Part 12 · Transport
Balloons
Hot air is lighter than cold air; a big enough bag of it lifts people. How to work out the size, cut and sew the envelope from silk or cotton, coat it, heat it, fly it tethered first — and why hydrogen lifts four times as much but turns any spark into a fireball. The first way humans ever flew, and still the safest place to start.
- Difficulty
- ●●●●●
- Time
- A weekend for a paper model; two to three months of sewing for a person-carrying envelope; much practice before free flight
- Steps from zero
- 4 prerequisites →
This unlocks
AirshipsThe full path from nothing — 4 steps before this one
Do them roughly in this order. See it on the tech tree →
Why it matters
A balloon is the simplest machine that flies. It has no engine, no wings and no moving parts: just a bag of air, heated so it is lighter than the air around it. People first left the ground in one in 1783, more than a hundred years before the first aeroplane.
The most useful thing a balloon does is let you see far. From the ground, the horizon is about 5 km away. From a tethered balloon 100 m up, it is about 36 km; from 300 m, about 60 km (the rule: horizon in km ≈ 3.6 × √(height in m)). From up there you can map a whole valley in an afternoon, follow rivers to their sources, spot smoke from distant fires or settlements, watch Reading the Weather coming, and signal across great distances. A balloon also carries instruments up to measure the air (The Barometer, The Thermometer).
A small paper hot-air balloon is a weekend project. A balloon that lifts a person needs a few hundred square metres of good cloth, careful sewing and great care with fire. It is honest to say that balloons drift where the wind takes them: they are not transport from A to B. For that you need the Gliders and Aeroplanes. But for observation, mapping and the joy of flight, nothing is simpler.
How it works
Buoyancy. Anything surrounded by air is pushed up with a force equal to the weight of the air it displaces. A cubic metre of air weighs about 1.2 kg at 20 °C. Heat it to 100 °C and it expands, so a cubic metre weighs only about 0.95 kg. Each cubic metre of hot air in the bag therefore gives about 0.25–0.3 kg of lift. On a cold morning (0 °C outside) it gives a little more, about 0.35 kg; on a hot afternoon, less. This is why balloons fly best in the cool of early morning.
Hydrogen weighs only 0.08 kg per cubic metre, so it lifts about 1.1 kg per cubic metre — four times as much as hot air, and it does not cool down. The price is that hydrogen mixed with air explodes from any spark.
Size. Lift grows with the volume of the bag (the cube of its size), but the bag's weight grows only with its surface (the square). So small balloons barely lift themselves and big balloons lift a lot. For a roughly spherical envelope of silk or fine cotton weighing, with coating, seams and tapes, about 200 g per m², with air inside at about 100 °C:
| Diameter | Volume | Envelope weight | Gross lift (0.27 kg/m³) | Left for basket, fuel, people |
|---|---|---|---|---|
| 4 m | 34 m³ | 10 kg | 9 kg | none — use paper instead |
| 10 m | 520 m³ | 63 kg | 140 kg | ~75 kg — too little for a person and fuel |
| 15 m | 1,770 m³ | 140 kg | 480 kg | ~340 kg — two people, basket and fuel |
| 18 m | 3,050 m³ | 200 kg | 820 kg | ~620 kg |
So a person-carrying hot-air balloon must be at least 14–15 m across. A tissue-paper model weighing 25–30 g per m² flies at only 2–3 m across.
Keeping it hot. The bag loses heat through its skin all the time, so the fire must keep burning. A modern 2,000 m³ balloon burns about 25–50 kg of propane an hour. The same heat from straw means more than 100 kg of straw an hour — which is why the earliest straw-fired flights lasted only minutes.
