 9 and 23 cm in railings, ladders and frames can trap a child's head while the body hangs. Make gaps smaller or larger.
- Poisons. No lead paint (white or red lead), chrome yellow, or green and yellow paints made with arsenic or copper. Use ochres, chalk and charcoal in milk or egg paint, or beeswax and linseed oil, which is safe once cured (Pigments, Paints and Varnish). No yew, laburnum or oleander wood (Dangerous Plants and Animals).
- Falls. Put 30 cm of loose bark chips or sand under anything a child can fall from.
- Inspect monthly. Wood cracks, seams split, rope rots. Mend or burn anything failing.
What you need
| Item | For | See |
|---|---|---|
| Close-grained hardwood (beech, maple, birch, boxwood, apple, pear) | Tops, yo-yos, blocks, wheels, heads | Basic Woodworking |
| Lime (basswood) or softwood | Carved bodies | Basic Woodworking |
| Sound, straight ash or oak | Rockers, swing frames, seesaw | Timber Framing and Log Building |
| Lathe, saw, knife, chisels, auger, rasp, sandstone | Shaping | The Lathe, Abrasives and Grinding Stones |
| Tight-woven cotton or linen, wool yarn, needle and thread; wool, kapok or rags for stuffing | Dolls, puppets | Sewing, Needles and Thread |
| Hemp or flax cord and rope | Strings, kites, swings | Cordage and Rope, Ropewalks and Sailcloth |
| Hide glue, beeswax, linseed oil, ochre paints | Assembly and finish | Glues and Adhesives |
Where to find it
Beech grows on chalk and loam; maple and birch across the northern forests; apple and pear prunings from any orchard make perfect toy wood. Boxwood, a slow, dense, yellow-wooded shrub of chalk hills, is the best of all for tops. Lime (basswood) is soft, pale and almost grainless, the carver's favourite. Ash, from damp, rich soil, bends before it breaks: ideal for rockers and swing seats.
Dolls
Rag doll
The safest doll for a baby.
- Pattern. Draw a gingerbread-man shape 30–40 cm tall with a head about a quarter of the height. Add 6 mm all round for seams.
- Cut two layers of tight-woven cotton or linen; loose weave lets stuffing work out.
- Sew them inside out with backstitches 2–3 mm long, leaving a 5 cm gap. Clip the seam allowance at curves and under the arms.
- Turn right side out with a blunt stick, stuff firmly with washed wool, kapok or clean rags (head hardest), and sew the gap shut.
- Stitch across the tops of the arms and legs so they bend.
- Embroider the face. For a child under three, never use buttons or beads for eyes. Sew on looped yarn hair. Make clothes separately so they can be washed.
A straw or corn-husk doll is quicker: fold soaked husks over a ball of husk for the head, tie the neck, push a rolled husk across for arms, and tie the waist. It falls to pieces, so it is for older children.
Wooden doll
A peg doll is a spindle 10–15 cm long and 2.5 cm thick, turned with a ball for a head, painted or dressed in scraps. A jointed doll 20–30 cm tall has a body, head and limbs carved from lime or birch, each joint drilled across with a 4 mm hole and pinned with a tight wooden peg glued at one end only, so the limb swings. Limbs that flop need a slightly thicker peg.
Puppet
Glove puppet. Cut two mitten shapes of cloth with a neck at the top and an arm stub each side, sew them together and leave the bottom open. Carve a head from lime with a hollow neck about 2.5 cm across for the forefinger, and glue and tie the cloth to it. Thumb and middle finger work the arms.
String puppet (marionette). Carve a figure 30–45 cm tall in parts: head, chest, hips, upper and lower arms and legs, hands and feet. Join them with cord loops or small wire rings (Iron and Brass Wire) so every joint moves freely, and make the feet a little heavy. The control is a wooden cross 20–25 cm each way, with fine waxed linen threads about 1 m long running to the sides of the head, the hands, the knees and the middle of the back. Tilt the control to walk it. Untangle the threads before every show.
