The jars and bottles on a bathroom shelf, made from chalk, soap, plant oils, beeswax, glycerine and distilled spirit — toothpaste, shampoo, deodorant, essential oils and perfume, hand cream, lip balm, face powder and hair oil — and the old poisons (lead, mercury, arsenic) that must never go back into them.

Difficulty
●●●●●
Time
An hour for most recipes; a day to steam-distil a batch of oil; three to six weeks to age a perfume
Steps from zero
11 prerequisites →

You need first

SoapDistillationOils and Pressing

This unlocks

—
The full path from nothing — 11 steps before this one
  1. Fire
  2. Stone Tools
  3. Finding and Preparing Clay
  4. Simple Machines
  5. Pottery
  6. Farming from Seed
  7. Oils and Pressing
  8. Lye and Potash
  9. Fermentation
  10. Soap
  11. Distillation
  12. Toothpaste, Shampoo, Perfume and Cosmetics

Do them roughly in this order. See it on the tech tree →

Why it matters

None of these things keeps you alive, but they keep people comfortable, healthy and willing to be close to one another. Toothpaste slows decay and gum disease (Dentistry). Hand cream heals the cracked skin of people who scrub, dig and do laundry all day — cracks that let in infection. Lip balm stops lips splitting in wind and frost. And in every society people have spent scarce money on scent and a clean face, so a settlement that can make them has something to trade.

Every product here is a mixture of things this book already teaches: chalk (Pencils and Chalk), soap and glycerine (Soap), plant oils and fats (Oils and Pressing), beeswax (Beekeeping), and spirit and fragrant oils from the still (Distillation). This chapter is about the mixing: proportions, order of work, and how to tell a good batch from a bad one. Daily washing, chew sticks, toothbrushes and plain tooth powder are in Personal Hygiene; razors and shaving soap are in Razors, Nail Clippers and Grooming Tools.

How it works

Most of these products are one of four kinds:

  • Powders polish, soak up oil and sweat, or hide colour. Everything depends on fineness: a gritty powder scratches enamel and looks patchy on skin.
  • Solutions — shampoo, perfume, deodorant rinses. Alcohol dissolves oils that water will not, so perfume is oil in spirit.
  • Ointments and balms — oil thickened with wax, with no water: lip balm, pomade. Nothing grows in them, so they keep for months.
  • Emulsions — creams and lotions: tiny droplets of oil held apart in water by an emulsifier, a substance one end of which likes oil and the other water. Soap is one; so is the soap that forms when a pinch of borax meets the natural acids in beeswax. Because they contain water, mould grows in them, so they must be made clean and used quickly.

A single rule runs through all of them: put nothing on the body that you would not be willing to swallow a little of — because lips, gums and broken skin absorb what you put on them.

What you need

Item Use Where it comes from
Water bath — a pot standing in a larger pot of simmering water Melting wax and fat without scorching Pottery, Pots, Pans and Kettles
Glazed or glass jars, small tins Containers Pottery, Laboratory Glassware, Tins, Cans, Drums and Tanks
Silk sieve, mortar and pestle Powders Silk, Pigments, Paints and Varnish
Balance weighing to 1 g; a whisk Recipes, creams Measurement from Scratch, Kitchen Utensils and Gadgets
Strong spirit, 85–95 % alcohol Perfume, deodorant Distillation

Glycerine is the sweet, syrupy liquid left in the brine when soap is salted out (Soap). Boil the spent brine down, skim off the salt as it crystallises, and keep boiling until the brown syrup is thick. It holds water in skin and keeps pastes moist.

Where to find it

  • Chalk and whiting: soft white rock that fizzes with vinegar (Lime). For a gentle tooth polish, prepare it by washing: stir ground chalk into ten times its volume of water, wait one minute for the grit to sink, and pour the milky water into a second pot. Let that settle overnight, pour off the clear water and dry the white mud. This prepared chalk is far finer than anything a mortar can make.
  • Kaolin (Stoneware and Porcelain) and talc — ground soapstone (Rocks and Minerals) — washed the same way make soft powder bases. Use only white talc with no fibres in it (see Dangers).
  • Starch: grate potatoes into water, strain, let the starch settle, wash and dry it.
  • Soapnuts (Sapindus), sticky brown tree fruits of India, China and the Americas, and the roots of soapwort, a pink-flowered weed of damp verges, foam in water: they contain natural soaps (saponins).
  • Lanolin (wool grease): the yellow grease in raw fleece (Wool). Scour fleece in soapy water at about 60 °C, let it cool, and skim the grease that floats; remelt it in clean hot water until pale. It soaks up twice its weight in water.
  • Alum: crystals made from alum stone, alum shale or clay (Alum and Alumina).
  • Fragrant plants: see Distillation. A crushed leaf whose scent lasts on the fingers is rich in oil.

