Part 15 · Knowledge and Science
Microfilm and Document Storage
Photograph pages twenty times smaller onto fine-grained silver plates or film, and a whole library fits in a drawer. Processed and stored properly, silver images last for centuries and can be read with nothing more than a lens and a light. How to make the camera, the plates and the reader, process for permanence, and build the boxes and stores that keep records safe.
- Difficulty
- ●●●●●
- Time
- A week to build a camera and reader; a day to film and process a book once everything works; storage is for centuries
- Steps from zero
- 21 prerequisites →
This unlocks
—The full path from nothing — 21 steps before this one
- Fire
- Cordage and Rope
- Stone Tools
- Finding and Preparing Clay
- Finding and Identifying Ores
- Hunting and Trapping
- Basic Woodworking
- The Kiln
- Pottery
- Charcoal
- Hides and Leather
- Lime
- Lye and Potash
- Glass
- Bellows
- Copper Smelting
- Lead
- Laboratory Glassware
- Lenses
- Gold and Silver
- Photography
- Microfilm and Document Storage
Do them roughly in this order. See it on the tech tree →
Why it matters
A book of 300 pages fills about 2 litres. Photographed 20 times smaller, the same book fits on about ten glass plates the size of a postcard, or 3 metres of 35 mm film — on film, about a hundredth of the space, and a fraction of the weight to carry to a safe place.
Size is only half of it. Silver in gelatin, properly fixed, washed and toned, is one of the most stable records humans have made: old glass plates from the 1850s still print perfectly, and modern silver microfilm on a stable base is expected to last about 500 years. Unlike any electronic record, it needs no machine to read — a hand lens and daylight will do. And it copies cheaply: one master can be contact-printed onto fresh film in minutes, so copies of a whole library can be sent to every town.
This chapter adds to the methods in Libraries and Preserving Knowledge (many copies in many places, recopied on schedule) and builds on the cameras and plates of Photography and the copy camera of Copying Documents and Xerography.
How it works
Three numbers decide everything.
- Reduction. How many times smaller the image is than the page. Pages are filmed at 10× to 25×; 20× is a good default. A page 30 cm tall becomes 15 mm.
- Resolution. How fine a detail the lens and the emulsion can record, measured in line pairs per millimetre (one black and one white line). To read small print (letters 2 mm tall, strokes about 0.25 mm) at 20×, a stroke becomes 12 µm wide: the system must resolve at least 80–100 line pairs per mm. A good camera negative resolves 30–60; microfilm needs better than twice that.
- Contrast. Text is black and white. A high-contrast emulsion and developer turn faint grey strokes into crisp black ones.
Fine detail needs fine grain, and fine grain means slow emulsion — the large crystals that make a plate fast also make it coarse. Microfilm is therefore exposed for seconds or minutes on a still copy board under steady light.
The film in the camera is a negative (clear letters on a dark ground). It is the master and should be read as little as possible. Readers use contact copies printed from it.
| Format | Reduction | Image size | Holds |
|---|---|---|---|
| Glass micro-plate, 9 × 12 cm | 15–20× | 15 × 20 mm frames | 25–40 book pages |
| Microfiche (sheet film) 105 × 148 mm | 24× | Grid of frames | 98 pages |
| 16 mm roll, 30 m | 24× | ~10 × 14 mm | ~2,400 letter-size pages |
| 35 mm roll, 30 m | 14–20× | up to 32 × 45 mm | ~600 frames: newspapers, maps, 2 book pages each |
What you need
| Item | Notes |
|---|---|
| Copy stand | Rigid column, copy board, two lamps; see below |
| Lens | Short focus, 3–6 cm, the best you have: a The Microscope objective or a small achromatic lens (Optical Glass and Achromatic Lenses) |
| Fine-grain plates or film | Unripened gelatin emulsion (Photography); film needs a clear base |
| Developer, fixer, sodium sulfite | As for plates (Photography); fixer is hypo |
| Liver of sulfur | Potash fused with sulfur, for toning (below) |
| Focusing magnifier, 10× | Any good magnifying glass |
| Darkroom, safelight, trays | As for Photography, The Darkroom and the Enlarger |
| Reader | Lens, lamp, condenser, screen (below) |
| Rag board, starch paste, linen thread | For archive boxes (Paper) |
The microfilm camera
A microfilm camera is a copy camera built for much greater reduction and much greater rigidity. The planetary kind, where the page lies flat and the camera looks down on it, is the easiest to build and the gentlest on books.
