Part 15 · Knowledge and Science
The Darkroom and the Enlarger
A light-tight room with a safe coloured light, a row of trays and a running tap turns photography from a sunshine craft into a daily trade. The enlarger, a camera run backwards, prints a small negative as large as you like on fast bromide paper. How to build the room, the safelight, the trays, the tanks, the timer and the enlarger, and how to make and test good prints.
- Difficulty
- ●●●●●
- Time
- A week to fit out a room; two to four weeks to build an enlarger; an hour for a first test strip
- Steps from zero
- 21 prerequisites →
This unlocks
—The full path from nothing — 21 steps before this one
- Fire
- Cordage and Rope
- Stone Tools
- Finding and Preparing Clay
- Finding and Identifying Ores
- Hunting and Trapping
- Basic Woodworking
- The Kiln
- Pottery
- Charcoal
- Hides and Leather
- Lime
- Lye and Potash
- Glass
- Bellows
- Copper Smelting
- Lead
- Laboratory Glassware
- Lenses
- Gold and Silver
- Photography
- The Darkroom and the Enlarger
Do them roughly in this order. See it on the tech tree →
Why it matters
Photography can be done with a dark cloth and a candle. But once photographs serve a whole community (identity records, medical pictures, Maps and Mapmaking, copies of drawings), you need a room where a person can work all day with film and paper that a moment of daylight would ruin.
The darkroom is that room. The enlarger is its central machine. It projects a small negative onto paper, so a camera can be small and light, film is cheap, and the print can still be large. A 24 × 36 mm negative enlarged eight times gives a 19 × 29 cm print. Enlarging also lets you crop the picture and lighten or darken parts of it by hand.
How it works
Light-sensitive layers are blind to some colours. Plain silver bromide, as made in Photography, responds only to violet and blue, so it can be handled in dim amber light. Emulsions sensitised to green as well (orthochromatic) need deep red light; those sensitive to all colours (panchromatic), total darkness. A safelight gives only colours the material cannot see.
The enlarger is a camera run backwards. A lamp shines through the negative and a lens throws a magnified image of it onto paper. From the lens equation (Lenses), for focal length f and magnification m:
- lens to paper = f × (1 + m)
- lens to negative = f × (1 + 1/m)
With a 50 mm lens at 8 times, the paper is 450 mm below the lens and the negative 56 mm above it.
Exposure grows with the square of the size, roughly as (1 + m)². Going from 4× to 8× needs (9 ÷ 5)² ≈ 3.2 times the exposure.
Choose the lens to suit the negative. The enlarging lens should have a focal length about equal to the diagonal of the negative: 50 mm for 24 × 36 mm film, 75–80 mm for 6 × 6 cm, 105 mm for 6 × 9 cm and 135–150 mm for 9 × 12 cm plates. Shorter does not cover the corners.
Even light. A bare lamp lights the middle of the negative more than the edges. Two remedies:
- A diffuser, a sheet of opal or ground glass. Soft, hides dust and scratches, but wastes light.
- A condenser, two large plano-convex lenses, curved faces together, that bend the lamp's light so all of it passes through the enlarging lens. Bright and crisp, but shows every speck of dust and gives more contrast.
What you need
| Item | Amount or size | Notes |
|---|---|---|
| A room | At least 2 × 2.5 m, ideally 2.5 × 3.5 m | Inner room, or a lean-to with no windows |
| Timber, boards, black paint | For door maze, benches, vents | Soot in glue or linseed oil makes matt black (Pigments, Paints and Varnish) |
| Running water and a drain | 5–10 litres a minute while washing | Pipes, Plumbing and Aqueducts; a raised barrel and hose works |
| Coloured glass or dyed cloth | For safelights | Copper-ruby or amber glass (Glass), madder-red cloth (Dyes and Mordants) |
| Trays | 4, each a few cm larger than the biggest print | Glazed stoneware, glass, enamel or waxed wood |
| Enlarger lens | f ≈ negative diagonal | A good camera lens works (Lenses) |
| Condenser lenses | 2, diameter 1.2–1.4 × negative diagonal | Or one sheet of opal glass |
| Lamp | 75–150 W opal bulb, or a limelight or paraffin lamp | The Light Bulb |
| Paper and chemicals | Made as below |
The darkroom
- Choose the room. An inner room with no window is easiest. Floor of concrete, tile or tarred boards, falling gently to a drain. Keep it at 18–24 °C: developers are slow when cold and fog when hot.
- Black out. Close every window with boards, then a layer of thick black cloth or tarred paper. Fill gaps round pipes and frames with putty or felt.
- Build a light maze instead of a door. A passage about 70 cm wide that turns twice through a right angle, its walls painted matt black, lets people in and out without a door, and lets air through. Light cannot turn two corners off black walls. Otherwise, a door with felt strips and a black curtain inside it.
