Part 2 · Earth and Fire
Tunnels and Rock Drilling
How to drive a tunnel through a hill so that two crews digging from opposite ends meet in the middle — surveying the line over the top and down shafts, breaking rock by hand drilling, wedges and fire, and later with compressed-air drills, timbering soft ground, lining with brick or stone, and keeping the tunnel drained and breathable. For canals, railways, roads, water supply and drainage.
- Difficulty
- ●●●●●
- Time
- A short water tunnel of 100 m takes a small crew a season or two in soft rock; a kilometre through hard rock took years even with compressed-air drills
- Steps from zero
- 24 prerequisites →
This unlocks
—The full path from nothing — 24 steps before this one
- Stone Tools
- Cordage and Rope
- Fire
- Finding and Preparing Clay
- Finding and Identifying Ores
- Simple Machines
- Basic Woodworking
- Hunting and Trapping
- Quarrying and Cutting Stone
- Charcoal
- The Kiln
- Hides and Leather
- Mining and Tunnelling
- Bricks
- The Wheel and Axle
- Firebrick and Refractories
- Bellows
- The Lathe
- Gears
- Iron (the Bloomery)
- Pumps
- The Waterwheel
- The Blast Furnace and Cast Iron
- Bellows to Air Compressors
- Tunnels and Rock Drilling
Do them roughly in this order. See it on the tech tree →
Why it matters
A tunnel lets water, boats, trains and roads go through a hill instead of over or round it. Canals cannot climb; railways can barely climb; water flows only downhill. When a hill stands in the way, a tunnel saves miles of route and dozens of locks (Canals and Locks, Railways, Roads and Bridges). Tunnels also bring water from a distant spring to a town (Pipes, Plumbing and Aqueducts), drain flooded mines and marshes (Mining and Tunnelling), and carry sewers under streets (Sewers and Wastewater).
This chapter builds on Mining and Tunnelling, which covers working underground: timbering, fire-setting, air, water and hauling. Read it first. A tunnel differs from a mine in three ways: it must be exactly on line and on level, it is usually bigger, and it must last for a century or more without falling in.
Explosives were used to break rock in most tunnels after the 1600s (Black Powder (history) tells that history). They are extremely dangerous, kill careless users, and are not covered in this book. Every method here — wedges, fire, hand and compressed-air drilling, splitting — works without them, only more slowly.
How it works
Line and level. A tunnel is a straight line (or a few straight lines) through the hill, at a planned slope. Before digging you fix that line on the surface over the hill, and you work out the height of each end. Then you carry the line underground — from the two ends (portals), and often from shafts sunk from the top — so that several faces can be worked at once and still meet. Small errors grow with distance: a sighting error of 1 mm over 3 m becomes 33 cm over a kilometre. That is why the surveying takes as much care as the digging.
Breaking rock. Hard rock is broken by making cracks and levering out the pieces. You can crack it with heat (Mining and Tunnelling: fire-setting); with wedges driven into drilled holes; or by drilling rows of holes close together and breaking out the rock between them. Drilling is slow by hand and fast with compressed-air drills, which made the long Alpine railway tunnels possible (Bellows to Air Compressors).
Soft ground is the opposite problem: it digs easily but will not stand up. It must be held with timber as soon as it is opened, and then lined permanently with masonry.
Water and air. A tunnel that slopes gently toward its portal drains itself. A tunnel worked downhill, or from a shaft, must be pumped. A tunnel's face is far from fresh air and must be ventilated with ducts and fans or bellows.