- Column and base. A heavy base board of hardwood or stone, at least 60 × 50 cm, and an upright of thick timber or iron pipe about 1.2 m tall, braced so that a tap with a finger does not shake it. Vibration is the enemy: at 20×, the camera moving 0.01 mm ruins the frame. Stand it on a solid floor or a stone slab, never a wooden upper floor.
- Copy board and book cradle. A matt black board on the base. For bound books, two hinged half-boards that tilt so the book opens to about 120° without cracking its spine, each on springs or wedges so both pages rise to the same height. A sheet of clean glass presses the pages flat. Mark the frame area in white at the board's edges.
- Lamps. Two equal lamps at 45°, one each side, about 60 cm from the page. Check the light is even by laying a white card on the board and looking at it through a tube: no bright spot or dark corner. Steady electric light (The Light Bulb) is best because exposures repeat; daylight changes minute by minute.
- Distances. For reduction m and lens focal length f, the page is f × (m + 1) from the lens and the plate f × (1 + 1/m) behind it. With f = 5 cm at 20×: page 105 cm away, plate 5.25 cm behind the lens. The plate distance is tiny and must be adjusted to a hundredth of a millimetre, so fit the lens in a fine screw — a tube threaded 0.5–1 mm per turn (Screws, Nuts and Bolts), with a pointer and scale round it.
- Stop. Set the lens to about f/8. Wider, its faults blur the frame; much narrower, light spreading round the hole (diffraction) blurs it instead.
- Plate holder, step and repeat. A plate slides in a frame with notches cut every frame-width (for 15 × 20 mm frames, 17 mm across and 22 mm down) so it clicks into each position. A shutter — a black flap or lens cap worked by a lever — opens for each exposure. A plate thus holds a grid of pages, a microfiche on glass.
- Roll film (when you have film): replace the plate holder with two spools and a sprocket turned by a crank that moves the film exactly one frame per turn. A pressure plate holds the film flat in the gate during exposure; a counter (Clockwork, Music Boxes and Counting Machines) records the frame number.
Focusing
Ground glass is far too coarse to see a 12 µm stroke. Instead:
- Put a piece of clear glass in the plate position, with a fine cross scratched on its inner face exactly where the emulsion will be.
- Look at the cross through the 10× magnifier and move your eye slightly side to side. Turn the focus screw until the image of the text and the scratched cross do not move relative to each other — then the image lies exactly in the emulsion plane.
- Prove it with a focus test. On one plate, film the same test page (a page of the smallest print you have, plus a chart of fine lines) at ten focus settings, turning the screw a small step each time. Develop and examine under a microscope. Use the sharpest setting and record it.
Fine-grain plates and film
Use the gelatin dry-plate recipe in Photography, with three changes:
- Use silver chloride (common salt instead of bromide) or bromide, and do not ripen: pour the silver in at 35–40 °C, stir 5 minutes, and add the extra gelatin at once. The grains stay tiny and the emulsion slow and contrasty.
- Coat thinly: about 3 ml per 9 × 12 cm plate. Use very flat, bubble-free glass (Window Glass); wavy glass cannot be focused.
- Develop in a contrasty developer, such as the pyrogallol developer with double the soda, for 3–4 minutes.
Exposures run from several seconds to a few minutes under lamps. Find yours with a test plate: the right one gives a dense, dark background through which you can just make out a bright lamp filament, with perfectly clear letters.
Roll film needs a flexible, clear, stable base. Cellulose acetate, made from cotton with acetic anhydride, or polyester (Petrochemicals and Modern Plastics) are the bases used (Photographic Film Base). Both need an established chemical industry. Never use cellulose nitrate film for records: it decays and can catch fire by itself (Early Plastics). Until a safe base exists, glass plates are the archival choice.
Archival processing
Most old photographs that faded did so because of careless processing. For records meant to last centuries:
- Fix completely. Use two fixing baths one after the other, each for the full time. Throw the first away when it has fixed about 20 plates; the second becomes the new first.
