◆ Rebuild

Part 14 · Electronics and Computing

Integrated Circuits

Instead of making transistors one at a time and wiring them together, print them — hundreds or millions at once — onto a single slice of silicon, using light, glass masks, acids and furnaces. How the planar process works, what the first realistic chip looks like, and why making them needs a whole industry.

Difficulty
●●●●●
Time
Months to set up a small chip workshop once pure silicon exists; a week or more per batch of wafers; years to reach a working processor
Steps from zero
47 prerequisites →

You need first

Semiconductors and the TransistorPhotography

This unlocks

The ComputerMaking MicrochipsSatellites, Mobile Phones and GPS (Overview)
The full path from nothing — 47 steps before this one
  1. Fire
  2. Cordage and Rope
  3. Stone Tools
  4. Finding and Preparing Clay
  5. Finding and Identifying Ores
  6. Sulfur
  7. Hunting and Trapping
  8. Basic Woodworking
  9. The Kiln
  10. Pottery
  11. Charcoal
  12. Hides and Leather
  13. Lime
  14. Bricks
  15. Salt
  16. Mercury
  17. Lye and Potash
  18. Fermentation
  19. The Wheel and Axle
  20. Glass
  21. Firebrick and Refractories
  22. Bellows
  23. Saltpeter
  24. The Lathe
  25. Gears
  26. Copper Smelting
  27. Iron (the Bloomery)
  28. Lead
  29. Laboratory Glassware
  30. Sulfuric Acid
  31. Pumps
  32. The Waterwheel
  33. Lenses
  34. Blacksmithing
  35. Gold and Silver
  36. Hydrochloric Acid
  37. The Battery
  38. The Vacuum Pump
  39. Magnets
  40. The Light Bulb
  41. Copper Wire
  42. Photography
  43. The Generator
  44. The Vacuum Tube
  45. The Electric Arc Furnace
  46. Pure Silicon
  47. Semiconductors and the Transistor
  48. Integrated Circuits

Do them roughly in this order. See it on the tech tree →

Why it matters

A The Computer needs thousands of switches. Built from separate transistors, each must be made, tested, mounted and soldered, and every solder joint is a place where the machine can fail. By the late 1950s engineers called this "the tyranny of numbers": machines big enough to be useful had too many parts to ever work at once.

The integrated circuit (IC, or "chip") escapes the tyranny. Transistors, resistors and the wires joining them are all made at once, in one piece of silicon, by a process more like Printing than like assembly. Make the pattern once, and every chip on every wafer gets it. A chip with ten transistors and a chip with ten thousand take roughly the same work to make. That is why computing became cheap: the cost of a transistor has fallen more than a billion times since 1960.

This chapter is honest about difficulty. Chips are the summit of the technology tree. They need Pure Silicon grown as perfect crystals, very pure chemicals and water, steady furnaces, a The Vacuum Pump, precise Photography and Lenses, and a dust-free room. No one person can supply all of that from scratch. But the first chips (1958–1965) were made with 1950s tools, with lines 20–50 micrometres wide — about half the width of a hair — and in recent years individual amateurs have made working chips of a few to a few thousand transistors in a garage, using bought chemicals and wafers. A rebuilt civilisation that already makes transistors (Semiconductors and the Transistor) can reach simple chips with a dedicated workshop of a few dozen skilled people.

How it works

The planar idea

Three facts make chips possible:

  1. Silicon grows its own glass. Heat silicon to about 1,100 °C in oxygen or steam and it grows a skin of silicon dioxide — glass, the same stuff as quartz — that is hard, insulating and smooth.
  2. The glass blocks dopants. Boron and phosphorus at high temperature soak into bare silicon, but hardly at all through a layer of oxide. So oxide with holes in it is a mask: dopant gets in only through the holes.
  3. Light can cut the holes. Coat the oxide with a varnish that hardens where light falls (photoresist), shine light through a glass plate printed with the pattern, wash away the unhardened varnish, and dissolve the oxide in acid wherever the varnish has gone. This is photolithography — "writing in stone with light" — and its ancestor is the very first photograph, made by Nicéphore Niépce in the 1820s with bitumen that hardened in sunlight.
1. Grow oxide Wafer in steam at 1,100 °C: a skin of glass (silicon dioxide), 0.5 μm 2. Coat with resist Light-hardening varnish, spun on thin and even, about 1 μm 3. Expose through a mask Light hardens the resist it reaches; the dark spot on the mask shields it mask 4. Wash off soft resist The shaded resist washes away, leaving a window 5. Etch the oxide Acid dissolves the glass only where the window is open acid 6. Strip resist, diffuse Dopant gets into the silicon only through the window in the glass dopant silicon oxide (glass) resist hardened resist doped silicon
Fig. 1 The basic cycle, repeated for every layer of a chip: grow oxide, coat with resist, expose through a mask, wash, etch, then diffuse dopant through the window.

