◆ Rebuild

Part 9 · Health and Medicine

Intravenous Fluids

When a person is too dehydrated, shocked or ill to drink, salt water must go straight into a vein — or, as a first and safer step, through a soft tube into the stomach. This chapter covers when that is truly needed, how to make sterile normal saline in sealed glass bottles, how to build a drip set, how to put a needle into a vein, how fast to give it, and the dangers — infection, fever from impure water, air in the line and drowning the lungs with too much fluid.

Difficulty
●●●●●
Time
A day to distil, fill and autoclave a batch of bottles; minutes to set up a drip once practised; weeks of supervised practice before anyone should put needles into the sick
Steps from zero
10 prerequisites →

You need first

Sterilising Instruments and DressingsOral Rehydration

This unlocks

Kidney Dialysis
The full path from nothing — 10 steps before this one
  1. Fire
  2. Finding and Preparing Clay
  3. Sanitation and Germs
  4. Finding and Purifying Water
  5. Pottery
  6. Salt
  7. Fermentation
  8. Distillation
  9. Oral Rehydration
  10. Sterilising Instruments and Dressings
  11. Intravenous Fluids

Do them roughly in this order. See it on the tech tree →

Why it matters

Cholera can drain 10–20 litres of watery stool from an adult in a day. Untreated, it kills half of those it strikes severely, mostly within a day — not from the germ itself but from the loss of water and salt. With fluids and salts replaced fast enough, fewer than one in a hundred die. Most of that replacement is done by mouth with oral rehydration solution (Oral Rehydration). But some people arrive too far gone to drink: collapsed, with no pulse at the wrist, too drowsy to swallow, or vomiting everything. For them, fluid straight into a vein — an intravenous drip — buys the hours that ORS needs to take over.

The same skill and the same bottles of sterile salt water serve for:

Warning A drip is a serious medical procedure. Every step below can kill if done carelessly: an unsterile bottle, water with the wrong saltiness, a bottle allowed to run dry, or too much fluid too fast. Learn it under someone who has done it, practise on each other's veins with sterile saline in calm conditions, and keep careful records. If there is any skilled health worker within reach, get the patient to them — giving ORS on the way.

How it works

Blood plasma is about as salty as a solution of 9 g of salt in a litre of water (0.9 %, called normal saline). The body's cells sit in a fluid of the same saltiness. Water always moves from the less salty side of a cell wall to the saltier side (this is osmosis). So:

  • Normal saline in a vein stays outside the cells, where the body has lost it. About a quarter stays in the blood vessels and the rest seeps into the tissues within an hour — which is why large volumes are needed.
  • Plain water in a vein rushes into the red blood cells and bursts them. Never give plain water, sugar water or distilled water into a vein. It can kill.
  • Strong salt water draws water out of the cells and shrivels them. Also dangerous.

What the fluid carries in is just as dangerous as its saltiness. A vein leads straight to the heart, with none of the skin's or the gut's defences. The fluid must be sterile (no living germs) and pyrogen-free — free of the invisible remains of dead bacteria, which cause violent shaking fever within an hour even though the fluid was sterilised. Pyrogens survive boiling and the autoclave. You avoid them by using freshly distilled water, clean glass, and baking the glass hot.

First choice: try the gut harder

Before anyone thinks of a vein, there are two gentler routes that save most people:

Route When How much
ORS by spoon or cup Can swallow, even if drowsy or vomiting Small sips every minute; vomiting usually settles after the first hour. See Oral Rehydration
ORS by nasogastric tube Conscious enough to protect the airway but too weak or unwilling to drink; or no one can find a vein 20 ml per kg of body weight per hour for 6 hours (120 ml/kg in all), then reassess
Saline under the skin (subcutaneous) Moderately dry, cannot drink, no vein; not for shock — too slow About 1 ml a minute per site; up to 1.5 litres a day per site
Intravenous drip Shock, collapse, no wrist pulse; or unconscious Rates below

Passing a nasogastric tube. Use a soft rubber tube, about 4–5 mm across for an adult and 3 mm for a small child (Rubber), boiled and cooled. Measure from the tip of the nose to the earlobe and down to the bottom of the breastbone; mark that length. Sitting the person up, slide the lubricated tube gently along the floor of one nostril and down, asking them to swallow if they can. Then check that it is in the stomach: suck back with a syringe — stomach juice is cloudy and turns blue litmus or red-cabbage paper red-pink (acid; Acids, Bases and Testing). If they cough, choke, cannot speak or turn blue, pull it out at once — it is in the windpipe. Tape it to the nose and run ORS in slowly from a funnel or bottle held a little above the head.