- Clear. Rinse, then soak 2 minutes in 2% sodium sulfite (20 g per litre). This loosens the hypo so it washes out much faster.
- Wash. Running water, or 10 changes of water 3 minutes each, for film; glass plates as long again. Water at 18–24 °C.
- Test. Put a drop of 1% silver nitrate on a clear margin. It must stay colourless after 2 minutes. Any yellow or brown means hypo is left: wash again.
- Tone. Silver slowly oxidises, especially near paint, fresh wood or cardboard, forming tiny red or orange spots (redox blemishes). Toning turns the surface of the silver grains into silver sulfide, which does not oxidise. Fuse 2 parts potash with 1 part Sulfur in an iron pot to make liver of sulfur (it smells of rotten eggs), dissolve 1–2 g per litre, and bathe the washed plate for 2–5 minutes, until the image turns very slightly warm in colour. Wash again 10 minutes.
- Dry in still, dust-free air, standing on edge. Never touch the emulsion.
- Inspect every frame with the magnifier. Refilm any page that is blurred, cut off or unreadable before the book goes back on its shelf.
Copies. Lay the master face to face with a fresh unexposed plate under a sheet of glass, expose briefly to a lamp, and develop: a positive copy. Copy that for a negative. Send copies out; keep the master in the best store you have, and never project it.
The microfilm reader
A hand lens. The simplest reader is a 10–20× magnifier and a light box: a white card or opal glass lit from behind. It is slow to read but needs nothing else.
The Stanhope viewer. A glass rod about 3–5 mm across, one end ground and polished to a dome, the other flat. For ordinary glass, a dome of radius R focuses parallel light at a distance of about 3R inside the glass, so make the rod 3R long: for R = 1.5 mm, a rod 4.5 mm long. Cement a tiny positive transparency onto the flat end with a drop of Canada balsam (The Microscope). Held to the eye and pointed at a window, it shows the image enlarged about 100×. It suits single small things — a key page, an index, a map — sealed into a box lid or a pendant.
The projection reader. For daily reading.
- Lamp — an electric bulb of 25–100 W, or a bright oil lamp (Lamps and Candles).
- Heat filter — a flat glass cell of water, 2–3 cm thick, between lamp and film. Without it the frame bakes.
- Condenser — one or two large plano-convex lenses (5–8 cm across) that gather the light into the projection lens.
- Gate — two plates of glass that sandwich the film or plate, sliding on rails so any frame can be centred. Rolls run between two hand-cranked reels.
- Projection lens — focal length 3–6 cm, in a focusing screw.
- Mirror at 45° and a screen of fine ground glass seen from the front, or white card inside a dark hood.
For the page to appear full size, the light path from lens to screen must be about f × (m + 1) — 1.05 m for a 5 cm lens at 20×. Fold it with one or two mirrors to make the box compact, about 50 × 40 × 60 cm. A good reader shows letters at least as sharp as a typed page.
Archive boxes and the store
Silver lasts centuries; the box it sits in often decides whether it does. Acid from poor board, sulfur from rubber and wool, and fumes from fresh paint and oak all attack silver and paper.
The archive box
- Board. Make thick board, 1.5–2 mm, from cotton or linen rag pulp with no wood, by couching several wet sheets together or pasting dry ones (Paper, Wood Pulp, Kraft Paper and Paperboard). Stir 2–3% chalk (by dry weight) into the pulp as an alkaline reserve that neutralises acids for decades. Size with gelatin or starch, never with alum and rosin, which are acid.
- Make it as one folded piece. Draw the box net on the board: base, four sides, and flaps that tuck in at the corners. Score fold lines with a bone folder against a straightedge and fold. Lock the corners with the flaps, or stitch them with linen thread. Where glue is needed, use wheat starch paste, never animal glue (which attracts insects and mould) or rubber cement.
- Lid. A second, slightly larger tray as a lid, or a hinged lid with a fall-down front so files lift out without being dragged.
- Sizes. For documents, about 39 × 27 × 12 cm inside — big enough for folio sheets, small enough to weigh under 10 kg full. For plates, a box just wider than the plate, in which plates stand on edge in folded paper sleeves; plates stacked flat crack under their own weight. For rolls, a small box or tin can per reel.