Spinning and turning toys
Spinning top
Twirling top. Turn a body of dense wood 5 cm across and 2–3 cm deep, with the weight left in the rim and a cone underneath ending in a sharp point exactly on the axis. Glue an 8 mm spindle 6–7 cm long into a hole down the centre. Spin it with finger and thumb.
String top (peg top). Turn a pear shape about 6 cm across and 7 cm tall with a small button on top. Drive a nail into the point, cut off its head and file it to a blunt point. Wind a 1 m cord tightly from the peg upwards, hold the free end, and throw the top at the ground while snapping the hand back. It lands spinning.
Whip top. A grooved cone 5 cm across, started by hand and kept going by lashing it with a leather thong on a stick.
A good top spins quietly and upright for half a minute or more. A growing wobble means the point is off-centre or the body lopsided; true it on the lathe.
Yo-yo
- Turn two discs 5–6 cm across and 1.5 cm thick, with rounded faces and inner edges, and drill each with a 6 mm hole exactly at the centre.
- Glue a hardwood dowel axle into both, leaving a gap of 3–4 mm. Use a coin as a spacer while the glue sets.
- Twist a doubled cotton or linen string (Cordage and Rope) about as thick as a bootlace, long enough to reach from the floor to your navel. Untwist one end a little, slip the axle through the loop and let it twist closed around the axle. Do not knot it on: a loose loop lets the yo-yo "sleep" (spin at the bottom), and a tug brings it back.
- Tie a finger loop in the other end.
A good yo-yo weighs 50–60 g, runs without rubbing either disc, and climbs back on its own.
Pinwheel
Cut a square of paper (Paper), glue-stiffened cloth or birch bark 15–20 cm across. Cut from each corner towards the centre, stopping 2 cm short. Bend every other point to the centre, push a pin through all four and the centre, slip a small bead behind as a spacer, and drive the pin into a 30 cm stick. It must turn freely. Bend over any sharp pin end.
Kite
A diamond kite:
- Lash and glue a spine of split bamboo, willow or pine 90 cm long across a spar 75 cm long, both about 5 × 8 mm, crossing a quarter of the way down the spine.
- Notch the four ends and run a tight string round them as an outline.
- Cover with paper or thin cloth cut 2–3 cm larger, the margin folded over the string and glued.
- Tie a bridle from the top of the spine to a point two-thirds down it, and tie the flying line to it a little above the crossing. Slide the tie until the kite climbs steeply.
- Add a 3–4 m tail of cloth bows; more if it spins, less if it will not climb.
Use a line that holds about 10 kg, and fly far from trees, roads and (later) power lines. Box kites and lifting kites are in Kites and Parachutes.
Rolling toys
Marbles
Marbles are only for children over three.
- Clay marbles. Roll fine Finding and Preparing Clay into balls 1.5–2 cm across, dry for a week, fire with a batch of Pottery, and tumble in a bag with sand to smooth them.
- Stone marbles. Knock limestone or marble into rough cubes and grind each round in a hemispherical hollow in sandstone with wet sand. The old German marble mills tumbled cubes between a grooved millstone and a wooden runner turned by a The Watermill.
- Glass marbles. Gather molten Glass on an iron rod, let it droop, snip off a gob the size of a hazelnut, and roll it in a hemispherical cup cut in wet hardwood or iron until it stiffens. Cool it slowly in warm ashes for several hours or it will crack later. Twists of coloured glass laid on the gob give the classic patterns.
A playing marble is about 1.6 cm, a "shooter" 2–2.5 cm. A good one rolls straight across a flat floor.
Hoop
A hoop 60–90 cm across, about waist-high to the child, is driven along with a stick 40–50 cm long. An iron barrel hoop is best (Barrels and Cooperage). A wooden one is a strip of ash or willow 2 cm wide and 6–8 mm thick, soaked or steamed until it bends, lapped 15 cm at the joint and nailed or bound. A cane or withy hoop swung round the waist makes a twirling hoop.