Saline under the skin (hypodermoclysis) needs only a fine needle slid flat under the loose skin of the belly, upper thigh or between the shoulder blades, and a bottle of sterile normal saline running slowly. A soft swelling forms and spreads; it is absorbed over hours. If the swelling becomes hard, red or painful, stop and choose another site.

What you need

Item Notes
Salt The purest you can make, recrystallised (Salt)
Distilled water Fresh from a glass or tinned-copper still with a glass receiver (Distillation)
Balance Weighing to 0.1 g (Measurement from Scratch). Saline cannot be made by spoonful
Glass bottles 500 ml or 1 litre, thick-walled, with narrow necks (Glass, Laboratory Glassware)
Rubber stoppers Bored with two holes, or a solid stopper the needle can pierce (Rubber)
Autoclave Pressure vessel reaching 121 °C (Sterilising Instruments and Dressings, Canning and Bottling)
Oven Reaching 250 °C, for baking glass (The Kiln)
Giving set Rubber tubing, glass drip chamber, air inlet tube, cotton, clamp (Laboratory Glassware)
Needles Hollow steel or silver, 1.0–1.3 mm across for adults, 0.8 mm for children, 3–4 cm long, with a hub (Metal Pipes and Tubes, Needles and Pins)
Tourniquet A strip of rubber or a cloth band
70 % alcohol For the skin (Distillation)
Splint board, cloth strips To hold the arm still
Watch, record sheet Every drip is charted

Making sterile normal saline

1. Weigh2. Fresh water3. Fill, tie4. Autoclave5. Inspect 9.0 g of puresalt per litre;never by spoon distilled today,into baked glass;first tenth thrown away filter into bottlesbaked at 250 °C, fillto nine-tenths, tiestoppers down 121 °C: 30 min for500 ml, 40 min for1 litre; let it coolby itself against the light:clear, or throw itaway (haze, specks,cracks, loose seal) 9/10
Fig. 1 Making normal saline. Weigh 9 g of pure salt into each litre of freshly distilled water, fill baked bottles, tie down the stoppers, and steam them at 121 °C. Every bottle is held to the light before use: any haze, speck or crack means it is thrown away.

1. Pure salt

  1. Dissolve sea or rock salt in distilled water, filter through clean cloth and paper, and boil down until crystals form; scoop them out while plenty of liquid is left (the impurities stay in it). Repeat once more.
  2. Heat the crystals in a clean iron or glazed pan until they crackle and stop steaming, and a little beyond, to burn off any organic dust — a scrap of paper laid on top should scorch brown.
  3. Store in a clean stoppered jar used for nothing else.

2. Glass

Wash bottles in hot water and soap, rinse many times, finish with distilled water, then bake them at about 250 °C for at least half an hour (a scrap of paper inside scorches dark brown) — this destroys pyrogens. Boil the rubber stoppers in three changes of distilled water; they cannot be baked.

3. Mixing

  1. Use water distilled that same day, collected in baked glass. Throw away the first tenth of each run.
  2. Weigh 9.0 g of salt per litre — never estimate. Between 8.5 and 9.5 g is acceptable; outside that, discard.
  3. Dissolve, then filter through a fresh paper filter in a baked funnel into the bottles. Fill each to nine-tenths (room for expansion).
  4. Check the strength if you can: 10 ml of correct saline contains 54.6 mg of chloride; titrated with silver nitrate standard of 1 mg chloride per ml, it takes 54–55 ml (Silver Nitrate and Silver Salts).

