◆ Rebuild

Part 10 · Machines

Sharpening and Honing

Why an edge cuts and how it goes dull, and how to bring it back — bench stones and slipstones, strops, honing steels, angle jigs and the saw vice — with the right method for knives, chisels, plane irons, gouges, axes, saws, scythes and drills, and honest tests of sharpness.

Difficulty
●●●●●
Time
Ten minutes to sharpen a chisel or knife; half an hour for a handsaw; an afternoon to make a stone box, strop and jig
Steps from zero
15 prerequisites →

You need first

Abrasives and Grinding StonesAxes, Chisels, Knives and Planes

This unlocks

—
The full path from nothing — 15 steps before this one
  1. Stone Tools
  2. Fire
  3. Cordage and Rope
  4. Finding and Preparing Clay
  5. Finding and Identifying Ores
  6. Hunting and Trapping
  7. Basic Woodworking
  8. Abrasives and Grinding Stones
  9. Charcoal
  10. Hides and Leather
  11. Bellows
  12. Iron (the Bloomery)
  13. Blacksmithing
  14. Steel
  15. Axes, Chisels, Knives and Planes
  16. Sharpening and Honing

Do them roughly in this order. See it on the tech tree →

Why it matters

Every cutting tool in this book — the axe, the plane, the scythe, the surgeon's knife, the lathe tool, the drill — is only as good as its edge, and every edge goes dull with use. A dull tool needs twice the force, tears instead of cutting, wanders off the line, and slips. More cuts happen with blunt knives than sharp ones, because people push hard and the blade skids.

Making the stones is covered in Abrasives and Grinding Stones and making the tools in Axes, Chisels, Knives and Planes. This chapter is the craft of keeping every kind of edge sharp, and the small objects that make it quick and repeatable.

How it works

An edge is where two surfaces meet. A shaving-sharp edge is rounded off to less than a thousandth of a millimetre — too fine to see. A dull edge is rounded, chipped or folded over, and catches light as a bright line.

The angle is a trade-off. The included angle is the full angle between the two faces at the edge. A thin angle slices easily but chips or rolls; a thick one is strong but pushes. Match the angle to the work:

Tool Included angle Notes
Razor 15–17° Only for hair; stropped every use
Carving and kitchen knife 30–40° Two bevels, 15–20° each
Chisel, plane iron 25° ground, 30° honed Single bevel; flat back
Gouge and turning tools 25–55° See Wood Turning and Treen
Felling axe 40–50°, convex Faces swell gently behind the edge
Splitting axe, maul 50–60° and more Must wedge, not slice
Scythe Very thin, peened Kept keen by peening and honing
Twist drill 118° point 8–12° clearance behind the lips
Cold chisel for metal 60–70° Struck with a hammer

Bevel shapes.

25° wheel 25° 30° strip (drawn wide) burr Flat bevel simple; the whole bevel is honed Hollow grind from the wheel; only two narrow lands Secondary bevel ground 25°, a thin strip honed at 30° Convex faces curve into the edge; axes, adzes The burr steel folded over; strop it off
Fig. 1 Edge shapes in section, and the burr. A flat bevel is simple; a hollow grind from a wheel leaves only two narrow lands to hone; a narrow secondary bevel a few degrees steeper hones in seconds; a convex edge is strongest. Grinding or honing one side folds a thin burr over to the other.
  • Flat (V) bevel — the bevel is ground straight. Simple, but the whole bevel must be honed each time.
  • Hollow grind — a grinding wheel leaves the bevel slightly hollow. Only the heel and the very edge touch the stone, so honing is quick, and the hollow tells you when to regrind.
  • Secondary (micro) bevel — grind the main bevel at 25°, then hone only a narrow strip 0.5–1 mm wide at the very edge at 30°. Re-honing that strip takes ten strokes; regrinding is needed only every few dozen sharpenings.
  • Convex edge — the faces curve into the edge like a lens. Strongest for chopping (axes, cleavers, adzes), made by rocking the tool on the stone or stropping on a soft backing.

The burr. When you abrade one face right down to the edge, the last sliver of steel folds over to the other side as a burr (wire edge). Feeling it along the whole length tells you that you have reached the edge. Remove it with lighter strokes on alternate sides, then stropping.

