Part 8 · Chemistry
Oxalic Acid
The sour poison of sorrel and rhubarb leaves, made in quantity by roasting sawdust with caustic potash or by warming sugar with nitric acid. Its clear crystals lift rust and ink stains out of cloth, take black iron stains out of oak, brighten brass, kill mites in beehives, serve as a weighed standard for titration and pull the rare earths out of solution. A teaspoon of it can kill, so it must be stored and labelled like the poison it is.
- Difficulty
- ●●●●●
- Time
- An afternoon for a sugar batch; two days for the sawdust route; a week to collect and work a big pile of sorrel leaves
- Steps from zero
- 14 prerequisites →
This unlocks
Platinum, Salt and Iron-Salt PrintsThe full path from nothing — 14 steps before this one
- Fire
- Stone Tools
- Finding and Preparing Clay
- Sulfur
- Pottery
- The Kiln
- Farming from Seed
- Lime
- Sugar
- Lye and Potash
- Glass
- Saltpeter
- Sulfuric Acid
- Nitric Acid
- Oxalic Acid
Do them roughly in this order. See it on the tech tree →
Why it matters
Rust is the commonest stain in a world of iron tools, iron pots and iron-gall Ink. Lemon juice and sorrel lift it slowly (Laundry and Bleaching Cloth). Oxalic acid does the same job in minutes, because it is the substance in sorrel that does the work, collected and concentrated into clear crystals.
With a jar of it you can:
- take rust spots and ink blots out of linen, cotton, paper and marble;
- derust iron tools in a soaking bath, and brighten tarnished brass and copper;
- take the black iron-tannin stains out of oak and other woods (the marks left by nails, wet iron and water) — the classic wood bleach for furniture and floors (Stairs, Floors and Interior Finishes);
- treat honeybee colonies against the deadly varroa mite (Beekeeping);
- weigh out an exact amount of acid for titration, because the crystals neither soak up water nor lose it in ordinary air (Acids, Bases and Testing, Potassium Permanganate);
- throw down calcium as a white powder to detect it in water and soil (Identifying Substances), and throw down the rare earths to separate them from iron (Rare Earths, Cerium and Phosphors);
It is also a real poison, as rhubarb leaves are.
How it works
Oxalic acid is the simplest acid with two acid "ends": two carbon atoms, each carrying an acid group. It is a far stronger acid than vinegar or citric acid — a 5 % solution is about as sour as weak hydrochloric acid — but it is a solid that dissolves in water: about 10 g in 100 ml of cold water, and many times that in boiling water. The crystals you will make hold two parts of water locked inside them; they melt at about 100 °C.
Three things make it useful:
- It grabs iron. Oxalic acid wraps itself around iron atoms and carries them into solution as a pale yellow-green dissolved salt. Rust is iron oxide, which water cannot touch; with oxalic acid it dissolves. Iron-gall ink and the black stain in oak are iron joined to tannin, and the acid strips the iron off them in the same way.
- Its calcium salt does not dissolve. Calcium oxalate is one of the most insoluble salts there is — it is the gritty stuff of most kidney stones, and the needles in rhubarb leaves. So oxalic acid throws calcium out of any solution as a white cloud, and the reverse is the key to making it: catch oxalate from a messy liquid as calcium oxalate, wash it clean, then free the acid with Sulfuric Acid. The calcium leaves as gypsum, which is also insoluble, and the pure acid stays in the water.
- It is half-burnt carbon. Oxalic acid sits between sugar or wood and fully burnt carbon dioxide. So it can be made by partly burning carbohydrate: chemically, with nitric acid, or with hot caustic alkali. Push the burning too far and you get only carbon dioxide; stop short and you get only brown tar.