4. Sealing and sterilising

  1. Push in the stoppers and tie them down with boiled cord or wire over the top — steam pressure pushes them out. Cover each neck with a cap of paper tied on.
  2. Load the autoclave so steam can reach every bottle. Purge the air as in Sterilising Instruments and Dressings.
  3. Hold at 121 °C (1 bar above air pressure) for 30 minutes for 500 ml bottles, 40 minutes for 1 litre, counted from when the whole load is hot. A sealed glass tube of sulfur crystals placed among the bottles must have melted.
  4. Let the autoclave cool by itself until the gauge reads zero. Never open the valve early: the hot liquid boils violently, blows out stoppers and can burst bottles.
  5. Label each bottle: "Normal saline 0.9 %", batch number, date.
  6. Keep one bottle from each batch in a warm place for a week. If it turns cloudy, the whole batch was not sterile — destroy it.

Inspecting before use

Turn the bottle upside down against a bright window and then against a dark cloth, and swirl it. It must be perfectly clear, with no specks, threads or cloudiness, no crack, and the stopper and seal intact. If in any doubt, throw it out. Use home-made bottles within about a month.

Note Better fluids. Normal saline replaces salt and water but not the potassium and the alkali that cholera also strips out. Ringer's lactate (Hartmann's solution) — salt, sodium lactate and a little potassium and calcium chloride — is better and is what clinics prefer, but making pure sodium lactate takes a chemistry laboratory. With saline alone, start ORS by mouth the moment the patient can drink: it supplies the potassium and alkali. Never add potassium to a drip yourself — potassium run too fast into a vein stops the heart.

The giving set

About1 m Sealed bottle of salinehung upside down; checked clear first Air inlet, cotton filterlong glass tube; air bubbles inas fluid runs out Drip chamberone-third full; count the dropsfor a full minute Screw clampsqueezes the tube to set the rate Needle flat in veinhub taped down arm bandaged to a padded board
Fig. 2 A gravity drip. The sealed bottle hangs upside down about a metre above the arm. Air enters through a cotton-plugged inlet tube as fluid leaves; drops are counted in the glass drip chamber; a screw clamp on the rubber tube sets the rate. The needle is taped flat in the vein and the arm splinted to a board.
  1. Bottle and stopper. Through a two-holed rubber stopper pass two glass tubes: a long air inlet that reaches the bottom of the bottle (the top, when hung upside down), plugged outside with a wad of baked cotton as an air filter; and a short outlet flush with the inside of the stopper.
  2. Drip chamber. A glass tube about 1.5 cm wide and 6 cm long, with a drawn-out glass jet at the top inside it, joined below the outlet. Drops form at the jet and fall through the air in the chamber, where you can count them. Keep it about one-third full of fluid so air bubbles cannot pass down.
  3. Tubing. About 1.5 m of rubber tube, 3–4 mm bore, ending in a tapered metal or glass nozzle that fits snugly into the needle's hub.
  4. Clamp. A screw clamp of brass or hardwood that squeezes the tube flat by turns of a thumbscrew.
  5. Calibrate the jet. Count how many drops fill 10 ml in a measuring cylinder. Most jets give 15–20 drops per ml. Scratch the number on the chamber.
  6. Sterilise the assembled set wrapped in cloth by autoclave, as for dressings.

The needle. Hollow steel needles are made from fine drawn tube (Metal Pipes and Tubes, Iron and Brass Wire), ground to a short bevel and soldered into a brass hub (Soldering and Brazing). Silver tube also works and does not rust. Making them is the hardest part of this chapter; treat each one as precious. After use, clean it at once with a fine wire and water, check under a lens for burrs and a sharp point (Lenses), hone on a fine stone if needed, and sterilise it. One needle, one patient, between each sterilisation — reused needles spread hepatitis and HIV (Sterilising Instruments and Dressings).