- Label the box on its end in carbon ink (Ink) with the contents and the date filmed.
Tests. Grind a scrap of board in a spoonful of rain water and add a drop of red cabbage indicator (Acids, Bases and Testing): it must turn blue to green, not pink. Leave a strip half-covered in strong sun for two weeks: the exposed half must not yellow (yellowing means wood lignin). Sniff a closed box after a week: no smell of vinegar, sulfur or paint.
The store
- Cool and steady: ideally below 18 °C and never above about 21 °C; cooler is better. Each 5 °C cooler roughly doubles the life of film and paper.
- Dry and steady: about 30–40% relative humidity (hygrometer). Damp breeds mould and spots; rapid swings crack emulsions. Underground rooms and deep cellars are steady but often damp; test as in Libraries and Preserving Knowledge.
- Dark, clean air: no fresh paint, varnish, new plywood or oak shelving in the room for a year; metal or well-aged softwood shelves. Shelves at least 15 cm off the floor against floods.
- Separate stores for master and copies, kilometres apart. Fire, flood and war take whole buildings.
- Inspect every 2–5 years: open 1 box in 20, check frames for spots, sticky emulsion or vinegar smell, and recopy anything that shows decay.
How to tell it worked
- Read the hardest page. Under the reader, the smallest print and the finest line chart must be readable in the corners of the frame, not only the centre.
- Even density. Every frame on a plate or roll has the same dark background. Light frames mean the lamps or exposure varied.
- Hypo test clean; cabbage test blue-green; no smell in the box.
Note Troubleshooting. Sharp centre, blurred corners → plate not parallel to the copy board; lens faults — stop down one step or use a better lens. All frames slightly blurred → focus off, or vibration. Redo the focus test; stand the camera on stone; wait 10 seconds after touching it before exposing. Letters fill in and blur together → overexposed or overdeveloped; halve the exposure. Thin strokes missing → underexposed, or emulsion too coarse; do not ripen it. Red or orange spots after months → oxidation; tone, and remove the source (cardboard, paint, wood fumes). Film smells of vinegar, curls and shrinks → acetate base decaying. Copy it at once onto fresh material, and keep it away from other film.
Dangers
Danger Nitrate film can burn violently and give off poisonous gas. Never make records on it; if you find old nitrate film (it smells of acid, may be sticky or powdery, and a snip burns fiercely), store it away from people in a cool outbuilding, copy it, and keep it away from heat and flame (Early Plastics).
- Silver nitrate (Silver Nitrate and Silver Salts) stains skin black and blinds if splashed in the eye. Wear eye protection.
- Liver of sulfur gives off hydrogen sulfide when it meets acid (including used fixer). Use it outdoors or in a draught, and never mix it with acid baths.
- Hot lamps in a reader or under a copy board can set paper alight. Keep the water cell filled and leave a gap for air.
- Heavy boxes and glass — keep plate boxes under 10 kg and on low shelves.
What this unlocks
With microfilm, every village library can hold the whole of this book and much more in a drawer, and a master copy can be buried deep for safety. Newspapers, land records, birth registers, Maps and Mapmaking, patents and engineering drawings can be kept without filling buildings. The same fine-grain plates and high-reduction cameras make photomasks for Integrated Circuits, and the reader is a cousin of the slide projector and the The Microscope.
How it was first done
In 1839, the year photography was announced, the Manchester instrument maker John Benjamin Dancer made tiny photographs through a microscope, and in the 1850s he sold microscope slides carrying whole pages that could only be read under the lens. The Frenchman René Dagron patented microfilm in 1859 and sold Stanhope viewers set in jewellery and souvenirs. During the siege of Paris in 1870–71 he filmed government dispatches and private letters onto thin collodion films that carrier pigeons flew into the city; about 115,000 messages arrived this way, read by projection and copied out by clerks. In 1925 the New York banker George McCarthy built a camera to film cheques; Kodak bought it as Recordak in 1928. From the 1930s, libraries filmed newspapers and rare books — Eugene Power's University Microfilms began in 1938 — and in the Second World War millions of soldiers' letters crossed the oceans as "V-mail" on microfilm. Microfiche was standardised in the 1960s, and silver film on polyester remains a long-term record format in archives today.
Source: content/entries/knowledge/microfilm.md