What you need
| Item | Amount | Notes |
|---|---|---|
| Sorrel, wood sorrel or rhubarb leaves | 10 kg fresh for a small batch | Method 1 |
| Dry sawdust | 1 kg | Method 2. Pine or any soft, clean wood; no painted or oily wood |
| Caustic potash | about 2 kg as strong lye | Method 2. Wood-ash lye made caustic with lime and boiled down (Lye and Potash) |
| Sugar | 100 g per batch | Method 3. White sugar, or clean honey or molasses (Sugar) |
| Nitric acid | about 350 ml (500 g) of 60–70 % acid per 100 g sugar | Method 3. Nitric Acid |
| Slaked lime | 1–2 kg | To catch the oxalate (Lime) |
| Sulfuric acid | about 3 kg of 25 % acid per kg of dry calcium oxalate | To free the acid (Sulfuric Acid) |
| Vessels | Iron pan 40–50 cm across with a flat bottom; glazed stoneware or glass pots; a porcelain evaporating dish; cloth filters; wooden or glass stirrers | |
| Test materials | Cabbage indicator or test paper (Acids, Bases and Testing), lime water |
Never use aluminium, zinc or galvanised vessels for any stage: the alkali and the acid both eat them.
Where to find it
- Wood sorrel (Oxalis): three heart-shaped leaflets like clover that fold down at night, sharply lemon-sour, in shady woods. Common and sheep's sorrel (Rumex): arrow-shaped sour leaves in meadows and on heaths. Rhubarb: the huge leaves of the garden plant whose red stalks are eaten. The leaves hold about 0.3–1 % oxalic acid by weight; the stalks much less.
- Sawdust from any saw pit or sawmill. It must be dry and free of bark and grit.
- Sugar from cane, beet or honey (Sugar). Starch, from potatoes or grain, also works with nitric acid but foams more.
Method 1: From sorrel and rhubarb leaves
This needs no strong acid or alkali beyond a little sulfuric, and is the right first route. The yield is small: roughly 20–50 g of oxalic acid from 10 kg of fresh leaves. For a stain remover, that is a year's supply.
Salt of sorrel (no acid needed)
- Pound the leaves in a wooden trough or a stone mortar and press out the juice through a cloth (Oils and Pressing). Add a little water to the pulp and press again.
- Clear the juice: bring it to the boil. Green protein curds come up; skim them off and strain through a cloth.
- Boil it down gently to about a tenth of its volume, a thin syrup.
- Cool it in a glazed pot for several days in a cool place. Small, hard, white crystals grow on the sides and bottom. This is salt of sorrel (potassium hydrogen oxalate), sold for centuries as "salt of lemons" for rust and ink stains. It works almost as well as oxalic acid itself.
- Pour off the dark liquid, rinse the crystals with a little ice-cold water, and dry them.
Pure oxalic acid (via calcium oxalate)
- Clear the juice as above, but do not boil it down.
- Catch the oxalate. Stir in thin milk of lime (slaked lime stirred into water) a little at a time until a test paper shows the juice is just neutral. A white cloud forms and settles over a few hours: calcium oxalate, with some green muck.
- Wash it: pour off the liquid, stir the sediment with clean water, settle, pour off again. Repeat 4–5 times until the water is colourless. Dry the white paste.
- Free the acid. In a glazed pot, cover the calcium oxalate with 25 % sulfuric acid — about 0.7 g of pure acid for each gram of dry calcium oxalate, which is close to 3 g of 25 % acid per gram. Keep it warm (60–80 °C, too hot to hold a finger in) and stir for an hour. The fine powder turns into coarser, gritty gypsum.
- Filter off the gypsum through cloth, and wash it with a little hot water, adding the washings to the filtrate.
- Crystallise. Boil the clear liquid down to about a third, and let it cool slowly. Colourless prisms of oxalic acid grow over a day. Recrystallise from the least possible boiling water for a cleaner product.
Method 2: From sawdust and potash
This was the industrial route from about 1856 until the twentieth century. It turns cheap waste into tonnes of acid, and the expensive alkali is recovered and used again.
- Make strong caustic potash from wood ash and lime (Lye and Potash), and boil it down in an iron pot until it is a heavy syrup: about 1.4 kg per litre (weigh a measured cupful against the same cup of water: it should be 1.4 times as heavy). You need about 2 kg of caustic potash (counted as dry solid) per kg of sawdust. Soda lye alone gives poor yields; potash, or a mix with more potash than soda, works far better.