- Ventilate. Aim for 6–10 changes of air an hour. Fit a vent low on one wall and one high on the other, each through a light-trapped box, a zigzag of black-painted baffles. A small fan in the high vent (Fans, Vacuum Cleaners and Washing Machines) pulls warm air out.
- Split dry from wet. The dry bench for the enlarger and paper on one wall; on the opposite wall the wet bench, about 90 cm high and 60 cm deep, with a raised rim 3 cm high and a fall to the sink. Line it with sheet lead, bitumen-painted boards or glazed tiles (Laying Tiles and Mosaics). Never let a drop from the wet side reach the dry side.
- Paint the walls pale. They reflect the safelight and make work easier; only white light is a danger. Keep the maze and the area round the enlarger black.
- Test. Sit in the dark room for 10 minutes until your eyes adjust, and seal every glimmer you see.
The safelight
A safelight is a closed, ventilated box with a lamp inside and a window of coloured glass or cloth.
- The box. Sheet tin or thin wood, about 20 × 15 × 12 cm, black inside. For a candle or oil lamp, add a capped chimney and a few low air holes, bent so light cannot leak out.
- The window. For bromide paper: amber or yellow-orange glass, or two layers of yellow and one of orange cloth. For orthochromatic film: copper-ruby glass or 3–4 layers of madder-red cloth. A sheet of ground glass behind the coloured layer spreads the light evenly.
- The lamp. A 15 W electric bulb, a candle, or a small oil lamp. Brighter is not better.
- Hang it at least 1.2 m from the paper; indirect light off the ceiling is safer.
- Test it with the coin test from Photography, under the conditions you really work in. Paper must survive at least 4 minutes under the light with no trace of the coin. Re-test every few months: dyes fade and become unsafe.
Print trays
You need at least four: developer, stop bath, fixer, wash. Each should be 5–8 cm larger than the paper each way and 5–6 cm deep. For 24 × 30 cm prints, trays of about 30 × 38 cm.
- Best: glazed stoneware (Stoneware and Porcelain) or thick glass. Throw them on a slab, as for a large dish (Pottery), with two or three low ribs on the bottom so the paper does not stick, and a pouring lip at one corner.
- Good: enamelled iron (Enamel on Metal), as long as the enamel is not chipped. Bare iron, copper, zinc or tin spoil developers and stain prints.
- Makeshift: a shallow wooden box, its joints glued and then soaked in hot beeswax and paraffin or painted inside with three coats of bitumen (Tar, Pitch and Glue).
Keep each tray for one chemical only: a trace of fixer in the developer fogs prints. Use tongs of bamboo or hardwood, one pair for developer and one for the rest.
A print washer is a deep tray or a wooden box with water entering at the bottom through a perforated pipe and leaving over a lip at the top. A dozen prints in a 40 × 50 cm washer is plenty.
The darkroom timer
- The metronome. A pendulum swings once in a time set by its length: 1 second for a pendulum 99 cm long, half a second for 25 cm. Count its swings aloud; it needs no light.
- A clock with a big seconds hand, at least 20 cm across, with white figures that show under the safelight.
- An electric exposure timer. A synchronous clock motor turning a cam that holds a switch closed for a set number of seconds, or a capacitor charging through a resistor until a relay drops out (Resistors, Capacitors and Coils). It switches the enlarger lamp.
The developing tank
Film and plates are developed in closed tanks, so the lights can go on once they are loaded.
For plates: a box of glazed stoneware or glass with vertical grooves moulded or cut into two opposite walls, 6–8 mm apart, holding a dozen plates on edge. Lower the plates into the developer in the dark and fit a lid; every minute, lift, drain and lower them again.
For roll film: the film must be wound in a spiral without any turn touching the next, or the developer cannot reach it.
- The tank. A cylinder of glazed stoneware, ebonite, enamelled tin or glass, about 9 cm across and 12 cm tall for one roll of 35 mm film (it takes about 300 ml); 9 × 10 cm with a wider reel for 6 cm roll film (about 500 ml).
- The light-trap lid. Through the lid runs a funnel whose spout, about 2 cm across, dips into a small cup fixed below it. Liquid poured into the funnel fills the cup and overflows into the tank, but light would have to turn back on itself twice, so none gets in. Paint both matt black. A cap over the funnel lets you turn the tank upside down.
- The reel. The easiest version to make is an apron: a strip of clear film base (Photographic Film Base) slightly wider than the film, with a row of raised bumps pressed into each edge every 2 cm by a hot rounded punch. Lay the film on the apron, emulsion side up, and roll the two together loosely. The bumps hold the turns about 1.5 mm apart. The better reel is a spiral of stainless or nickel wire (Nickel and Cobalt) about 2 mm between turns, soldered to three cross-bars on each side.