Grit steps. Each stone leaves scratches the size of its grit, and the next finer stone must remove them. Go coarse (grit about 0.1 mm), medium (0.03 mm), fine (0.01 mm), then polish (0.001–0.003 mm on a strop). Skipping a step leaves deep scratches and a ragged edge.

Lubricant. Water or thin oil floats away the swarf — steel and stone particles — so the stone keeps cutting. Soft, open stones use water; dense, hard ones like novaculite cut better with thin oil. An oiled stone will not take water again.

What you need

Item Size or grade Notes
Grindstone 50–80 cm wet sandstone wheel Reshaping, chips, new bevels (Abrasives and Grinding Stones)
Coarse bench stone Sandstone or coarse emery, 20 × 5 × 2.5 cm Removing nicks, setting bevels
Fine bench stone Fine sandstone, slate, coticule, or fine bonded emery Everyday honing
Polishing stone Novaculite or very fine slate Final edge on chisels, razors, gravers
Slipstones 10 × 5 cm, round and sharp edges Insides of gouges, hook knives, bits
Flattening plate Flat sandstone slab 30 × 30 cm or iron plate, with loose sand Keeping stones flat
Strop Leather 30–60 × 5–6 cm With rouge or tripoli
Honing steel 25–30 cm hardened rod Kitchen and butchers' knives
Files 20–25 cm flat "mill" file; triangular saw files Axes, mower blades, saws (Files and Saws)
Jigs Honing guide, angle wedges, saw vice, drill gauge Made below
Lubricant Water, or thin plant oil cut with a little turpentine

Where to find it

  • Sandstone for grindstones and coarse stones: even-grained, medium-hard, not crumbly (Rocks and Minerals). The best scratches steel quickly without its grains falling out in lumps.
  • Fine natural hones. Novaculite — a very hard, very fine, white to grey, slightly translucent rock like flint, in thick beds in folded mountains (those of Arkansas are famous) — gives the finest edges of all. Slate — fine roofing slate, used wet. Coticule — a yellowish layer full of microscopic garnets in the slates of the Belgian Ardennes. Test any fine, uniform, hard rock by rubbing a wet steel blade on it: a good hone turns grey with slurry within a few strokes and leaves fine, even scratches.
  • Emery and corundum to make artificial stones bonded like grinding wheels (Precision Grinding).
  • Polishing powders: red hematite ground to rouge, tripoli (rottenstone), fine pumice, or the finest silt settled from clay (Abrasives and Grinding Stones).
  • Leather for strops: the thick back (butt) of cow or horse hide, 3–5 mm thick, vegetable-tanned (Hides and Leather).

The sharpening tools

Bench stone

The everyday stone that lives on the workbench. Make it 20 × 5 × 2.5 cm — long enough for a full stroke, wide enough for a 5 cm plane iron. A combination stone, coarse on one face and fine on the other, does most jobs. Shape and flatten it as in Abrasives and Grinding Stones.

  1. Box it. Chisel a snug recess 5 mm deep into a hardwood block 25 × 8 × 4 cm, make a matching lid to keep grit off, and glue a strip of leather under the box so it does not slide.
  2. Artificial stones. Mix 85 parts graded emery or corundum to 15 parts fired-clay bond by weight, press into a wooden or iron mould 22 × 6 × 3 cm, dry for a week, and fire it like a grinding wheel to about 1,200–1,250 °C (Precision Grinding). Coarse grit for the coarse stone; settled flour-fine grit for the fine one.
  3. Keep it flat. A hollow stone rounds edges. Every few sessions, scribble pencil lines over the face and rub it in figure-of-eight strokes on the flattening plate with water and sand until the lines are gone. No light should show under a straightedge laid across it.

A good stone bites steel at once, raises slurry, and is even-grained; a bad one glazes shiny, scratches unevenly, or has hard specks that cut deep lines.

Slipstone

A small hand-held stone for curved edges: the inside of gouges, hook knives, auger bits and cutters. Grind fine stone on the flattening plate into a wedge about 10 × 5 cm, one long edge 1 cm thick and rounded, the other tapering to 2 mm. Make two or three curves so one fits every gouge. Rub it flat inside the curve to remove the burr, never tilting it into a second bevel.