- Mix 1 kg of dry sawdust into the warm lye to a stiff, even paste.
- Fuse. Spread the paste 1–2 cm deep in a wide, flat iron pan over a low fire, outdoors. Heat it slowly to 200–250 °C and keep it there for 2–4 hours, stirring and turning it constantly with an iron paddle so no part sticks and scorches. Without a thermometer: a pine shaving laid on the mass turns golden brown in a minute but does not blacken or flame; a drop of water dances and hisses away.
- Watch the colour. The paste froths, steams and gives off a sweetish smell, then goes yellow and then light brown, and slowly dries to a crumbly, yellow-brown mass. That is the end. If it goes dark brown to black, it is overheated and the oxalate is burning on to carbonate — take it off the fire at once.
- Leach. Cool the mass, break it up, and stir it into about 3 litres of warm water. Settle, and pour or filter the brown liquid off the woody residue. Wash the residue once more.
- Catch the oxalate with milk of lime, as in Method 1, adding lime until a drop of the liquid gives no more white cloud with lime water. Boiling for a few minutes helps the calcium oxalate settle.
- Recover the potash. The clear liquid above the calcium oxalate is now caustic potash again — the lime has taken the oxalate and given back the alkali. Pour it off, boil it down, and use it for the next batch. A works recovered most of its alkali this way.
- Wash, free and crystallise the calcium oxalate exactly as in Method 1, steps 3–6.
Yield. Careful works with good temperature control got about 40 kg of crystals per 100 kg of sawdust. At home, expect a third to a half of that on early batches.
The fusion pan
The fusion pan is the one special tool of Method 2. Forge or rivet a shallow tray from 3–4 mm iron plate (Sheet Metal and Rolling, Blacksmithing): about 50 cm across and 8–10 cm deep, with a flat floor so the layer heats evenly, and two handles. Set it on a low brick or stone firebox with a flue at the back (Chimneys, Stoves and Heating), so flames lick the underside evenly and never reach over the rim. A thin iron plate of 2 cm between the fire and the pan floor, as a heat spreader, prevents hot spots. The stirrer is an iron paddle with a 1 m handle, so you can stir standing back from the fumes and spitting alkali. A good pan is flat enough that water poured in lies evenly with no dry spots; a warped one scorches the thin edges while the deep middle stays wet.
Method 3: From sugar and nitric acid
This is how Carl Scheele first made it in 1776. It is quick and gives clean crystals, but it spends a lot of nitric acid and gives off great clouds of toxic brown nitrogen dioxide. Do it only outdoors, upwind, in small batches.
- Put 100 g of sugar in a porcelain dish or a large glass beaker that holds at least 2 litres — it foams.
- Add about 350 ml of 60–70 % nitric acid (the strength used for etching, Nitric Acid).
- Stand the dish in a pan of hot water (60–70 °C) to start it. Within minutes brown fumes rise and the liquid froths. Take it off the heat at once; the reaction keeps itself going.
- When the fuming slows, put it back on the warm water until no more brown fumes come off — about an hour in all.
- Boil it down to a third of its volume over a gentle fire, outdoors.
- Cool it overnight. Long, colourless needle crystals form. Pour off the acid liquid (it still holds nitric acid; add it to the next batch), and recrystallise the crystals twice from a little boiling water to remove the nitric acid.
Expect very roughly as much oxalic acid as the sugar you started with, by weight, from a good run; often less.