Step by step: putting up a drip

  1. Decide. Is the patient truly unable to take ORS by mouth or tube, or in shock? Weigh them, or estimate (an adult is usually 50–70 kg; see Examining a Patient). Write down the plan.
  2. Prepare. Inspect the bottle. Hang it 1 metre above the bed. Fill the drip chamber one-third by squeezing it, then open the clamp and run fluid through the whole tube until no bubbles remain. Clamp it.
  3. Hands. Wash with soap for a full minute (Sanitation and Germs).
  4. Find a vein. Use the back of the hand, the forearm, or the crease inside the elbow (largest, but the elbow must then be splinted straight). Tie the tourniquet 5–10 cm above, tight enough to swell the veins but not to stop the wrist pulse. Hang the arm down, tap the vein, have the person open and close their fist. A good vein feels springy.
  5. Clean the skin with alcohol and let it dry. Do not touch it again.
  6. Insert. Hold the skin below taut with your thumb. With the needle bevel up, at about 20° to the skin, go through the skin just beside or below the vein, then into the vein. You feel a slight "give", and blood appears in the hub. Lower the needle almost flat and slide it 0.5–1 cm further along the vein.
  7. Release the tourniquet. Connect the line, open the clamp, and watch: it should run freely and the skin around should not swell. If it swells, the needle is outside the vein: clamp, pull out, press, and try another site.
  8. Secure. Tape or tie the hub flat with cloth strips, cover with sterile gauze, and bandage the arm to a padded board so it cannot bend. A steel needle in a vein cuts through it if the arm moves.
  9. Two attempts each, then let someone else try. Collapsed patients have flat veins and are hard; do not waste the patient's time. Start a nasogastric tube while you keep trying.

Veins in babies and collapsed small children are tiny and very hard to find. Use the nasogastric tube for them and look for skilled help. Cutting down onto a vein, or putting a needle into the bone marrow of the shin, are procedures for trained hands only (Basic Surgery).

How much and how fast

For severe dehydration from diarrhoea or cholera, give 100 ml per kg of body weight of normal saline (or Ringer's lactate) in two parts:

Age First 30 ml/kg in Then 70 ml/kg in
Under 12 months 1 hour 5 hours
12 months and older, including adults 30 minutes 2½ hours
  • If the wrist pulse is still very weak or absent after the first part, give the first part once more.
  • Check every 15–30 minutes: pulse, alertness, skin pinch (Oral Rehydration). If not improving, run faster.
  • Start ORS by mouth (about 5 ml per kg per hour) as soon as the person can drink — usually after 1–2 hours for adults, 3–4 for babies.
  • At the end, reassess fully. If still severely dry, repeat the whole course; if some signs remain, continue with ORS; if well, stop the drip.

Example: a 60 kg adult in collapse needs 1,800 ml in the first 30 minutes — 60 ml a minute — and then 4,200 ml over 2½ hours. One gravity drip through a 1.2 mm needle cannot run that fast: use the widest needle you have, raise the bottle higher, or put up two drips, one in each arm.

Converting to drops. Drops per minute = millilitres per hour × drops per ml ÷ 60. With a jet of 20 drops per ml, drops per minute = millilitres per hour ÷ 3. A litre over 4 hours is 250 ml per hour, about 83 drops a minute. Count for a full minute; recount every 15 minutes, because the rate drifts as the bottle empties.

Warning Go slowly for the frail. For a severely malnourished child, give only 15 ml per kg over 1 hour, and only if in shock; then switch to oral or tube feeding of rehydration fluid and watch the breathing closely (Nutrition and Deficiency Diseases). The very old, and people with heart or kidney disease, also drown easily in fluid. For them, give smaller amounts — perhaps 250 ml at a time — and listen to the chest before each. In shock from bleeding, give saline only until bleeding is stopped and blood is ready; do not try to raise the pulse to normal with saline alone.

How to tell it worked

Keep a chart: time, volume given, pulse rate and strength, breathing rate, alertness, urine passed, and the state of the drip site.