What you need
| Item | Notes |
|---|---|
| Surveying gear | Ranging poles, plumb lines with heavy bobs, a water level or levelling instrument, a sighting instrument or telescope on a stand, measuring rods or chain (Surveying and Levelling, The Telescope) |
| Hand drills | Drill steels 20–25 mm thick in sets of increasing length (30, 60, 90, 120 cm), each with a chisel edge slightly narrower than the one before |
| Hammers | Single jack: 1.5–2 kg, short handle. Double jack: 3.5–4.5 kg, long handle |
| Wedges | Iron wedges and plug-and-feathers (a tapered wedge between two half-round shims) (Quarrying and Cutting Stone) |
| Picks, shovels, bars | For soft ground and for levering out loosened rock |
| Compressed-air plant | A compressor and receiver of 5–7 bar, pipes, and pneumatic rock drills (Bellows to Air Compressors) |
| Timber | Squared oak or softwood sets (posts and caps), planks for lagging and poling (Timber Framing and Log Building) |
| Lining | Bricks or dressed stone and lime or cement mortar (Bricks, Stone Masonry, Mortar and Concrete) |
| Mucking | Rails, tubs or barrows, a turntable or switch, horses or a winch (Railways) |
| Ventilation | Wooden or sheet-metal ducts 30–60 cm across, and a fan or bellows (Bellows) |
| Pumps | Hand or powered pumps for downhill faces and shafts (Pumps) |
| Lights | Oil lamps or candles (in coal-free ground); later electric lamps (Lamps and Candles, The Light Bulb) |
Step 1: Survey the line
- Choose the line. Walk the hill and pick two portal sites on solid, dry ground, with room to tip spoil. Keep the tunnel as short as you can. Learn the rock: look at cliffs, quarries, wells and stream beds, and dig trial pits. Avoid crossing water-bearing gravel and soft clay if you can (Rocks and Minerals).
- Set out the line over the hill. Put a ranging pole at each portal. Working from both ends at once, set poles over the hilltop so that, looking along them from either end, every pole hides the one behind it. This is ranging a line (Surveying and Levelling). On a clear night, lamps can be used instead of poles. Mark the final line with permanent stone or masonry pillars on the hilltop, each with a hole or brass pin exactly on the line.
- Fix two marks at each portal, one at the mouth and one 50–100 m back along the line. These are your sighting marks: underground, you keep the tunnel on line by sighting back over them.
- Level. Carry levels over the hill from one portal to the other with a water level or levelling instrument, closing the loop back to where you started (Surveying and Levelling). Decide the floor height at each portal and the slope between.
- The gradient. For drainage, a tunnel should fall at least 1 in 500 (2 mm per metre) toward each portal, with the high point in the middle. Canal tunnels are level, with drainage in side channels; railway tunnels are kept under about 1 in 100.
- Shafts. On a long tunnel, sink shafts from the hilltop down onto the line, every few hundred metres. Each shaft, sunk straight down over the line, adds two more faces and a ventilation route. Fence its mouth, and never let anyone stand at the shaft bottom while loads are moving above.
- Carry the line down a shaft. Hang two plumb lines of thin wire down the shaft, as far apart as the shaft allows (3–4 m), both exactly on the tunnel line as set from the surface marks. Hang heavy bobs (10–20 kg) in buckets of water or oil to stop them swinging. At the bottom, sight past both wires to set the direction of the tunnel. Check it repeatedly; this is the weakest link in the whole survey.
Step 2: Break the rock
Hand drilling
- Single jack. One person holds a short drill steel in one hand and strikes it with a 1.5–2 kg hammer in the other, turning the steel about an eighth of a turn after every blow so the chisel edge strikes fresh rock and the hole stays round.
- Double jack. One person holds and turns the steel with both hands while one or two strikers swing heavy hammers in turn. Faster, but the holder trusts his hands to the strikers: only practised teams.
- Start with the shortest steel. When it is nearly buried, change to the next longer one; each has a slightly narrower edge so it fits the hole. Pour a little water into the hole often and clear the mud with a thin scraper or a wooden spoon — the water also keeps dust down.
- Pace. In hard granite, a hand-drilled hole 1 m deep can take a team an hour or more; in limestone or sandstone, much less. Keep the steels sharp: a smith at the portal forges and hardens a fresh edge on every steel each shift (Blacksmithing, Steel).
Splitting without explosives
- Drill a line of holes, 25–35 mm across and as deep as you want to break, 10–20 cm apart along where you want the rock to part, or round the edge of a block.
- Plug and feathers. Put two feathers (half-round iron shims) in each hole, with a steel wedge (plug) between them. Tap each plug in turn along the row, a little at a time, listening to the ring change. Within minutes to an hour, a crack runs from hole to hole. Lever the slab out with bars (Quarrying and Cutting Stone).
- Fire. In hard, brittle rock such as quartz or granite, fire-setting against the face cracks it deeply (see Mining and Tunnelling for the method and its smoke dangers).