Repeat the cycle with different masks, lined up exactly on top of each other, and you build up p-type and n-type regions, thin and thick glass, and finally a layer of aluminium wiring on top. Everything stays flat ("planar"), protected under its glass, and connected by metal lines printed like the rest.

The simplest useful chip transistor

The easiest transistor to make on a chip is not the junction transistor of Semiconductors and the Transistor but the MOS transistor (metal–oxide–semiconductor). It needs only four masks.

Take n-type silicon. Make two p-type islands, the source and the drain, a few tens of micrometres apart. Over the gap, grow a very thin, very clean layer of oxide, and lay an aluminium gate on top of it. Now:

  • Gate at the same voltage as the source: the n-type gap separates the two islands, and no current flows.
  • Gate made negative (about −10 V): it pulls holes up to the surface under the oxide, forming a thin p-type channel that joins source and drain. Current flows.

The gate draws no current at all — it is insulated by the oxide — so one transistor's output can drive many gates. Wire a MOS transistor with a resistor (or another transistor as a load) and you have an inverter; two in series or parallel make NAND and NOR; from those, everything in The Relay Computer and The Computer follows.

Seen from above about a tenth of a millimetre across S G D Mask 1 p-type source and drain Mask 2 gate window (thin oxide) Mask 3 contact holes Mask 4 aluminium wiring Cut through the middle SGD Thick oxideabout 1 μm Thin oxide0.1 μm, very clean Aluminiumwiring p-type regionsboron diffused in Channelforms when G ismade negative Wafern-type silicon
Fig. 2 A metal-gate MOS transistor, the simplest transistor to make on a chip. Left: the four mask layers seen from above. Right: a cut through the middle. A negative voltage on the gate draws a thin conducting channel between source and drain.

What you need

Item Notes
Silicon wafers Single-crystal n-type silicon (Pure Silicon), sliced 0.3–0.5 mm thick, lapped flat and polished to a mirror
Oxidation and diffusion furnaces Tubes of fused quartz 3–5 cm wide, heated by resistance wire to 900–1,150 °C, holding temperature within ±2–5 °C over the middle 20 cm. Oxygen (or clean air) and steam bubbled from boiling pure water
Dopant sources Boron: boric acid from borax. Phosphorus: phosphoric acid from bone ash or rock phosphate and Sulfuric Acid
Photoresist Dichromated gelatin or fish glue (gelatin plus 1–3% potassium dichromate, obtained by trade or from a chromate works, Chromium and Its Compounds), or bitumen dissolved in turpentine
Masks Fine-grained photographic plates (Photography); two cameras with very good Lenses
Ultraviolet light Strong sunlight, or an electric arc or mercury lamp
Etchants Hydrofluoric acid (from fluorite and sulfuric acid), best buffered with ammonium fluoride, for oxide; warm phosphoric acid for aluminium
Aluminium A few grams of the purest Aluminium, evaporated from a hot tungsten coil in a vacuum chamber (The Vacuum Pump)
Water Distilled twice in glass (Distillation), many litres a day
Inspection A The Microscope at 50–200×; fine steel needles on screw-driven holders to touch test pads
A clean room A closed room with filtered air, washed floors and walls, people in clean cotton gowns and caps (Clean Rooms)

Where to find it

Most raw materials appear elsewhere in this book: quartz sand and fluorite (a glassy, cubic, often purple or green mineral, soft enough to scratch with a knife, that glows when heated) in Rocks and Minerals; chromite (heavy black grains in dark serpentine rocks), from which a chromate works makes the dichromate (Chromium and Its Compounds); bitumen from natural seeps (Tar, Pitch and Glue); borax from dry salt lakes; rock phosphate and bones for phosphorus. Gelatin comes from boiling hide and bone (Glues and Adhesives).

What you cannot find in nature is purity. Every chemical that touches the wafer — water, acids, gases, resist — must be cleaner than anything else your civilisation makes. Sodium from sweat, salt or ordinary glass is the worst enemy of MOS transistors: a fingerprint on a gate oxide ruins it. Use quartz vessels where you can, and gloves always.