Toothpaste

What it is

A paste for cleaning teeth with a brush. It does three jobs: a mild abrasive scrubs off the sticky film of bacteria (plaque) and stains; a foaming agent loosens food and carries it away; flavour makes people use it. Modern toothpaste also carries fluoride, which hardens enamel against decay — and that is the one part you probably cannot make safely (below).

Making it

Start with tooth powder: prepared chalk 10 parts, salt 1 part, with a pinch of dried, powdered mint (Personal Hygiene). Toothpaste is the same powder held in a paste:

Ingredient Weight Job
Prepared chalk 50 g Abrasive
Glycerine 25 g Keeps it moist and smooth
Boiled water 15–20 g Makes it a paste
Gum arabic or fine starch 1–2 g Binder; stops the liquid separating
Soap, finely shaved 2–3 g Foam
Peppermint, clove or wintergreen oil 5–10 drops Flavour
  1. Dissolve the gum (or cook the starch into a clear jelly) in the hot water. Stir in the glycerine and the shaved soap until smooth.
  2. Work the chalk in a spoonful at a time, like making dough, until the paste is as stiff as soft butter.
  3. Stir in the oil last, and store in a lidded glazed jar or a squeeze tube. Without glycerine (water and honey instead), make only a week's worth; it dries and ferments.

A collapsible tube of soft tin keeps it cleaner and moister than a jar (Tin and Pewter). Never use lead for tubes.

How to tell a good one

  • No grit. Rub a pea of paste between thumb and finger beside your ear; you should hear and feel nothing. Rub it on window glass for a minute with a wet fingertip: a good paste leaves no scratches visible against the light. One that scratches glass wears enamel.
  • It stays soft in the jar for a month and does not separate into liquid and a hard cake.
  • It tastes clean and slightly salty, not soapy-bitter. Too much soap is the commonest fault.

Warning Leave fluoride out. Making it means handling hydrogen fluoride, one of the most dangerous chemicals there is, and too much swallowed by children mottles their teeth. Instead, brush twice a day and eat sweet things only at meals. Never put charcoal, brick dust, pumice or sand in tooth powder: they are too hard.

Shampoo

What it is

A soap thin enough to spread through hair and rinse out completely. Plain soap works, but in hard water (Water Treatment for a Town) it reacts with lime in the water to form grey, sticky lime soap that dulls hair. Two cures: a soap made soft and liquid, and an acid rinse afterwards.

Making it

  • Soap shampoo. Dissolve 50 g of shaved hard soap (or 100 g of soft potash soap, Soap) in 1 litre of hot rainwater, with 15 g of glycerine and 10–20 drops of rosemary or lavender oil. It sets to a soft jelly; shake before use. Plant-oil soap is gentler than tallow soap.
  • Acid rinse. After washing, pour over the hair 1–2 tablespoons of vinegar (Vinegar and Pickling) or the juice of half a lemon in a litre of water. The acid dissolves lime soap and smooths the hair. Rinse with clean water.
  • Soapnut or soapwort shampoo. Simmer 8–10 soapnuts (shells only, seeds removed) or a handful of crushed soapwort root in 1 litre of water for 20 minutes, strain and cool. It is gentle, needs no acid rinse, and keeps three or four days.
  • Dry shampoo. For the sick in bed or for winter: rub a handful of starch or kaolin into the roots, wait five minutes while it soaks up the grease, and brush it out thoroughly.

How to tell a good one

Hair should squeak slightly when wet and dry soft, without a grey film. Test a new batch of soap shampoo with litmus (Acids, Bases and Testing): it should turn red litmus faintly blue, no more. A strong blue means free lye — it will burn the scalp. Re-make the soap with more fat.

Deodorant

What it is

Fresh sweat barely smells; bacteria breaking it down make the smell. A deodorant slows those bacteria; an antiperspirant also plugs the sweat ducts with aluminium salts.