Strop

A strip of leather charged with very fine polish. It removes the last of the burr and polishes the edge.

  • Paddle strop for tools: glue a strip of leather 30 × 6 cm, flesh side up, onto a flat hardwood board 40 × 6 × 2 cm with a handle at one end (Glues and Adhesives). Rub in a crayon of rouge or tripoli mixed with tallow or beeswax (about 3 parts powder to 1 part wax, melted and cast in a stick). A hard backing keeps chisel edges flat.
  • Hanging strop for razors: a strip of smooth leather 50–60 × 6 cm with a ring at one end to hang from a hook and a handle at the other; a second strip of linen canvas hangs beside it. Draw the strop taut and use it bare or very lightly charged.

Always pull the edge trailing — spine first — so it cannot dig in. Use light pressure; 10–30 strokes a side. Heavy pressure on a soft strop rounds the edge over.

Honing steel

A butcher's steel does not remove much metal: it pushes a rolled or wavy edge back into line, so a knife can be kept keen through a day's work between stonings.

  1. Forge a round rod of high-carbon Steel 1–1.3 cm thick and 25–30 cm long, tapering slightly, with a tang.
  2. File or chisel fine, shallow grooves along its length, about 0.3–0.5 mm apart — or leave it smooth and polished for fine knives.
  3. Harden it and temper only to pale straw (about 220 °C): it must be harder than any knife.
  4. Fit a handle with a guard — a metal or horn disc at least 5 cm across — to stop the hand sliding onto the blade.

Use: hold the steel point-down on a board. Lay the knife's heel against it at its edge angle (15–20°) and draw the blade down and back so the whole edge, heel to tip, crosses the steel. Alternate sides, five or six light strokes each. If the knife still drags after steeling, it needs the stone.

Sharpening jigs

Holding a steady angle by hand takes practice. A jig makes every sharpening the same.

ROLLER HONING GUIDE STONE BOX AND SLIP 25–30° Projection longer = lower angle Clamp screw blade bevel-down Edge Roller rides on the stone push and pull lid keeps grit off Bench stone 20 × 5 × 2.5 cm Leather strip stops sliding Slipstone flat in the flute Gouge end view
Fig. 2 Sharpening jigs. Left: a roller honing guide clamps a chisel so its edge meets the stone at a set angle; the projection — the distance from clamp to edge — sets that angle. Right: the bench stone in its box, and a slipstone for the inside of a gouge.
  • Roller honing guide for chisels and plane irons. A hardwood block 8 × 5 × 3 cm with a clamp plate and two screws (Screws, Nuts and Bolts) on top and a roller 2 cm across underneath, which rolls on the stone behind the edge. Clamp the blade bevel-down. The projection from the clamp to the edge sets the angle: longer projection, lower angle. If the clamp holds the blade's back 2.5 cm above the stone, about 5.9 cm of projection gives 25° and 5 cm gives 30°. Check once with an angle template (Measuring Angles: Theodolite and Sextant), then make a setting board with stops at those distances so every blade is set the same in seconds.
  • Angle wedges for knives. Hardwood wedges at 15° and 20°: rest the spine on one to find the angle, then hold it. Better, a clamp-and-rod jig: the knife is clamped in jaws, and a small stone on a rod slides through a hole in a post on the jaws set at the chosen angle, so the angle cannot wander.
  • Grinding rest. On the grindstone, a hinged platform locked at the bevel angle supports chisels squarely. For gouges, an arm with a V-shaped pocket holds the end of the handle a set distance from the wheel; the gouge pivots and rolls in the pocket and grinds the same fingernail shape every time.

Saw vice

SAW VICE (END SECTION) DRILL ON ITS GAUGE File push stroke only Teeth gullets 3–5 mm above the jaws Jaws hardwood, as long as the saw Wedge or screw axis Lip at 59° 118° point 59° edge marked in mm; both lips reach the same mark Drill gauge sheet steel; body lies along the straight side
Fig. 3 Left: a saw vice grips the saw plate along its length with the gullets just above the jaws, so the file does not chatter. Right: a drill laid on its gauge; each lip should lie along the 59° edge and reach the same mark.