Step by step

1. Make the masks

Making a mask by shrinking a drawing twice Artwork drawn 200× full size, black ink or cut film; + = alignment cross Camera 1 shrinks 20× onto a glass plate Camera 2 shrinks 10× more; plate moved one step between shots Mask full size; many chips on one glass plate One mask for each layer of the chip. The crosses on every mask must land exactly on top of each other.
Fig. 3 Masks are made by drawing each layer large and photographing it smaller, twice. The second camera steps the plate between shots to put many copies of the chip on one mask.
  1. Design the chip on squared paper. Use generous rules for your first chips: no line or gap narrower than 25 μm, and every layer overlapping the one it must touch by at least 10 μm, because your masks will never line up perfectly.
  2. Draw each layer 200 times full size on a white board, in solid black (cut paper, black ink, or red film which looks black to photographic plates). A 25 μm line becomes 5 mm — easy to draw accurately. Put the same alignment crosses in the same corners of every layer.
  3. Photograph each drawing with the first camera onto a glass plate, reducing 20 times. Light the board evenly from both sides.
  4. Reduce again 10 times with the second camera, using a short, sharp lens (a The Microscope objective works). Move the plate sideways one chip-width between exposures with a screw-driven slide, so that the final plate carries a grid of many identical chips.
  5. Contact-print working copies from this master; masks scratch and get dirty quickly in use.

2. Prepare the wafers

  1. Slice the crystal with a thin steel wire or blade fed with abrasive slurry. Lap each slice flat on a glass plate with progressively finer abrasive (Abrasives and Grinding Stones) and polish it to a perfect mirror on cloth with the finest powder you can make.
  2. Clean it: boil in a mix of Sulfuric Acid and an oxidiser, rinse in pure water, dip for a few seconds in dilute hydrofluoric acid to strip any oxide, rinse again. Test: bare clean silicon sheds water completely, like a waxed leaf; silicon with oxide or a film on it stays wet.

3. Grow the thick oxide

Slide the wafers, standing on edge in a quartz rack, into the furnace at 1,100 °C with steam flowing. About half a micrometre grows in roughly an hour.

Judge the thickness by colour. Thin oxide on silicon shows bright interference colours, like oil on water. In daylight, looking straight down: about 0.05 μm looks tan, 0.1 μm violet, 0.12–0.15 μm blue, 0.2 μm pale gold, 0.25 μm orange, 0.3 μm blue again. The colours repeat about every 0.2 μm, so to count the cycles, etch a sloping edge on a test piece (lower it slowly into hydrofluoric acid) and count the bands up from bare grey silicon.

4. The lithography cycle (for each mask)

  1. Coat with resist. Put a few drops in the middle of the wafer on a turntable and spin it fast (a few thousand turns a minute) for 30 seconds, to leave a thin, even film. Dry gently at about 90 °C.
  2. Align and expose: lay the mask on the wafer, slide it with fine screws under a microscope until the crosses match the marks from the previous layer, clamp, and expose to ultraviolet. Find the exposure by test strips: seconds to minutes for dichromated gelatin in strong sun, hours for bitumen.
  3. Develop: warm water (about 40 °C) for gelatin; turpentine and oil of lavender for bitumen. The unhardened resist washes away. Hard-bake at 120–150 °C for half an hour.
  4. Etch the oxide in buffered hydrofluoric acid. When the windows turn from coloured to bare grey and shed water, it is done — typically a few minutes for half a micrometre. Rinse at once.
  5. Strip the resist in hot sulfuric acid with an oxidiser, rinse, and inspect every wafer under the microscope.

5. Make the transistors (four masks)

Mask Step Conditions (starting points)
1 — source and drain Open windows; deposit boron from a boric-acid source upstream in the furnace, then drive it in About 1,000 °C for 20–30 minutes, then 1,100 °C for an hour in oxygen; oxide regrows over the windows
2 — gate Open the gate area down to bare silicon; grow the thin gate oxide in dry, very clean oxygen 1,100 °C, 1–2 hours, for about 0.1 μm (violet to blue)
3 — contacts Open small holes through the oxide to the source and drain islands
4 — metal Evaporate 1 μm of aluminium over the whole wafer in vacuum; pattern it and etch in warm phosphoric acid Then heat to about 450 °C for 15–30 minutes in nitrogen, so the aluminium bonds to the silicon

Treat these numbers as places to begin. Every furnace is different: run test wafers, cut them, stain them and measure, and write everything in the log.

6. Test, cut and mount

  1. Probe each chip on the wafer under the microscope with fine needles. First the diodes (each p island to the wafer: one-way), then single transistors (lamp or galvanometer in the drain circuit, voltage on the gate), then gates.
  2. Mark the bad ones with a dot of ink. Expect many: in the 1960s, factories were happy if a few chips in ten worked.
  3. Scribe between chips with a diamond point and snap them apart. Glue good chips to a small base, and connect their large pads (make them at least 0.1 mm square) to the pins with very fine gold wire, pressed on hot, or with silver paint. Seal against air and moisture.