Making it

The most important deodorant is daily washing with soap. Beyond that:

  • Alum stone. A large, clear crystal of potash alum (Alum and Alumina). Grow one egg-sized by hanging a seed crystal on a thread in saturated alum solution for two or three weeks. Wet it and rub it over clean armpits; one crystal lasts a year.
  • Deodorant powder. 1 part baking soda (Soda Ash and Baking Soda) to 3 parts starch or kaolin, sifted together. Pat on clean, dry skin. More soda than this can redden the skin.
  • Spirit rinse. 70 % alcohol with 1 % lavender or thyme oil, dabbed on with cloth. It kills bacteria for some hours and smells clean.
  • Antiperspirant. About 15 % aluminium chloride in water, put on at night. It is made by dissolving Aluminium in Hydrochloric Acid, so it belongs to a later stage.

A good deodorant stops the smell for a full working day and does not redden or itch the skin.

Essential oils

Essential oils are the fragrant, volatile oils of plants. The basic steam method and the yields of each plant are in Distillation. Here are the improvements that make it a real trade.

The separate-boiler still and the oil separator

A plant sitting over boiling water scorches and stews. Better: raise steam in one vessel and lead it through the plant in another.

Boiler half full of water Fire Safety vent loose weighted lid Plant vessel plant packed loosely on a perforated grid Steam enters below grid Steam + oil vapour Condenser copper worm in cold water Oil separator (Florentine flask) Oil floats water out
Fig. 1 A steam still for essential oils. Steam from a separate boiler rises through a column of plant packed on a grid, carries the oil vapour into the condenser, and drips into an oil separator. Water leaves through the side arm that rises from the bottom; the oil stays floating on top.
  1. Boiler: a lidded pot or sealed copper kettle, half full, with a pipe from the lid. Fit a simple safety vent — a loose weighted lid or a cork stopper — so it can never build pressure.
  2. Plant vessel: a tall pot or barrel-shaped copper can, 40–60 cm high, with a perforated grid 5 cm above the bottom. The steam pipe enters below the grid. Pack the plant loosely and evenly; channels let steam slip past without picking up oil.
  3. Condenser: a copper coil (worm) in a tub of cold water (Distillation). The outflow should be cool to the hand; warm outflow loses oil as vapour.
  4. Oil separator (the "Florentine flask"): a tall, narrow bottle with a side arm that leaves near the bottom and rises to just below the neck before turning down. Oil floats and gathers in the neck; the heavier water flows out at the bottom, up the side arm and over the bend, so the level never rises. For oils heavier than water — clove, cinnamon, wintergreen — the oil sinks; draw it off through a tap at the bottom instead.
  5. Run until the drips at the separator carry no more film of oil, usually 1–3 hours for leaves, longer for woods and seeds. Grind roots, seeds and wood coarsely first.

Return the scented water to the boiler for the next charge, or keep it as rose water or lavender water.

Expression: citrus oil

Citrus oils, in tiny bags in the coloured peel, are spoiled by heat. Fold strips of fresh peel and squeeze them against a sponge over a bowl; let the liquid stand a day and the oil rises. A hundred oranges give roughly 50–100 ml of oil.

Enfleurage: scent from delicate flowers

Jasmine, tuberose and violet give almost no oil in a still. Catch their scent in fat instead: spread odourless lard 3 mm thick on glass plates in wooden frames, press fresh flowers into it, stack the frames, and replace the flowers every day for 3–8 weeks. Stir the scented fat with strong spirit for a day, chill, and pour off the spirit, which now carries the scent. For roses and orange flowers, warm maceration is quicker: steep flowers in fat at 60–70 °C for two hours, strain, and repeat with fresh flowers ten to twenty times.

Storing and judging oil

Store essential oils in full, small, dark-glass bottles with tight stoppers in a cool place. Citrus oils last about a year, most others two or three. Test a drop on a strip of filter paper: a good oil evaporates leaving no greasy ring (a ring means it has been thinned with plant oil) and smells true and fresh at every stage. A sharp, turpentine-like or stale smell means it has oxidised.

Perfume

What it is

Perfume is fragrant oils dissolved in strong alcohol, which carries the scent off the skin and evaporates. Strength is set by how much oil is in it:

Kind Oil in spirit Lasts on skin
Perfume (extract) 15–30 % 6–8 hours
Eau de toilette 5–15 % 3–4 hours
Eau de cologne, toilet water 2–5 % 1–2 hours

Top notes fade within half an hour (citrus, lavender, mint); heart notes last hours (rose, neroli, rosemary); base notes last a day (resins such as benzoin and myrrh, sandalwood, vanilla, aged iris root) and act as fixatives that slow the rest.