  • Working: the wrist pulse comes back and strengthens; the person wakes, speaks, asks to drink; skin pinch springs back faster; eyes look less sunken; urine is passed within a few hours. These, not the bottle count, decide when to stop.
  • Too much: breathing becomes faster, the person coughs, the eyelids puff, ankles swell, and with your ear to the lower back you hear fine crackles like hair rubbed between fingers near the ear. Neck veins stay swollen when the person sits up. Stop or slow the drip at once, sit them up, and reassess.

Note Troubleshooting. Drip stops → clamp too tight; bottle too low; air inlet cotton wet (replace); needle blocked by clot or against the vein wall — lift or turn the arm a little. Never flush a blocked needle by force; take it out and put in another. Swelling, coolness or pain around the needle → fluid is going under the skin. Stop, remove, re-site in the other arm. Shaking chills and fever within an hour of a new bottle → pyrogens or contamination. Stop that bottle, keep the person warm, and discard the whole batch. Red, hot, tender cord along the vein → inflammation or infection of the vein. Remove the needle, re-site, apply warm cloths. Change drip sites every 2–3 days anyway. Cannot get into a vein → nasogastric ORS, now. Then warm the limb in warm water for five minutes and try again, or let a more experienced person try.

Dangers

Danger Contaminated fluid kills quickly. Bacteria growing in a bottle of saline cause overwhelming blood poisoning — fever, rigors, collapse — that is often fatal. Never use a bottle that is cloudy, cracked, has a loose stopper, has been opened before, or comes from a batch whose test bottle went cloudy. Never top up a bottle. Never use the same bottle for two patients.

Danger Air in the vein. Prime the whole line before connecting, keep the drip chamber one-third full, and never let the bottle run dry — with an air-vented glass bottle, air follows the fluid down the line. Clamp the tube while there is still fluid in the neck of the bottle, then change bottles. Small bubbles in the tube are harmless; a long column of air reaching the vein is not.

Danger Wrong fluid kills. Plain or distilled water, sugar water, strong salt water, or anything with potassium run in fast can stop the heart or destroy the blood. Every bottle is labelled at filling and checked again at the bedside, aloud, by two people.

  • Fluid overload drowns the lungs. Watch the breathing as closely as the pulse.
  • Blood-borne disease. One sterile needle per patient; sharps into a closed tin; never recap a used needle by hand.
  • Hurting the arm. Repeated stabbing bruises veins and nerves. Two attempts each, then stop.
  • Giving the drip and forgetting ORS. Saline lacks potassium. A patient kept on saline for a day without ORS or food grows weak and their heart rhythm can fail.

What this unlocks

Sterile, pyrogen-free fluid and a reliable drip set are the gateway to Blood Typing and Transfusion, to safe major Basic Surgery (fluids during and after operations), to treating severe burns, and to slow intravenous medicines such as Penicillin. The skills — sterile bottling, counting drops, charting — are the core of hospital Nursing the Sick.

How it was first done

In 1831, during the first cholera epidemic in Britain, the young Irish doctor William O'Shaughnessy analysed cholera patients' blood and found it had lost water and salts; he urged replacing them in the veins. In May 1832 Thomas Latta of Leith, near Edinburgh, did it: he injected several litres of salt water into the vein of an elderly woman near death, and she revived dramatically — though she relapsed and died after he left her, because no one kept the fluid going. Without sterility many patients died of infection, the practice was forgotten for decades, and doctors went back to bleeding and purging. In the 1880s Sydney Ringer in London found that a frog's heart kept beating far longer in salt water containing a little potassium and calcium — the origin of Ringer's solution; Alexis Hartmann added lactate for children in the 1930s. Leonard Rogers in Calcutta, from about 1909, cut cholera deaths sharply with large volumes of intravenous salt solution. In 1923 Florence Seibert in the United States showed that the fevers which often followed infusions came from bacterial remains in poorly distilled water, and that careful distillation prevented them — making drips routine. Plastic cannulas and bags replaced steel needles and glass bottles from the 1950s and 1960s; and from the late 1960s, oral rehydration showed that most cholera patients need no drip at all.

Source: content/entries/health/iv-fluids.md