Using it
Keep a stock solution of 50 g of crystals per litre of warm water (5 %) in a labelled, stoppered bottle, and dry crystals for stronger work. Always rinse well afterwards: left in cloth or wood, the acid slowly weakens fibres.
| Job | Strength | How |
|---|---|---|
| Rust spots and ink on linen or cotton | 5 % warm | Stretch the cloth over a bowl, wet the stain, dab on the solution with a glass rod; the stain fades in 1–5 minutes. Rinse at once in plenty of water, then wash. Not on coloured cloth until tested on a hidden corner |
| Ink blots on paper | 2–5 % | Touch with a brush, blot with clean paper, then a brush of clean water. Works only on iron-gall ink, not soot ink |
| Black stains in oak and other wood | 10 % hot (100 g per litre, saturated when cold) | Brush over the whole board, not only the stain, so it does not leave a pale patch. Dry, repeat if needed. Neutralise with a wash of borax or baking-soda water (a spoonful per litre), rinse, dry a day, then sand lightly with a dust mask |
| Derusting iron and steel | 5–10 % | Soak for 2–12 hours in a wooden or stoneware tub; scrub with a stiff brush. The metal comes out dull grey. Rinse, dry by the fire at once, and oil (Corrosion and Its Prevention) |
| Brass and copper | 2–5 % | Wipe on, rub with a cloth, rinse, dry and polish. Do not leave copper in it for long |
| Marble and stone | paste (below) | Rubbed on with felt, it removes rust marks and leaves a hard shine. Test first: it etches limestone if left wet |
| Varroa mites in bees | 3.5 % in syrup | See below |
The rust remover
A rust remover is a ready-to-use jar for the household: a soaking bath for tools and a scouring paste for sinks, pots and stone.
- Bath: dissolve 75 g of crystals in 1 litre of warm water in a stoneware crock with a wooden lid and a rack of wooden slats in the bottom, so small parts do not sit in the sludge. Mark the crock with the poison sign. Reuse it until it turns muddy green and stops working, then neutralise it with chalk before pouring it away.
- Oxalic acid paste: grind 1 part of crystals with 9 parts of fine pumice or tripoli powder (Abrasives and Grinding Stones) and store dry in a stoppered jar. To use, wet the surface, sprinkle the powder, rub with a damp cloth, and rinse. This is the scouring powder that cleans rust rings from enamel and pot marks from sinks. Never use chalk or whiting as the abrasive: chalk eats the acid.
A good rust remover lifts a fresh rust spot from white linen in under five minutes and leaves no yellow ring after rinsing. A bad one is either too weak (crystals contaminated with gypsum or potash; the stain only fades) or leaves the cloth tender because it was not rinsed out.
Against varroa mites
For honeybees, dissolve 35 g of oxalic acid crystals in 1 litre of 1:1 sugar syrup (equal weights of sugar and warm water). In midwinter, when the colony has no sealed brood, open the hive on a mild day and trickle 5 ml of the warm syrup from a syringe or measured spoon onto the bees in each gap between combs, no more than 50 ml per colony. The acid kills mites riding on the bees. Treat once a year only: repeated doses harm the bees. Mix it fresh — it turns brown and stronger-tasting in storage. This is a widely used modern treatment; see Beekeeping.
In the laboratory
- A weighed acid. Dissolve 63.0 g of pure, air-dry crystals in water to make exactly 1 litre. Millilitre for millilitre, this matches the soda standard of Acids, Bases and Testing, and lets you check that standard or make a second one. It also standardises Potassium Permanganate solution: in warm dilute sulfuric acid, oxalic acid bleaches the purple drop by drop until one drop stays pink.
- Calcium test. A few drops of oxalic acid or salt of sorrel in a little water made faintly alkaline with ammonia: a white cloud means calcium (Identifying Substances, Finding and Purifying Water).
- Rare earths. Oxalic acid throws the rare earths out of acid solution, leaving iron behind (Rare Earths, Cerium and Phosphors).
How to tell it worked
- The crystals are colourless and clear, long prisms or needles, and leave no ash. Heat a few in an iron spoon, outdoors: they melt, give off steam, and then vanish almost completely. A white or grey residue is potash, lime or gypsum — recrystallise.
- The lime test. A few drops of your solution into lime water gives an instant thick white cloud that does not dissolve when you add vinegar.