- Use it. Load the reel and close the lid in total darkness; then lights on. Pour in developer at 20 °C, tap the tank to dislodge bubbles, and invert it 4 times in the first 30 seconds, then twice every 30 seconds. Then stop, fixer, and wash with the lid off.
Time and temperature. Find each developer's time at 20 °C by testing; for each 1 °C warmer, shorten it by about 10 %. Below 15 °C, warm the developer; above 26 °C, the gelatin softens and may lift.
The enlarger
Simplest: the horizontal enlarger
Lay your camera on its side on a bench, its back to a window covered with opal or ground glass, its lens facing a board on the wall 1–2 m away. Put the negative where the ground glass was, emulsion towards the lens. Slide the camera until the image on a white card on the board is the size you want, focus, then swap the card for paper and use the lens cap as shutter. Most enlargements before about 1900 were made like this, often with sunlight from a mirror outside the window. Daylight changes minute to minute; a lamp box behind the negative is steadier.
The vertical condenser enlarger
- Baseboard. Hardwood, about 50 × 60 cm and 25 mm thick, with battens beneath so it lies flat.
- Column. A straight, seasoned hardwood post 5 × 7 cm and 90–110 cm tall, mortised and braced into the back of the board so it stands exactly square to it (Doors, Windows and Joinery). Or a steel tube (Metal Pipes and Tubes). Plane a flat face on the front for the carriage to slide on.
- Carriage. A wooden or cast block that slides up the column, with a clamping screw. The head is heavy, so hang a counterweight on a cord over a pulley at the top of the column, or the head will drop when unclamped.
- Lamphouse. A tin box about 15 × 15 × 15 cm for 35 mm or 6 × 6 negatives, larger for plates, painted matt white inside, with light-trapped vents top and bottom. The lamp is an opal bulb of 75–150 W (The Light Bulb). It must be adjustable up and down a few centimetres, so that you can put its image into the enlarging lens.
- Heat filter. Every lamp heats the negative (before electric light, a paraffin lamp or limelight from Hydrogen, Oxygen and Gases was used). A glass cell of water 2–3 cm thick between lamp and condenser stops most of the heat.
- Condenser. Two plano-convex lenses, curved faces facing each other and almost touching. Diameter 1.2–1.4 times the negative diagonal: about 60 mm for 35 mm film, 130–150 mm for 6 × 9 cm, 180–200 mm for 9 × 12 cm plates. Simple ground lenses do (Lenses). Or use a sheet of opal glass instead.
- Negative carrier. Two thin metal plates with an opening the size of the negative, hinged together like a book, the negative clamped between them. It slides into a slot under the condenser.
- Bellows and lens board. A bellows of black cloth or thin leather, folded over card stiffeners (Leatherwork and Harness-Making), joins the negative stage to a lens board below. A rack and pinion (Gears) or a fine screw moves the lens board 5–10 cm for focusing.
- Red filter. A disc of red glass on a swing arm under the lens. With it in place you can position the paper by the safe red image, then swing it aside to expose.
- Align it. The negative, the lens board and the baseboard must be exactly parallel. Check with a spirit level, then focus on the grain and look at all four corners with a magnifier; shim the lens board until all are sharp.
Centre the lamp. Remove the negative, open the lens fully and look at the baseboard. Move the lamp up and down until the disc of light is even with no dark ring at the edge or hot spot in the middle.
The enlarging easel
A flat board, painted yellow or matt black (white reflects light back through the paper), with two L-shaped steel or brass arms that slide over the edges of the paper. They hold it flat and leave a clean white border, typically 5–10 mm wide.
Making prints
Bromide paper
Make a silver bromide gelatin emulsion exactly as for dry plates in Photography, but ripen it for only 10–15 minutes: the paper will be slower and give more contrast, which suits prints. Coat smooth, well-sized Paper that has first been given a thin layer of gelatin with a little white barium sulfate ("baryta", from barite) to make it bright and to stop the emulsion soaking in. Pour or brush about half the amount used per area on a plate, and dry it flat in the dark. Coating paper by the roll, and gaslight and chloride papers, are in Making Photographic Papers and Plates.
Developer for prints
- Hydroquinone developer (Organic Synthesis and Fine Chemicals): a contrasty formula for line work. For pictures, dilute it about 1 part to 4 of water and test.
- Ferrous oxalate developer, the bromide-paper developer of the 1880s, made from iron and oxalic acid: dissolve 1 part potassium oxalate in 3 parts warm water (Oxalic Acid); separately 1 part ferrous sulfate (green vitriol) in 3 parts water with 2–3 drops of Sulfuric Acid per 100 ml. Just before use, pour 1 part of the iron into 4 parts of the oxalate, never the other way round, and add a few drops of 10 % potassium bromide. It is a clear orange-red. After developing, rinse the print in dilute acetic acid (a spoonful of strong vinegar in a litre of water) to clear the iron, then fix.
