Part 4 · Food and Farming
Grain, Flour and Bread
How to turn a standing field of grain into flour and bread — harvesting, threshing, winnowing, grinding on stone, raising a sourdough from nothing, and building an oven of clay.
- Difficulty
- ●●●●●
- Time
- Harvest and threshing take days; a loaf takes a day; a clay oven takes a weekend plus weeks of drying
- Steps from zero
- 3 prerequisites →
The full path from nothing — 3 steps before this one
- Stone Tools
- Fire
- Farming from Seed
- Grain, Flour and Bread
Do them roughly in this order. See it on the tech tree →
Why it matters
Grain is the food that built cities. It is dense in energy (about 3,400 kcal per kilogram), it keeps dry for years, it can be measured, traded and taxed, and one field of it feeds many people through winter. But a grain of wheat is a hard seed wrapped in an inedible husk. Between the field and a meal stand five jobs: cut, thresh, winnow, grind, cook. Each is simple; together they are hours of work every day, which is why later chapters put so much effort into machines to do them (The Watermill, The Windmill).
Bread — ground grain mixed with water and baked — is the most efficient way to eat it. Raised with a sourdough, it is also lighter, tastier, keeps longer, and its nutrients are easier to absorb.
How it works
- A grain is a seed. Inside is the endosperm (starch, the flour), the germ (the oily embryo), and the bran (the tough skin). Outside is the husk or chaff, which is indigestible.
- Threshing breaks the grain loose from the stalk. Winnowing separates the light chaff from the heavy grain using wind. Grinding crushes the endosperm into flour.
- Gluten. When wheat flour is wetted and worked, two proteins join into a stretchy net called gluten. Gas bubbles trapped in that net make dough rise. Rye and barley have weak gluten (they make dense loaves); oats, maize, rice, millet and sorghum have none (they make flatbreads, porridges and cakes).
- Sourdough is a living culture of wild yeasts (which make carbon-dioxide gas that raises the dough) and lactic-acid bacteria (which sour it, keep away moulds, and break down substances in bran that block the absorption of iron and zinc). Both live naturally on grain and flour; you only have to give them food and warmth.
What you need
| Job | Tools | Notes |
|---|---|---|
| Cutting | Sickle | A curved wooden handle with flint flakes set in a groove with pitch (Stone Tools, Tar, Pitch and Glue), or a metal blade later (Sickle, Scythe and Hand Harvest Tools) |
| Threshing | Flail, threshing floor | Two sticks joined by a leather or cord hinge; a floor of hard-beaten clay or flat stone |
| Winnowing | Shallow basket or tray, a breeze | Baskets and Containers |
| Grinding | Saddle quern or rotary quern | Hard stone; see below |
| Sieving | Fine cloth or a tight-woven basket | Spinning and Weaving Cloth |
| Baking | Flat stone, pot, or a clay oven | Pottery, Finding and Preparing Clay |
Where to find it
- Grain: from your own fields (Farming from Seed), or wild grasses gathered as in Foraging Wild Food.
- Quern stone: you need a hard, tough stone with a slightly rough grain that does not crumble. The best is vesicular basalt — dark volcanic rock full of small gas holes, whose sharp edges keep cutting as it wears. Good alternatives: granite, hard gritstone (coarse, well-cemented sandstone), and conglomerate. Test a candidate by rubbing two pieces together hard for a minute: if loose sand pours off, reject it — that sand ends up in your bread and grinds your teeth to stumps. River boulders of the right size are common in hilly country.
- Clay and sand for the oven: see Finding and Preparing Clay.
Step by step: from field to flour
1. Harvest
- Judge ripeness. The straw has turned golden and the heads droop. Press a grain with your thumbnail: if milky juice comes out, wait. When it is firm like cheese and just dents ("hard dough"), it is ready to cut. If it is so hard it cannot dent at all, cut quickly — it will soon start dropping its seed.
- Cut with a sickle: grab a handful of stalks, cut 10–20 cm above the ground with a pulling stroke. Lay the handfuls in a row, heads all one way.
- Bind armfuls into sheaves with a twist of straw. Stand 8–12 sheaves leaning together, heads up, in a stook, so rain runs off.
- Dry in the stook for 1–2 weeks. The grain should crack, not squash, between your teeth before you bring it in.
2. Thresh
Spread sheaves on a clean, hard threshing floor, heads to the middle. Beat them with a flail — a handle about 1.4 m long joined by a loose leather loop to a heavier striking stick about 80 cm long. Swing it overhead so the striker lands flat on the heads. Turn the straw over and beat again. Shake out the straw and set it aside (it is fodder, bedding, thatch and fuel). Small amounts can simply be beaten against a log or rubbed between the palms. Animals walked in circles over the sheaves do it faster.
Hulled grains — emmer, einkorn, spelt and most barley — keep their husks after threshing. Parch them lightly (warm them on a hot stone or in a pot until they smell toasty, but before they brown), then pound them in a wooden mortar with a pestle, gently, to crack the husks free.
3. Winnow
- Wait for a light, steady breeze — enough to lift a dry leaf, not enough to bend branches.