A classic cologne

To 1 litre of 90 % spirit add:

Oil Amount
Bergamot or lemon 15 ml
Sweet orange 5 ml
Lavender 3 ml
Rosemary 2 ml
Neroli or petitgrain (orange flower or leaf) 2 ml
A pinch of benzoin resin, dissolved Optional fixative

That is about 2.7 % oil — a true eau de cologne. A simpler Hungary water is just rosemary in spirit: steep 100 g of fresh rosemary tops in a litre for two weeks, or add 10 ml of rosemary oil.

  1. Mix the oils, pour them into the spirit and shake.
  2. Age it stoppered in the dark for 3–6 weeks; the raw edge of the alcohol softens.
  3. Chill it for a day so waxes drop out as a haze, and filter through paper while cold.

Test a perfume on a paper strip and on the inside of the wrist: smell at 1 minute, 1 hour and 6 hours. A good one fades smoothly and never smells of raw spirit or anything sour.

Danger Use only clean ethyl alcohol — the "hearts" of a careful second distillation (Distillation). Never use the first runnings (heads) or wood spirit: they contain methanol, which blinds and kills when someone drinks it. Label perfume and keep it out of reach. Undiluted essential oils burn skin and eyes; a teaspoon of some (wintergreen, eucalyptus, camphor, pennyroyal) can kill a small child.

Hand cream and cold cream

What it is

A cream puts back the oil washing strips from skin; its water evaporates with a cooling feel, hence "cold cream". Unlike plain grease, it rubs in.

Making it

The simplest — glycerine and rose water. 1 part glycerine to 3 parts rose water, rubbed into hands after washing.

Cold cream with borax — the standard recipe for more than a century:

Oil phase Water phase
Beeswax 15 g Boiled water or rose water 35 g
Plant oil (almond, olive, sunflower) 50 g Borax 1 g
1 Heat both to 70 °C 2 Pour slowly 3 Whisk till cool 4 Scent and pot Oil + beeswax 50 g oil, 15 g wax Water + borax 35 g water, 1 g borax each pot stands in a larger pot of simmering water thin stream of hot water into the oil, whisking hard turns milky white; beat 10–15 min until cool or it separates Scent drops below 40 °C small scalded jars; use within 2–4 weeks
Fig. 2 Making cold cream. Melt the wax in the oil, and dissolve the borax in the water, both at about 70 °C in water baths; pour the hot water slowly into the oil while whisking; keep whisking until the cream is cool and white; then add scent and pot it.
  1. In one water bath, melt the beeswax into the oil. In another, dissolve the borax (Borax and Boric Acid) in the water. Bring both to about 70 °C — too hot to keep a finger in for more than a second.
  2. Pour the hot water slowly, in a thin stream, into the oil while beating hard with a whisk. The borax and the acids in beeswax form a soap that holds the mixture together; it turns milky white at once.
  3. Take it off the heat and keep beating until it is cool, 10–15 minutes. If you stop while it is warm, it separates.
  4. Stir in a few drops of rose or lavender oil below 40 °C, and fill small clean jars.

For a richer barrier cream for laundry and dirty work, replace 15 g of the oil with lanolin.

Without borax, Galen's ancient recipe works with more effort: 1 part beeswax, 4 parts oil, 2 parts rose water, beaten in a warm mortar for a long time.

How to tell a good one

Smooth and white, with no beads of water or oil after a week. It rubs in within a minute without greasiness. Any spot of mould, sour smell or pink, green or black speck: throw the jar away. Make small batches with boiled water and scalded jars, and take cream out with a clean spoon.

Lip balm and hair oil

Lip balm

Lip balm is a water-free ointment that seals the lips against wind and cold. Melt in a water bath 1 part beeswax with 2–3 parts plant oil by weight — more wax for a firm stick for hot weather, more oil for a soft pot balm for cold. Test a drop on a cold plate: firm, but melting under a rubbing fingertip.

60 mm 15 mm Cap push-fit tin or turned wood Balm stick 1 part beeswax : 2 parts oil Tube rolled tin, or a hollowed elder stem Sliding piston a cork or wooden disc on a rod Push from below Or a small tin softer: 1 wax : 3 oil Test first: a drop on a cold plate must set firm but melt under a rubbing fingertip.
Fig. 3 A push-up lip balm stick. Balm is poured into a thin tin or wooden tube closed by a sliding piston; pushing the stick up from below feeds out the balm. A simple pot or folded tin with a lid does just as well.