- The permanganate test. It bleaches a pink drop of warm, acidified permanganate with tiny bubbles.
- The stain test. It removes a rust spot from a scrap of white linen within five minutes.
Note Troubleshooting. Sawdust mass turned black and gave little or no oxalate → overheated or unstirred. Lower the fire, thin the layer, stir all the time. Sawdust mass stayed sticky and pale → too cool, too short, or the lye was too weak or mostly soda. Use stronger potash lye and hold 200–250 °C longer. No crystals from the final liquid → too dilute, or too much sulfuric acid left in it. Boil down further; check the gypsum was fully converted (gritty, not slimy). Crystals are brown or sticky → plant or wood tars. Recrystallise twice; or boil the solution with a handful of powdered charcoal and filter (Activated Charcoal). Rust stain went yellow-brown instead of disappearing → not rinsed out; the iron oxalate dried in the cloth. Re-wet, dab again, and rinse in running water.
Dangers
Danger Oxalic acid is a poison. As little as 5 g — a heaped teaspoon of crystals — can kill an adult, and less a child. It burns the mouth and throat, causes vomiting and collapse, pulls calcium out of the blood (twitching, cramps and fits), and blocks the kidneys with crystals over the following days. The crystals look exactly like Epsom salt and washing soda, and in the 1800s hundreds of people died from that mix-up. Store it locked, in a distinctive bottle, with the poison mark, never in the kitchen.
If swallowed: do not make the person vomit. At once give a glass or two of milk, or chalk stirred in water — the calcium catches the acid in the stomach as harmless, insoluble calcium oxalate. Then get them to whoever gives medical care (Emergencies).
Danger Nitrogen dioxide (Method 3). The brown fumes from sugar and nitric acid can kill hours after you breathe them, when the lungs fill with fluid. Work outdoors, upwind, and leave the area if you smell them. See Nitric Acid.
Danger Hot caustic potash (Method 2). The fusion paste is boiling lye with wood in it; it spits and blinds. Wear eye protection and wool or leather, keep water and vinegar nearby (Lye and Potash). The fusion also gives off hydrogen, which burns: no closed vessels, and keep flames from the top of the pan.
- Skin. Dilute solutions sting cuts and, used for weeks without gloves, make fingertips cracked and painful. Wear gloves or rinse hands often.
- Dust. Sanding oak treated with oxalic acid puts the acid in the air: neutralise first and wear a mask.
- Never heat oxalic acid with strong sulfuric acid. The mix gives off carbon monoxide, which kills without smell.
- Rhubarb and sorrel leaves are poisonous in quantity. Cooked sorrel in sauce is fine in moderation; never eat rhubarb leaves (Foraging Wild Food).
What this unlocks
- Cleaner textiles and paper: rust and ink stain removal (Laundry and Bleaching Cloth), and restoring old documents (Libraries and Preserving Knowledge).
- Wood finishing: bleaching oak and cleaning weathered timber before oiling (Stairs, Floors and Interior Finishes, Furniture).
- Healthy hives in a world with varroa (Beekeeping).
- Analysis and separation: calcium testing (Identifying Substances), titration standards (pH, Indicators and Buffers, Potassium Permanganate), and the separation of the rare earths (Rare Earths, Cerium and Phosphors).
- Photography: ferric oxalate, made by dissolving fresh iron hydroxide in oxalic acid, is the light-sensitive salt of platinum and kallitype prints (Photography).
How it was first done
Salt of sorrel was crystallised from sorrel juice by the 1600s and sold in Europe for taking out ink and rust stains. In 1776 the Swedish chemist Carl Wilhelm Scheele made the acid itself by warming sugar with nitric acid, and in 1784 he showed it was the same acid as in sorrel. In 1829 the French chemist Joseph Gay-Lussac found that sawdust heated with caustic potash gives oxalate, and from about 1856 the firm of Roberts, Dale and Co. near Manchester ran it as a large factory process, recovering the alkali with lime. Later factories made it from sodium formate.
Source: content/entries/chemistry/oxalic-acid.md