- Lime. Packed into dry holes and wetted, quicklime (Lime) swells as it slakes and can crack soft rock and coal. It is slow and weak, but quiet and safe from sparks.
Compressed-air drills
A pneumatic rock drill is a cylinder with a piston that compressed air shuttles back and forth hundreds of times a minute, hammering a drill steel. A ratchet turns the steel a little on each return stroke. Air at 5–7 bar comes from a compressor or a water-powered trompe outside the tunnel through an iron pipe (Bellows to Air Compressors); its exhaust helps ventilate the face. Small drills are held by hand or on a leg; big ones are clamped to a frame or a wheeled carriage that holds several drills at the face.
Always drill wet. Feed water down a hollow drill steel or squirt it into the hole. Dry drilling fills the air with fine rock dust that scars the lungs (silicosis; see Dangers).
Step 3: The face, timbering and spoil
- Heading and bench. In hard rock, drive a smaller heading — about 2 m high and 2–3 m wide — at the top of the tunnel's final shape. Then take down the bench below it, a few metres behind. The heading tells you the rock ahead before you commit to the full size, and the bench is easier to break because it has two free faces.
- Bar down. After every break, and at the start of every shift, a careful worker taps the roof and walls with a long bar. Sound rock rings; loose rock sounds hollow or "drummy". Pull it down from a safe position before anyone works beneath.
- Timber the soft ground. Where the ground will not stand, set timber sets — two posts and a cap (crown bar), notched together — every 1–1.5 m, with planks (lagging) behind them against the ground (Mining and Tunnelling). In loose ground, forepole: drive pointed planks ahead over the cap, into the ground above the face, before digging forward under them. Never leave unsupported soft ground overnight.
- Muck out. Shovel the broken rock (muck) into tubs on light rails, and haul it out by hand, horse or winch. Put a turntable or a passing loop near the face. Mucking usually takes longer than breaking; plan for it.
- Measure progress each shift, and check line and level every 10–20 m by sighting back to the portal marks and plumb lines.
Step 4: Lining
Rock that is sound, hard and dry may be left bare. Everything else needs a permanent lining, because timber rots in 10–30 years.
- Shape. A horseshoe or round arch carries the ground's weight best (Arches, Vaults and Domes). In swelling clay, add an invert — an upside-down arch across the floor — so the tunnel is a closed ring.
- Brick or stone. Build the side walls on footings, then turn the arch over a wooden centring (a curved timber frame) that is moved forward as each length is finished. Railway tunnels used 2–4 rings of brick (25–45 cm); canal tunnels often less in good ground.
- Fill behind. Pack every gap between lining and rock with rubble and mortar, or the ground will move until it bears on the lining unevenly and cracks it.
- Drain it. Leave weep holes through the lining low on the walls, and a drain along the floor, so water behind the lining escapes instead of building up pressure.
- Mortar. Use hydraulic lime or cement mortar, which sets in the wet (Mortar and Concrete, Portland Cement).
Step 5: Air and water
- Air. Blow air to the face through a duct with a fan, bellows or the compressor's exhaust, or draw foul air out (better while smoke is about). As a rule of thumb, supply at least 6 m³ of fresh air per minute for every person underground (modern tunnel rules ask about this much), and much more after fire-setting or where dust is made. Test the air with a flame before entering (Mining and Tunnelling). Shafts help hugely: hot air from a fire basket at the foot of one shaft draws air through the whole working.
- Water. Drive uphill from the low portal whenever you can; water then runs out by itself along a ditch. Where you must drive downhill, or from a shaft, pump continuously and keep a sump (a pit) at the face. Probe ahead: in suspect ground, drill a few holes 3–5 m ahead of the face before each advance. If water spurts out under pressure, stop and plan drainage before going on — tunnels have flooded in minutes when a face broke into a water-filled cave or gravel bed.
How to tell it worked
- The meeting. When two headings approach, you will hear the other crew's hammers through the rock at 20–30 m. Check line and level once more. A good survey meets within a few centimetres in a few hundred metres; the ancient tunnel of Eupalinos (over 1 km) met with an error of well under a metre.
- Straightness. Sight down a lining with a lamp at the far end: the walls should line up without kinks.