What you need
For a 15 m person-carrying hot-air balloon, tethered:
| Item | Amount | Notes |
|---|---|---|
| Envelope fabric | 750–800 m² (about 710 m² plus waste) | Tightly woven Silk (best: light and strong), or fine Cotton or linen calico. 50–120 g per m² before coating |
| Coating | 40–80 litres | For hot air: a fire-retardant alum wash, then size; for hydrogen: rubber solution or boiled linseed varnish (see below) |
| Load tapes and thread | 400–500 m of strong tape, 2.5 cm wide; several km of thread | Sewn over every vertical seam and around the crown and mouth; hemp or linen |
| Rigging | 16–24 ropes 6–8 mm, each 8–10 m | Carry the load from the tapes to the basket or burner frame |
| Basket | About 1.2 × 1.2 × 1.1 m | Woven willow or rattan around a frame; it flexes and absorbs a hard landing (Baskets and Containers) |
| Heat source | See Heating below | Brazier, or a vaporising liquid-fuel burner |
| Tether ropes | Three ropes, 50–150 m each | Strong hemp, 15–20 mm, staked to heavy anchors |
| Ground crew | 6–10 people | To hold the mouth open, tend the fire and handle the tethers |
| Sewing | Needles, thread, a large clean floor | A The Sewing Machine makes it weeks instead of months |
For a model (to learn on): 30–40 sheets of tissue or thin Paper, flour paste glue, a wire or cane ring for the mouth, a 2–3 m model of the same gore pattern.
Where to find it
- Silk — reeled from silkworm cocoons (Silk). The best balloon fabric: strongest for its weight, tightly woven, and slow to let gas through.
- Cotton and flax (linen) — heavier but fine for hot-air balloons (Cotton, Flax, Hemp and Linen).
- Linseed — the seed of flax, pressed for oil (Oils and Pressing); boiled, it becomes a drying varnish.
- Animal gut — the outer membrane of ox or cattle large intestine, scraped thin, makes goldbeater's skin, the most gas-tight natural material; it was used for the gas bags of hydrogen airships.
- Native sulfur — a few crumbs are used as a temperature check (see below).
- Straw and willow — straw for an early fire; willow rods for the basket (Baskets and Containers).
Step by step
1. Learn on a model
- Make a gore pattern (below) for a 2.5 m sphere with 8–12 gores, cut from tissue paper, and paste the edges together with a 1 cm overlap of flour paste.
- Glue the bottom edge to a light cane ring 50–60 cm across (the mouth).
- Fill it from a chimney: a 1 m stovepipe or clay pipe over a small charcoal fire, with the balloon held over the top. Never let flames reach the paper.
- When it tugs upward, let it rise on a thread tether and pull it back down.
Warning Never release a balloon with a burning fuel cup aboard (a "sky lantern"). They land where the wind takes them, still burning, and start roof and grass fires.
The model teaches you the pattern, seams, how fast the air cools, and how wind handles a balloon — for almost nothing.
2. Cut the gores
The envelope is made of gores — long, pointed panels like the segments of an orange peel, sewn edge to edge. For a sphere of diameter D made from N gores:
- Gore length (crown to bottom pole) = 3.14 × D ÷ 2.
- Width at a distance s down the gore from the crown = (3.14 × D ÷ N) × sin(360° × s ÷ (3.14 × D)).
In practice: divide the gore length into 8 equal parts and mark the widths from the table in the drawing, scaled to your balloon; join the points in a smooth curve. Add 2 cm of seam allowance on each edge. Stop each gore at the mouth, where the balloon's diameter has shrunk to about 4 m on a 15 m balloon — wide enough that the flame cannot touch the fabric.
Use 12 gores for a model, 16–24 for a full-size balloon. More gores means more sewing, but a rounder shape and more seams to carry load.
3. Sew
- Sew gores together with a flat-felled seam: fold the edges together, sew, fold over, sew again. This gives four layers of cloth and two rows of stitches, and does not fray.
- Over each vertical seam, sew a load tape running from the crown down past the mouth, ending in a loop. The tapes, not the cloth, carry the weight of the basket.