A saw filed on the open bench chatters and blunts the file. A saw vice grips the plate along its whole length just below the teeth: two hardwood jaws 5–8 cm deep and 40–70 cm long, bevelled on top for the file, hinged at the bottom on a post at elbow height (or held in the bench vice) and closed with a wedge or screw. Set the gullets 3–5 mm above the jaws.

Drill gauge

A plate of sheet steel (Sheet Metal and Rolling) 8 × 4 cm with one edge cut at 59° to a straight side, and that edge marked off in millimetres. Lay the drill's body along the straight side: each lip should lie along the 59° edge and both lips should reach the same mark. Unequal lips drill oversize holes.

Sharpening each tool

Knives

  1. On the coarse stone, sharpen one side at its angle, sweeping so the whole edge from heel to tip passes over the stone. Lift the handle slightly as you reach the curved belly so the angle stays the same there.
  2. Stop when a burr runs the whole length. Do the other side the same.
  3. On the fine stone, alternate sides with lighter strokes until the burr is tiny; strop.
  4. When sharpening takes many strokes, the edge has crept back into thick steel: thin the blade a little way behind the bevel on the coarse stone.

Chisels and plane irons

The flat back is half of the edge. A back that is rounded or pitted can never make a keen edge, however good the bevel.

  1. Flatten the back once. Rub the first 3–5 cm of the back flat on the coarse stone, then the fine, then the polishing stone, until it is one even mirror with scratches all one way. Keep the stone flat.
  2. Grind the main bevel at 25° on the grindstone, square to the sides (check with a try square), slightly hollow.
  3. Hone a secondary bevel at 30° in the honing guide: ten to twenty strokes on the fine stone until a burr forms all along.
  4. Remove the burr with two or three strokes of the back flat on the polishing stone, never lifted. Then a few strokes on bevel and back alternately, and strop.
  5. Re-sharpen by honing only the secondary bevel. When it grows wider than 1–2 mm, regrind.
  6. A smoothing plane iron is rounded very slightly at the corners — a few strokes of extra pressure at each side — so the plane leaves no ridges.

Gouges and carving tools

Hone the outside bevel by rolling the gouge from one side to the other as you push it along the stone, or work across the stone in a figure-of-eight, so every part of the curve is honed at the same angle. Take the burr off the inside with a slipstone held flat in the curve. Strop the inside with leather wrapped round a shaped stick. Turning tools are dealt with in Wood Turning and Treen.

Axes and adzes

  1. Brace the head against a log and wear a glove. Push a flat file from the edge back into the body, forward strokes only, over a band about 2.5 cm wide each side. Keep the faces gently convex, never ground to a sharp shoulder. File both sides until no nicks remain and a small burr forms.
  2. Finish with a round axe stone ("puck"), coarse then fine, in small circles along both sides, wet.
  3. Sight along the edge in good light: an even narrow polished band each side, no bright spots on the very edge.

Scythes and sickles

Scythe blades are kept sharp by peening — cold-hammering the edge thin on a small anvil every few hours — and by honing with a long curved stone in the field every 10–15 minutes. The full method is in Sickle, Scythe and Hand Harvest Tools. A sickle is honed the same way, with a small stone stroked along the inside curve.

Saws

In the saw vice, in four steps described in Files and Saws: joint the teeth level with a flat file along their tops; shape uneven teeth; set alternate teeth outward (only every third or fourth time); and sharpen each tooth with a triangular file until the shiny flat left by jointing just disappears. Use a file whose face is about twice as wide as the teeth are deep, file on the push stroke only, and give every gullet the same strokes at the same pressure. A handsaw in daily use needs it every few weeks; it takes half an hour.

Drills and bits

Twist drills (Drills and Boring). Hold the drill with its axis at 59° to the wheel face and one lip level. Grind while swinging the shank down and twisting it slightly, so the surface behind the lip falls away by 8–12° — the clearance that lets it cut. Turn it half round and grind the other lip the same, then check on the gauge. End-on, the short chisel edge across the centre should lie at about 120–135° to the lips. For brass and bronze, grind a tiny flat on the front of each lip so the drill does not grab.