- Dry floor. Water should run steadily out of the portals and no puddles stand in the tunnel.
- No movement. Mark hairline cracks in the lining with a pencil line across and a date. If they grow over months, the ground is moving: add support or an invert.
Note Troubleshooting. Headings don't meet → the plumb lines down the shaft were too close together, or swung. Space them wider, damp them in water, take many readings, and resurvey from the surface marks. Drill steel sticks or the hole goes oval → not turning the steel each blow, or the edge is worn wider than the next steel. Turn steadily; resharpen and gauge every steel. Plug and feathers won't split the rock → holes too far apart or too shallow, or the rock is tough and grainless. Drill closer and deeper, or use fire. Timber sets crushing → ground pressure too high. Set them closer, use heavier timber, and line permanently sooner. Water rising at the face → stop and drain before advancing; drive a drainage heading or pump. Lamps burning dim → bad air. Get out, then improve ventilation.
Dangers
Danger Falls of rock and collapse kill more tunnel workers than anything else. Bar down every shift, timber soft ground immediately, never work under unsupported roof, and never take out a timber set to make room. If the timbers creak, crack or drip fine dirt, get everyone out and add support from behind the danger.
Danger Silicosis. Dust from drilling and breaking quartz-bearing rock — sandstone, granite and many others — scars the lungs permanently; workers die of breathlessness years later. In the Hawks Nest tunnel in West Virginia in the early 1930s, hundreds of workers died after drilling dry through almost pure quartz rock. Drill wet, spray water on broken rock, ventilate, and cover nose and mouth. No profit is worth it.
Danger Bad air and smoke. After fire-setting, the face is full of carbon monoxide and the air may be short of oxygen. Never re-enter until a flame burns normally and the smoke is gone (Mining and Tunnelling). Never use fire or open flames where coal or oily shale is cut: firedamp can explode (Coal and Coke).
- Flooding. Probe ahead in suspect ground; keep a clear escape route to the portal; never work below a full sump without a watch on the pumps.
- Compressed air. Burst hoses whip; never point an air hose at a person. Soft-ground tunnels under rivers were sometimes filled with compressed air to hold back the water, and workers who came out too fast got "the bends" (decompression sickness), which crippled and killed many. Do not attempt this.
- Noise. Rock drills deafen. Plug your ears with wax and wool.
- Hauling. Runaway tubs on a slope crush people. Fit brakes and stop blocks, and keep the track clear.
What this unlocks
Canal tunnels that carry boats through watersheds (Canals and Locks); railway and road tunnels (Railways, Roads and Bridges); water-supply tunnels and drainage tunnels for towns and mines (Pipes, Plumbing and Aqueducts, Sewers and Wastewater, Mining and Tunnelling); underground storage and shelter. The same drilling and splitting skills serve Quarrying and Cutting Stone and the foundations of Dams and Reservoirs and harbours.
How it was first done
Qanats — gently sloping tunnels that bring groundwater from the foot of mountains, dug from a line of vertical shafts — appeared in Iran during the first millennium BC and spread across the Middle East, North Africa and Central Asia; many still flow. Around 700 BC, King Hezekiah's water tunnel in Jerusalem (about 530 m) was dug from both ends, and an inscription records the moment the two crews heard each other and broke through. About 530 BC, Eupalinos of Megara drove a 1,036 m water tunnel through a mountain on the Greek island of Samos from both ends, meeting with an error of under a metre — a feat of pure geometry. The Romans drained Lake Fucino through a 5.6 km tunnel with dozens of shafts in the 1st century AD.
The Malpas tunnel on the Canal du Midi in France (1679–1681) is often said to be the first canal tunnel and the first driven with gunpowder. James Brindley's Harecastle canal tunnel in England (opened 1777) took eleven years. Marc Brunel drove the first tunnel under a navigable river, beneath the Thames in London (1825–1843), using a tunnelling shield he invented. Compressed-air rock drills were first used at scale in the Mont Cenis (Fréjus) railway tunnel under the Alps (1857–1871), and the Gotthard (1882) and Simplon (1906) tunnels followed, with water-flushed drills slowly replacing the deadly dry ones in the early 1900s.
Source: content/entries/earth/tunnelling.md