- At the crown, sew the tapes to a strong crown ring of iron or bent ash, about 30–50 cm across. Close the hole with a separate circular cap fastened with ties — the vent, which the pilot can open by a cord to let hot air out and come down.
- Around the mouth, sew a broad band of tight cloth soaked in alum, or better, a skirt of tightly woven linen soaked in alum or a clay wash, to resist sparks and heat.
4. Coat it
- For hot air: the fabric must be tight, not gas-proof. Soak the lower third (near the fire) in a strong solution of alum — the mordant used in dyeing (Dyes and Mordants) — and let it dry; this makes cloth char rather than flare. The Montgolfiers also lined their cloth with paper.
- For hydrogen: coat the whole envelope with a gas-tight varnish: natural rubber dissolved in turpentine (Rubber, Ether, Acetone and Solvents), or boiled linseed oil, in several thin coats, each dried for days in open air.
Danger Oiled cloth can catch fire by itself. Linseed oil heats as it hardens. A heap of freshly oiled cloth, folded or bundled, can grow hot enough to burst into flame hours later. Dry oiled fabric spread out, in the open air, for weeks, before folding it.
5. Heating
- Straw, wool and wood shavings in an iron brazier hung beneath the mouth, as the Montgolfiers did: very hot, but sparks rise into the envelope. Only for short, tethered flights, with a bucket of water and wet sponges on poles to put out sparks on the cloth.
- Charcoal in a brazier: fewer sparks, steadier heat, but slow to respond.
- A vaporising liquid-fuel burner: alcohol or kerosene from a pressurised tank, heated through a coil so it boils into vapour before burning, like a blowtorch. This is how the modern hot-air balloon became practical. It needs a pressure tank, valves and careful testing; build it only after much experience with fuel and pressure (Petroleum and Refining, Distillation).
Temperature check. The fabric must stay below about 120 °C; silk and cotton scorch above 150 °C. Sew a small cloth pocket at the crown holding a few crumbs of sulfur (melts at 115 °C) and a small piece of tin–lead solder (melts at about 180–190 °C). After each flight look in the pocket: melted sulfur means the crown ran too hot. Melted solder means the fabric is probably damaged.
6. Inflate and fly tethered
- Choose a dawn with almost no wind (under 8–10 km/h — leaves stirring, smoke drifting gently), on a large open field with no trees or buildings downwind.
- Lay the envelope out downwind of the basket. Crew members hold the mouth open while a large hand-cranked fan, or simply the crew flapping the mouth, pushes cold air in until it is half full.
- Light the heat source and direct the heat into the mouth. The balloon rises upright over the basket.
- Attach three tether ropes to stakes at 120° around the launch spot. Load the people and enough ballast (sandbags) to keep it on the ground.
- Add heat until the balloon just lifts, then let it rise slowly on the tethers to 20–30 m on the first flights. Bring it down by letting it cool or by hauling on the tethers.
Free flight comes only after many tethered flights, in steady light winds, with the vent cord, ballast to drop, a long trailing drag rope to slow landing, and a crew following on the ground.
Hydrogen balloons
A hydrogen balloon (a charlière) is a sealed, gas-tight bag with a net or tapes carrying a basket, a valve at the top to let gas out to come down, and sand ballast to throw out to go up. It needs about a quarter the size of a hot-air balloon for the same lift: an 8 m sphere (270 m³) has a gross lift of about 300 kg, or about 250 kg after its own weight.
Hydrogen is made by:
- Iron and dilute sulfuric acid (Sulfuric Acid, Hydrogen, Oxygen and Gases): about 2.3 kg of iron and 4 kg of acid for every cubic metre, plus losses — more than half a tonne of iron to fill an 8 m balloon. The gas must be washed through water and lime water to remove acid spray.
- Steam over red-hot iron in iron or clay tubes in a furnace: the iron rusts and releases hydrogen. French army balloonists made their hydrogen this way in 1794. The rusted iron can be turned back to iron with charcoal and used again.