Auger and brace bits. File the spurs from the inside only and the cutting lips from the shank side only; filing the outside of the spurs makes the bit cut undersize and bind.

Scissors and shears

Hone only the narrow outer bevel of each blade, at its original angle (usually 60–75°), and never the flat inside face. See Scissors, Shears and Folding Knives.

How to tell it worked

  • The light test. Hold the edge up under a light and look straight down on it. A sharp edge is invisible. A bright line or bright dots show dull or chipped places.
  • The thumbnail test. Rest the edge on your thumbnail at about 30°, with no pressure, and push it gently along. A sharp edge bites and stops; a dull one skates. Test along the whole edge. Gravers and chisels are tested this way.
  • Paper. Hold a sheet of paper up by one corner and slice it from the top: a sharp knife cuts a clean, silent curl; a dull one tears or snags.
  • End grain. A sharp chisel pares a thin, shiny shaving from the end grain of soft pine without crumbling the fibres; a sharp plane takes a shaving thin enough to read print through.
  • Hair. A razor or knife shaves forearm hair without pressure.
  • Under a lens (Lenses), a good edge is a single straight line, with even scratches running the same way on both faces.

Note Troubleshooting. Never gets sharp → you never raised a burr along the whole edge, or the angle rocked. Use a guide; go back to the coarse stone until the burr runs from end to end. Sharp at first, dull in minutes → a burr left on and folding over, or an angle too low for the job. Strop well; add a steeper secondary bevel. Edge rounded, will not bite → stone hollow, or too much pressure on a soft strop. Flatten the stone; use a hard-backed strop. Chisel edge out of square → uneven pressure. Push on the centre of the blade; regrind square. Saw runs to one side → more set on one side, or uneven filing. Joint lightly, file the weak side, or take set off with a stroke of a stone along the side that runs. Drill squeals and will not cut → no clearance behind the lips. Drill cuts oversize → unequal lips. Stone glazed and shiny → clogged; scrub it with sand and water, or use more lubricant. Edge turned blue on the grinder → temper lost; grind back past it with lighter pressure and more water.

Dangers

Danger Dry grinding dust killed whole trades. In 19th-century Sheffield, cutlers who dry-ground forks on sandstone breathed stone and steel dust all day; many died of lung disease ("grinders' asthma", now called silicosis) before the age of forty. Always grind sandstone wet, keep the trough full, and work where the air moves.

  • Cuts. Most sharpening injuries happen when testing or wiping the edge. Never run a finger along an edge; wipe a blade from the spine outward; test on paper, not skin. Keep fingers behind the stone when honing scythes and axes.
  • Grinding wheels turned by power can burst. Never run a wheel faster than it was made for, and stand aside when starting one (Precision Grinding).
  • Eyes. Sparks and grit fly from dry wheels and files. Wear eye protection.
  • Overheating draws the temper and ruins a tool. Dip in water often; if it turns straw or blue, stop.

What this unlocks

Sharp tools make every other craft faster and safer: Basic Woodworking, Timber Framing and Log Building, Wood Turning and Treen, Hides and Leather, Butchery and Meat, Basic Surgery and the harvest (Sickle, Scythe and Hand Harvest Tools). The skills here — holding an angle, judging flatness, removing a burr — lead straight to Precision Grinding, the sharpening of lathe and milling tools (Machine Tools), and the fine gravers of Engraving, Seals and Etching and Watches and Small Clocks.

How it was first done

The first edges were renewed by striking fresh flakes off a stone tool (Stone Tools). Neolithic people ground and polished stone axes on big sandstone boulders, and the grooves worn by thousands of sharpenings — polissoirs — can still be seen on rocks across Europe. Bronze and iron tools were honed on whetstones from the start; the Roman writer Pliny the Elder, in the 1st century AD, described whetstones used with oil and with water and named the best sources. Arkansas novaculite was used by Native Americans long before it was quarried commercially in the 19th century. The dry-grinding disease of Sheffield's cutlers was one of the first industrial illnesses studied by doctors, and led to wet grinding and dust extraction. Artificial abrasives — silicon carbide (1891) and fused alumina (about 1900) — made uniform stones cheap everywhere.

Source: content/entries/mechanics/sharpening.md