Pull-along toy
- Cut a body, such as a duck or a wagon, 15–20 cm long, from hardwood.
- Slice four wheels 1.5 cm thick from a turned cylinder 4–5 cm across.
- Drill two axle holes across the body 1 mm larger than the 8 mm dowel axles, so they turn freely, and glue a wheel firmly on each end of each axle with 2 mm of play.
- Tie a cord about 50 cm long to the front with a wooden ball over 4.5 cm across as a handle; for a child under 18 months keep it under 30 cm. Do not knot the end into a loop.
An off-centre axle makes the toy bob; a peg on the axle lifting a hinged head makes it peck.
Building blocks
Good blocks are used from age one to ten. The rule is that every block is an exact multiple of one unit, so they stack and bridge.
- Use dry, close-grained hardwood (maple, beech, birch) seasoned at least a year, or the blocks will warp.
- Plane boards to exactly 3.5 cm thick and rip strips 7 cm wide. The unit block is 3.5 × 7 × 14 cm. Cut half units (7 cm), double units (28 cm) and quadruple units (56 cm), plus some columns, arches and triangles.
- Every length within 0.5 mm and every cut square: use a stop block on the saw bench and check each block against a master unit.
- Round the edges about 2 mm, sand, and leave bare or rub with beeswax.
Sixty to a hundred blocks make a good first set. Small 2.5 cm cubes are for children past the mouthing age.
Rocking horse
The most demanding toy here, and it can last a hundred years.
- Rockers. On a board of ash or oak 3–4 cm thick, 25 cm wide and 1.2–1.5 m long, draw an arc with a trammel: a nail 1.5–2 m away, a string, and a pencil at its end. Draw a second arc 8 cm inside the first. Saw both rockers together so they match, and smooth with a spokeshave.
- Stops. Fix a block near each end of each rocker, standing slightly proud, so that if the horse rocks too far the stop hits the floor first.
- Body. Glue up a block of lime or softwood about 30 × 15 × 50 cm, hollowed inside to save weight, and carve the barrel shape. The simplest version is a board horse: head and body cut from one 3 cm board, with a seat board across.
- Head. Carve it separately, fix it with a long glued tenon, and drill across it for a 2.5 cm handle peg 15 cm long.
- Legs. Four splayed ash legs, tenoned and pegged into body and rockers (Doors, Windows and Joinery). Add a footboard if the child's feet do not reach.
- Seat 50–60 cm from the floor for ages two to five. Glue on a leather saddle and a horsehair or wool mane.
- Finish with milk paint and linseed oil.
Test before any child rides. Strap about 20 kg of sand onto the seat and rock it hard both ways. It must come to rest on its stops and never roll over. If it does, lengthen or flatten the rockers or lower the seat.
Ropes, swings, seesaws and slides
Climbing frames, sandpits, roundabouts and the layout of a whole play area are in Playgrounds and Outdoor Play.
Skipping rope
A rope 8–10 mm thick of hemp, flax or cotton (Ropewalks and Sailcloth). Standing on its middle, the ends should reach the armpits: about 2.1 m for a child, 2.7 m for an adult. Thread the ends through turned handles 12 cm long bored with a 10 mm hole, and knot them inside. For group skipping use a rope 5–6 m long and 12 mm thick.
Swing
- Frame. Two posts 12–15 cm thick, set 60 cm into the ground and packed with stones, carry a 15 × 15 cm hardwood beam 2.2–2.5 m above the ground, braced at each corner. A sound living branch at least 20 cm thick will also do; never a dead one.
- Hangers. Forged eye bolts through the beam with washer and nut (Blacksmithing, Screws, Nuts and Bolts), or rope wrapped twice round the beam over a leather pad. Set them a little wider apart than the seat so it does not twist.
- Rope at least 12 mm hemp, or chain.
- Seat. A hardwood board 45 × 15 × 3 cm, or a heavy leather strap for small children, which does less harm if it hits someone.
- Space. Seat 35–45 cm up. Keep 90 cm between seat and post and 60 cm between seats. Keep clear, and soft, a zone twice the beam height in front and behind.