What to make first

  1. A test chip of diodes, resistors (long, thin p-type strips) and single transistors of several sizes. This tells you whether your process works.
  2. An inverter, then NAND and NOR gates.
  3. A ring oscillator: an odd number of inverters joined in a loop. It cannot settle and must oscillate, so if it does, every gate in it works.
  4. A flip-flop (one bit of memory), then a 4-bit adder — about a hundred transistors.

For a sense of scale: the first microprocessor, the Intel 4004 of 1971, had about 2,300 transistors with lines 10 μm wide.

How to tell it worked

  • Oxide has an even colour across the wafer, with no spots.
  • Windows are sharp-edged under the microscope and shed water when etched through.
  • Diodes block one way. Transistors switch: with the gate at the source voltage the drain current is tiny; with the gate at −10 V it is large.
  • Gates give the right truth table, and a ring oscillator oscillates. Watch it on an oscilloscope (Electronic Test Equipment), or put a chain of on-chip flip-flops after it to divide its speed down until a lamp blinks.

Note Troubleshooting. Resist lifts off during etching → wafer not clean or not dry; hard-bake longer; make the resist slightly thicker. Windows ragged or with "mouse bites" → dust on the mask or wafer; clean the room and the masks. Every transistor is on even with no gate voltage, or drifts → sodium in the gate oxide. Clean everything again, use quartz, wear gloves, never let tap water near the wafers. Shorts between source and drain → pinholes in the oxide or the gate overlapping badly; check mask alignment. Aluminium contacts don't conduct → oxide left in the contact holes; etch a little longer, or anneal the metal. Results change from batch to batch → furnace temperature drift. Measure it every run and keep the log.

Dangers

Danger Hydrofluoric acid is the deadliest chemical in this chapter. It feels like water, often causes no pain for hours, and passes through skin to destroy flesh and bone and to poison the heart. A splash of strong acid over an area the size of a hand can kill. Use it only in plastic or wax vessels, with heavy rubber gloves over cotton gloves, an apron and a face shield. Have calcium gluconate gel within reach and running water before the bottle is opened. Any contact: wash under running water for about 5 minutes, then rub in the gel at once and keep rubbing for at least 15 minutes, and treat it as an emergency (Emergencies). Chalk paste is useless because chalk does not dissolve; the full first aid is in Fluorspar and Fluorine Compounds.

Danger Dichromates cause skin ulcers and cancer and are poisonous to drink. Weigh them with care, wear gloves, and never pour them into streams.

  • Hot acids (sulfuric acid with an oxidiser) can boil over and splatter; add solids slowly, wear a face shield.
  • Solvents (turpentine, alcohol) are flammable near furnaces; keep them in a separate room.
  • Hydrogen, if used in annealing, explodes in air: see Semiconductors and the Transistor.
  • Vacuum chambers of glass can implode; put a wire mesh cage around them.
  • Furnaces at 1,100 °C run for days. Guard against burns and fire.

Going further

  • Smaller lines: better lenses and projection printing instead of contact printing; the full workshop-to-factory road is in Making Microchips. Each halving of line width gives four times as many transistors on a chip.
  • Silicon gates (polysilicon instead of aluminium) align themselves automatically and allowed the first microprocessors.
  • Bipolar chips, made with more masks and a layer of crystal grown on the wafer, are faster.
  • Memory chips, processors (Microprocessors and Personal Computers), and finally the whole The Computer on one chip (Microcontrollers); with Programming they become the general-purpose machines of the modern world. Chips also make Solar Cells cheaper and Networks and the Internet possible.

How it was first done

The British radar engineer Geoffrey Dummer described the idea of a circuit made in one solid block in 1952, but could not make it work. In 1955 Jules Andrus and Walter Bond at Bell Laboratories adapted the photoengraver's photoresist to semiconductors, and in 1957 Carl Frosch and Lincoln Derick, also at Bell Labs, showed that a grown oxide masks silicon from dopants.

In September 1958 Jack Kilby at Texas Instruments demonstrated the first integrated circuit: a sliver of germanium holding a transistor, resistors and a capacitor, joined by tiny gold wires bonded by hand. In early 1959, at Fairchild Semiconductor in California, Jean Hoerni developed the planar process, and Robert Noyce saw that a layer of aluminium printed on top of the oxide could connect everything without loose wires; Fairchild's team made the first working planar chips in 1960, and sold them from 1961. Mohamed Atalla and Dawon Kahng made the first MOS transistor at Bell Labs in 1959–60.

The Apollo Guidance Computer, flown to the Moon in 1969, was built from a few thousand identical chips each holding one or two simple gates. In 1965 Gordon Moore noticed that the number of transistors on a chip was doubling every year or two, and it went on doing so for half a century — from a handful to tens of billions.

Source: content/entries/electronics/integrated-circuits.md