Stop bath: about 2 % acetic acid, distilled vinegar diluted to that strength (Vinegar and Pickling). Fixer: hypo, 20 g in 100 ml, as in Photography.
Step by step
- Clean the negative with a soft brush.
- Compose and focus. Negative in, emulsion side down, lens wide open, room lights off. Raise the head until the image fills the easel; focus with a magnifier on the grain.
- Stop down the lens 2–3 stops (to about f/8). This sharpens the corners and lengthens the exposure to a useful 5–30 seconds.
- Make a test strip. Lay a strip of paper across an important part of the image. Expose it all for 2 seconds; then cover a fifth with card and give 2 more; cover two-fifths, 4 more; three-fifths, 8; four-fifths, 16. The bands have had 2, 4, 8, 16 and 32 seconds.
- Develop the strip for the full time, 90 seconds to 2 minutes at 20 °C, rocking the tray. Stop 30 seconds, fix 1 minute, then look at it in white light.
- Choose the exposure: the band where the darkest shadows are fully black and the brightest highlights just show a trace of tone.
- Expose the whole print, develop the full time (never pull a print early because it looks dark; it then looks muddy), stop 30 seconds, fix 5–10 minutes, wash. Paper prints need at least an hour of running water to last; glass plates and film 30 minutes.
- Dry prints face down on muslin stretched on wooden frames.
Dodging and burning. A small card on a wire, waved over a shadow during part of the exposure, lightens it ("dodging"). A card with a hole, letting extra light onto a pale sky after the main exposure, darkens it ("burning in"). Keep it moving, or the edge shows.
Contrast. Print a flat negative with a condenser or a contrasty paper, a harsh one with a diffuser or a softer paper. Next time, develop the film longer for more contrast, shorter for less.
How to tell it worked
- Blacks are black, whites are white. Lay the print beside a scrap of unexposed paper that has been developed and fixed: the borders should match it. Grey borders mean fog.
- Sharp all over. Look at grain in all four corners with a magnifier.
- Fully washed. The silver-nitrate drop test from Photography on a margin stays clear.
- Safelight safe. The coin test, under real working conditions.
Note Troubleshooting. Grey fog over the whole print, borders included → safelight unsafe, light leak, old paper or developer too warm. Do the coin test; develop a sheet of paper with no exposure at all. Dark middle, pale corners → lamp not centred over the condenser. Adjust it with no negative in place. Sharp on one side only → negative, lens and baseboard not parallel. White spots → dust on the negative or the condenser. Black spots or lines → scratches or pinholes in the negative. Brown or yellow stains → developer exhausted or contaminated with fixer; or poor fixing. With ferrous oxalate, skipped the acid rinse. Muddy blacks → print pulled early, developer cold or exhausted. Streaks on film → not enough agitation in the first 30 seconds, or turns of the film touching on the reel.
Dangers
Danger Water and mains electricity in the same small room can kill. Keep every electric switch, socket and lamp on the dry side, or high on the wall where wet hands cannot reach. Use pull cords and foot switches. Earth every metal enlarger and lamp housing (Wiring and Electrical Safety). Never handle the enlarger with wet hands.
Danger A flame in a sealed room uses up the air and makes carbon monoxide, which gives no warning. Never run an oil lamp, candle safelight, limelight or stove in a darkroom without ventilation, and never sleep in one. Headache, dizziness or sleepiness: get out into fresh air at once.
- Developers irritate skin and some (pyrogallol, hydroquinone) are poisonous. Use tongs and wash hands often.
- Nitrate film is fiercely flammable and must never be near an enlarger lamp or heat filter (Photographic Film Base).
- Recover silver from used fixer rather than pouring it away (Silver Nitrate and Silver Salts).
What this unlocks
The darkroom serves Microfilm and Document Storage, X-Rays, Copying Documents and Xerography, the enlarged negatives of Platinum, Salt and Iron-Salt Prints, plates for Lithography and Offset Printing and Screen Printing, the long film of Cinema: Film Cameras and Projectors, and Colour Photography. Run backwards, the enlarger becomes a reducing camera, the first step towards Making Microchips.
How it was first done
Early photographers worked under yellow-glazed windows or in tents of yellow cloth. The American David Acheson Woodward patented his daylight solar camera enlarger in 1857. Fast gelatin bromide paper, made commercially from the late 1870s and 1880s, made enlarging with artificial light practical, and ferrous oxalate was its usual developer. Electric lamps and condenser enlargers became normal around 1900–1910, and daylight developing tanks for roll film appeared at about the same time. Small cameras using 35 mm cine film, above all the Leica of 1925, made enlarging the normal way to print, and the darkroom changed little after that until digital photography replaced it.
Source: content/entries/knowledge/darkroom-and-enlarger.md