Pour into small tins or a tube about 15 mm across and 60 mm long — a rolled tin tube or a drilled elder stem with a sliding plug pushed up from below. For colour, warm the oil with dried alkanet root or beetroot powder before adding the wax, and strain. Never colour lips with vermilion (mercury) or red lead — both were once used and both poison.

Hair oil and pomade

Hair oil stops dry hair breaking and gives it a shine. Coconut, olive, castor or almond oil, with 20 drops of rosemary or lavender oil per 100 ml, or with dried herbs steeped in it (Medicinal Plants). Work a few drops through the ends. Rancid oil smells like old paint or stale nuts: throw it out.

Pomade, which holds hair in place, is 1 part beeswax to 3–4 parts oil, or scented lard. It washes out only with soap.

Face powder and colour

Face powder takes the shine off skin and evens its colour. A good base:

Ingredient Parts
Talc (washed, ground soapstone) 60
Kaolin 15
Zinc oxide (Zinc and Brass) 15
Starch 10

Tint it to skin colour with tiny amounts of yellow and red ochre (Pigments, Paints and Varnish) — start with 1 part in 200 and add more slowly. Grind everything together for half an hour and sift three times through silk. Test on the back of the hand: a good powder feels silky, shows no specks, and does not look chalky in daylight.

Rouge for cheeks is the same base with more red ochre, or the red of safflower petals. Eyeliner (kohl) is fine lampblack or soot from an oil lamp (Lamps and Candles) worked into a little oil or fat. Never share kohl sticks: they spread eye infections.

Dangers

Danger Never use lead, mercury, arsenic or antimony on the body. People did, for thousands of years, and they died of it.

  • White lead (ceruse), the white face paint of Rome, China, Japan and Tudor England, and kohl ground from galena cause lead poisoning: grey skin, colic, wrist drop, madness, and damage to children's brains.
  • Mercury — vermilion lipstick and "skin-whitening" creams — damages kidneys and nerves.
  • Arsenic complexion wafers, lead acetate hair dyes and belladonna eye drops are poisons too.

Use only the white bases in this chapter (chalk, kaolin, talc, starch, zinc oxide), iron-oxide ochres and plant colours. See Lead, Mercury and Arsenic for the signs of poisoning.

  • Talc and asbestos. Some soapstone carries asbestos — silky, flexible fibres visible with a lens (The Microscope). Reject any talc with fibres, and never powder babies, who inhale it.
  • Allergy. Test any new product on the inside of the forearm and wait a day.
  • Fire. Warm spirit and oils in a water bath, never over a naked flame.
  • Borax is poisonous if swallowed; never use boric products on babies.

How to tell it worked

Each section above gives its tests: powders pass the glass-scratch test, creams stay mixed and clean for a week, perfumes stay clear and sweet at 6 hours, shampoos leave no film.

Note Troubleshooting.

  • Cream separates into oil and water → water poured too fast, phases at different temperatures, or beating stopped while warm. Reheat both to 70 °C and start again, pouring slowly.
  • Cream grows mould in days → water not boiled, jar not scalded, or fingers in the jar.
  • Perfume cloudy → water added too fast, or waxes from the oils; chill and filter.
  • No oil in the separator → condenser too warm, plant packed too tight, or plant old and dry.
  • Lip balm grainy → cooled too slowly; remelt and pour quickly into cold tins.

What this unlocks

The same skills make ointments and liniments, and the same still makes flavourings for sweets. Tubes and jars lead to Sacks, Boxes, Crates and Packaging. Clean small-batch work — boiled water, scalded jars, labels and dates — is the habit of a real Pharmacy: Tablets, Capsules, Ointments and Inhalers.

How it was first done

Egyptian tombs hold kohl pots and perfume jars from before 3000 BC, and a 4th-century AD Egyptian papyrus gives a tooth powder of salt, mint, iris and pepper. The Greek physician Galen, about AD 150, wrote the recipe for cold cream of wax, oil and rose water. Ibn Sina (Avicenna), about 1000, distilled rose water on a large scale, and Giovanni Maria Farina created Eau de Cologne in Cologne in 1709; enfleurage was perfected in Grasse, France, in the 1700s and 1800s. The word shampoo comes from the Hindi chāmpo, "press, knead", brought to Brighton by Sake Dean Mahomed in 1814. Colgate sold toothpaste in jars from 1873, and the dentist Washington Sheffield put it in collapsible tubes in the 1890s. The first trademarked deodorant, Mum, appeared in Philadelphia in 1888. Lead face paint was known to kill by the 1700s, but laws keeping lead, mercury and arsenic out of cosmetics came only in the 1900s.