- Stand with your side to the wind. Scoop grain and chaff into a shallow basket and toss it 20–30 cm into the air, catching it again. The chaff blows downwind; the grain falls back.
- Or pour it slowly from shoulder height onto a cloth or clean floor: chaff drifts aside, grain lands in a heap.
- Repeat until no chaff blows off. Finish by shaking the grain in the tray: the remaining bits of straw come to the top and can be picked off.
- Pick over by hand for stones, weed seeds and the purple-black spurs of ergot fungus, which is poisonous (see Foraging Wild Food).
4. Grind
The saddle quern — the oldest tool for the job.
- Choose or shape a lower stone about 40–60 cm long and 25–35 cm wide, with a flat or slightly hollow top, and a hand stone (rubber) as wide as the lower stone and about 20–30 cm long.
- Dress the faces: peck them all over with a pointed hard pebble until rough, then grind a handful of sand between them and wash it all away. Re-peck whenever they turn smooth.
- Set the lower stone on a firm base, tilted slightly away from you. Kneel at the near end.
- Put a small handful of grain on the upper part, and push the hand stone forward with your weight, then pull it back. Crushed grain gathers at the far end; move it back up and grind again until it is as fine as you want.
- Expect about 1 kg of coarse flour per hour of hard work. A family's daily bread takes 2–3 hours.
The rotary quern — two to three times faster, and less punishing to the knees.
- Make two round stones about 40 cm across and 8–12 cm thick. The lower one is fixed, with its top slightly domed. The upper one has its underside slightly hollow to match, a central hole (the eye) about 6 cm wide, and a hole near the rim for a wooden handle.
- Set a hardwood peg (the spindle) firmly in the centre of the lower stone. A wooden bar (the rynd) across the eye of the upper stone rests on the spindle, so the upper stone turns on it with a thin gap between the faces.
- Cut shallow grooves in both faces radiating from the centre, curving slightly, so the grain is pushed outward as it is ground.
- Pour grain into the eye a handful at a time and turn the handle. Flour spills out around the rim onto a cloth. Wedging the spindle higher makes coarser meal; lower makes finer flour.
5. Sieve
Shake the meal through a fine cloth stretched over a frame, or a tightly woven basket. What passes is flour; what stays is bran and coarse bits. Wholemeal (unsifted) flour is more nourishing; sifted flour rises better. Grind and sift again for finer flour. Use flour within a few weeks — the oily germ goes rancid. Whole grain keeps for years.
Warning Maize must be treated with lime or ash. People who live mostly on maize without this treatment develop pellagra — rough skin, diarrhoea, madness and death — because the vitamin niacin in maize is locked away. The Mesoamerican fix (called nixtamalization) frees it: simmer dry maize kernels for about an hour in water with about 1% slaked Lime (a heaped tablespoon per litre) or a double handful of sifted wood ash, leave to soak overnight, then rinse off the loosened skins and grind the wet kernels into dough (masa). See Nutrition and Deficiency Diseases.
Step by step: bread
Flatbread (today, with nothing but flour and water)
- Mix 100 g of flour with about 60 ml of water (a ratio of about 5 to 3) and a pinch of salt.
- Knead for 5 minutes until smooth. Rest it under a cloth for 20–30 minutes.
- Pull off balls the size of an egg. Flatten each to 2–3 mm thick with your palms or a round stick.
- Cook on a flat stone or clay plate heated in the fire, or directly on clean embers. Ready to cook when a drop of water dances and vanishes in 1–2 seconds. Cook 1–2 minutes a side, until brown spots appear and it puffs.
Sourdough starter from scratch
- Day 1: in a clean pot, mix 50 g wholemeal flour (rye is easiest, then wholemeal wheat) with 50 g water (about 3½ level tablespoons each). Stir hard to add air. Cover with a cloth. Keep it warm — 20–27 °C, comfortable shirt-sleeve warmth.
- Days 2–7: once a day, throw away half, and add 50 g flour and 50 g water. Stir well.
- You will often see a burst of bubbles on day 2–3, then a quiet spell of a day or two. Keep feeding — the first bubbles are bacteria, not yeast; the true yeasts take over afterwards.
- It is ready (usually day 5–10) when it reliably doubles in height within 4–8 hours of feeding, is full of bubbles, and smells pleasantly sour — like yoghurt, beer or green apples. A spoonful dropped in water floats.
- Keep it alive: feed it daily if warm, or keep it cool (a cellar, about 10 °C) and feed once or twice a week. A dried flake of starter, smeared thin and dried, can be revived weeks later with flour and water.
A sourdough loaf
| Ingredient | Amount |
|---|---|
| Flour (half wholemeal is good) | 500 g |
| Water, lukewarm | 350 ml |
| Active starter (fed 4–8 hours before) | 100 g |
| Salt | 10 g (2 level teaspoons) |
- Mix flour, water and starter into a shaggy dough. Rest 30 minutes, then work in the salt.
- Every 30 minutes for 2 hours, wet your hand and stretch one side of the dough up and fold it over; turn the bowl and repeat 4 times.