Replace the rope every year; it rots from the inside.
Seesaw
A straight, knot-free plank 3–4 m long, 25 cm wide and 5 cm thick, on a pivot 50–60 cm high: an iron axle 2–2.5 cm thick through a hardwood block bolted under the plank's middle and through two posts. Fix a handle across the plank 40 cm from each end, bury a half-log or a stuffed sack under each end as a bumper, and box in the pivot so no finger can reach the axle.
Slide
The safest slide has no height: cut a shallow channel down a grassy bank and line it with planed boards. For a free-standing slide:
- Platform no higher than 1.2–1.5 m for under-sixes, with a 70 cm railing (minding the 9–23 cm rule).
- Chute no steeper than 30°, of planed hardwood with the grain running downhill, joints sanded flush, side walls 10–15 cm high, waxed with beeswax.
- A nearly flat run-out 30–40 cm long at the bottom, 20–30 cm above the ground.
- A sheet-metal chute (Sheet Metal and Rolling) is slick but burns skin in summer sun; shade it.
How to tell it worked
- Pull test: nothing comes off a small child's toy, however hard you pull.
- Cloth test: a cotton cloth dragged over it does not snag.
- Play test: the top spins half a minute; the yo-yo climbs back; the kite climbs and holds steady; the rocking horse cannot be rolled with 20 kg on it.
- Load test: an adult bouncing on the swing and seesaw makes no creak, bend or movement of the posts.
Note Troubleshooting. Top wobbles → point off-centre or rim lopsided; true it on the lathe. Yo-yo will not climb back → string knotted to the axle or discs rubbing; loosen the loop, widen the gap. Yo-yo will not sleep → string too tight round the axle; untwist it slightly. Kite spins or dives → add tail or move the bridle tie up. Will not climb → less tail, tie lower. Blocks will not stack → lengths or squareness off; recut against a stop block. Swing seat twists → hangers closer than the seat is wide; spread them.
Dangers
Danger Choking and strangling kill small children quickly and silently (if it happens, see Emergency Cards). Keep marbles, small balls, beads and small blocks away from under-threes. Never leave cords, skipping ropes or pull-toys in a cot or bed.
Danger Failing frames and falls. A swing beam, seesaw or slide that breaks or tips can kill. Use sound timber, set posts deep, inspect monthly, replace rope yearly, and keep soft ground beneath. One child per swing, sitting down, and small children out of the swing's path.
- Lead and arsenic paints poison slowly; children chew toys.
- Kites and power lines: once there is an Power Lines and Distribution, a kite line touching a wire can kill, especially when wet.
- The lathe catches loose sleeves and long hair; tie them back.
What this unlocks
Wind-up toys come with Springs and Clockwork, Music Boxes and Counting Machines, and moving figures with Automata, Barrel Organs and Player Pianos; balls, board games and sports gear are in Games and Sports Equipment; kites lead to Kites and Parachutes and, slowly, Gliders and Aeroplanes. Moulded rubber and celluloid toys come with Rubber and Early Plastics. Learning through play is part of Teaching and Schools.
How it was first done
Children have played with dolls and balls as far back as records go. Small clay carts and animals on wheels, probably toys, come from Indus Valley cities such as Mohenjo-daro around 2500 BC, and Egyptian children had wooden dolls, tops and stuffed balls. Greek vases of the 400s BC show boys playing with yo-yo-like discs. Kites were flown in China at least 2,000 years ago. The rocking horse appeared in Europe in the 1600s. Glassmakers in Thuringia, Germany, began mass-producing glass marbles in the 1840s. Friedrich Froebel, who opened the first kindergarten in 1837, designed wooden blocks as teaching toys, and the American teacher Caroline Pratt created the unit block in about 1913. Pedro Flores, a Filipino immigrant, popularised the modern yo-yo with its looped "sleeping" string in the United States in 1928. Public playgrounds with swings and slides spread through European and American cities from the late 1800s.
Source: content/entries/home/toys.md