How to tell it worked
- Model: rises steadily on its tether and stays up while the chimney heat lasts.
- Lift test: with the balloon hot and held down by the crew, hang a spring balance or a bag of known weight; the net lift should match the table within about 20%.
- Leaks: hot spots of escaping air show as shimmering above the fabric; daylight seen through the envelope from inside means loose weave or torn seams.
- Hydrogen: a hydrogen balloon should lose less than 1–2% of its lift a day. Faster loss means poor varnish.
Note Troubleshooting. Will not lift → too small for its weight, air not hot enough, or a cold, windy day. Make it larger, use lighter cloth, or fly at dawn. Rises then sinks quickly → heat lost through leaks or thin cloth; or the fire too small. Coat the upper part, add heat steadily. Envelope flaps and spills air → wind too strong. Do not fly. Fabric scorched near the mouth → mouth too narrow or flame too high. Widen the mouth, add an alum-soaked skirt. Seams tearing → load carried by the cloth instead of tapes. Every tape must run continuously from the crown to a rigging line.
Dangers
Danger Fire. An envelope fire spreads in seconds. Keep wet sponges on poles and water ready on the ground and aboard. Never let the flame touch fabric. Never fly a straw or wood fire free, with no way to put out sparks. Fill fuel tanks on the ground, away from any flame.
Danger Hydrogen explodes. Hydrogen mixed with air explodes from a spark — static electricity from clothing, a nail in a boot on stone, a pipe, a lamp. Never bring fire within 50 m of hydrogen. Never combine hot air and hydrogen in one balloon: Jean-François Pilâtre de Rozier, the first man to fly, died in 1785 when his combined balloon caught fire. The airship Hindenburg burned in 34 seconds in 1937.
- Falls. People fall out at hard landings, or try to hold on to a rising balloon by a rope. Never hold a rope with the balloon lifting you: let go while your feet are still on the ground.
- Wind. A balloon caught by a gust drags its basket across the ground at the speed of the wind. Fly only in light winds; land into open fields.
- Altitude. Above about 3,000 m there is too little oxygen and it is very cold. Stay low.
- Lightning and storms. Never fly when storms are about (Reading the Weather).
What this unlocks
Tethered observation balloons give you Maps and Mapmaking from above, Surveying and Levelling checks, weather observation and long-distance signalling. Carrying a The Barometer and The Thermometer aloft measures how the air changes with height. With a light engine and a propeller, a long gas balloon becomes a steerable airship (Airships). And watching how a balloon moves on the wind is the first lesson for the Gliders and Aeroplanes.
How it was first done
Small hot-air lanterns are an old invention in China. In 1709 the Brazilian-born priest Bartolomeu de Gusmão is reported to have floated a small hot-air balloon before the Portuguese court in Lisbon.
The brothers Joseph-Michel and Jacques-Étienne Montgolfier, paper makers of Annonay in France, flew an unmanned hot-air balloon of cloth lined with paper in public on 4 June 1783. In September they sent up a sheep, a duck and a rooster at Versailles; all landed safely. On 21 November 1783 Jean-François Pilâtre de Rozier and the Marquis d'Arlandes made the first free flight by humans, from the Bois de Boulogne in Paris, for about 25 minutes and about 9 km, feeding straw into a fire hung below the mouth.
Ten days later, on 1 December 1783, the physicist Jacques Charles and Nicolas-Louis Robert flew a hydrogen balloon of rubber-coated silk from the Tuileries gardens for about two hours, landing some 36 km away — with a valve, ballast and a basket, the design of every gas balloon that followed. Jean-Pierre Blanchard and John Jeffries crossed the English Channel by balloon in 1785. In 1794 the French army used a tethered hydrogen balloon to watch the battle of Fleurus. Hot-air balloons were then almost forgotten until the 1950s and 1960s, when Ed Yost in the United States combined nylon fabric with a propane burner, making the modern sport balloon.
Source: content/entries/transport/hot-air-balloon.md