- Leave covered to rise — 4–8 hours at 20–25 °C, longer when cool — until about half again as big, domed and bubbly.
- Shape into a tight round, put it seam up in a basket lined with a floured cloth, and let it rise again for 1–3 hours (or overnight somewhere cool).
- Turn it onto a floured board, slash the top 1 cm deep with a sharp blade so it can expand, and bake in a hot oven (see below) for 40–50 minutes.
- It is done when the crust is deep brown and the bottom sounds hollow when knocked. Let it cool at least an hour before cutting — it is still cooking inside.
Without an oven, bake under an upturned clay pot heaped with embers, or in a lidded pot set in the coals with embers on the lid.
Building a clay oven
- Base. Build a solid platform at waist height (about 80–90 cm) from stones, logs filled with rubble, or packed earth. Top it with a 10 cm insulating layer — dry ash, or clay mixed with sawdust — then a level floor of flat stones, fired bricks (Bricks), or a smooth 5 cm layer of clay and sand.
- Sand form. On the floor, heap damp sand into a dome about 60–70 cm across and 40–45 cm high — the shape of the inside. Cover it with wet newspaper or large leaves so the clay will not stick.
- Thermal layer. Mix 1 part clay to 2–3 parts sharp sand with just enough water to form a stiff ball that holds a thumbprint without cracking. Pack it over the form in a layer 8–10 cm thick, pressing down firmly, not smearing. Keep it the same thickness all over.
- Door. Mark a door with its height about 63% of the inside height (about 26–28 cm for a 42 cm dome) and as wide as it needs to be for your loaves. A door this height lets the oven breathe and still holds the heat.
- Wait a day or two until the clay is leather-hard, then cut out the door and scoop out the sand.
- Insulation layer. Cover the dome with a further 8–10 cm of clay slip (runny clay) mixed with as much straw or sawdust as it will hold — this traps air and keeps the heat in.
- Dry slowly under a roof for 2–4 weeks, then light small fires daily for several days before the first hot firing. Cracks in the outer layer are normal; fill them with clay.
Firing and baking. Burn dry hardwood (about an armful of split wrist-thick sticks) for 1½–3 hours. At first the inside of the dome blackens with soot; when it burns clean and pale, the oven walls are near 350–400 °C. Rake out the coals, wipe the floor with a damp rag on a stick, and close the door for 10 minutes to even out the heat. Flour test: toss a pinch of flour on the floor. If it blackens within seconds, wait; if it browns in about 10–15 seconds, put in the bread and close the door. One firing bakes several batches: loaves first, then slower things as the oven cools.
How to tell it worked
- Winnowed grain is clean in your hand, with no chaff blowing off it.
- Good flour rubbed between fingers feels soft, with no grit crunching between your teeth.
- Good bread has an open, springy crumb, no raw grey streak at the bottom, and a pleasantly sour smell.
Note Troubleshooting. Gritty flour → the quern stone is too soft, or newly dressed; grind and discard a handful of bran first. Starter smells of acetone or nail varnish → it is hungry; feed it twice a day. Starter grew pink, orange or fuzzy mould → throw it away and start again with cleaner pots. Dense, flat loaf → starter not active enough, too short a rise, or flour too low in gluten (rye, barley). Burnt bottom, raw middle → oven floor too hot; wait longer after raking out, or bake on a layer of leaves.
Dangers
- Ergot in grain causes gangrene, convulsions and miscarriage. Pick it out; never use grain with many black spurs. See Foraging Wild Food.
- Mouldy grain can carry invisible poisons (aflatoxins) that damage the liver. Grain that smells musty, has clumped, or is discoloured should not be eaten.
- Dust. A cloud of fine flour or grain dust can explode if a flame reaches it. Keep open fires away from milling and sieving.
- Burns from ovens and hot stones: use long wooden peels and rakes. See Wound Care and Antiseptics.
- Grit from soft querns wore down the teeth of ancient people to the gums. Choose hard stone.
What this unlocks
Grain can be cooked into porridge and bread (Cooking and Recipes), brewed into beer and vinegar (Fermentation, Beer, Wine and Cider, Vinegar and Pickling), boiled for starch paste, malted for Sugar, and fed to animals (Keeping Animals). Grinding by hand is so laborious that it drove the invention of the The Watermill and The Windmill — the first engines. Stored grain needs protection from damp, insects and rats (Preserving Food, Granaries and Food Storage).
How it was first done
People were grinding wild grains long before farming: at Ohalo II in Israel, about 23,000 years ago, foragers ground wild barley and wheat on a basalt slab. Charred crumbs of flatbread about 14,400 years old, made from wild cereals and tubers, were found at Shubayqa 1 in Jordan — four thousand years before the first fields. Saddle querns were the standard tool of the early farmers, and skeletons of Neolithic women show the damage to toes, knees and spine from hours of daily grinding. The rotary quern appeared around 2,500 years ago, probably in the western Mediterranean, and spread across Europe. Leavened bread was baked in ancient Egypt, where loaves and bakeries are known from tombs about 4,500 years old. The basic sourdough you make today is probably very close to theirs.